# US 2024/0174861 A1 · Modified lignin products for rigid foams

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0174861 A1
- Document ID: US20240174861A1
- Status: Published application
- Kind: A1
- Application number: 18/432,603
- Filed: 2024-02-05
- Published: 2024-05-30
- Earliest claimed: 2021-07-26
- Assignees: MCPU Polymer Engineering, LLC
- Applicants: MCPU Polymer Engineering LLC
- Inventors: Thomas M. GARRETT; Swarup Kumar MAITI
- Web page: https://patentgrep.com/patent/US20240174861A1

## CPC

- C08L 97/005: {Lignin}
- C07G 1/00: Low-molecular-weight derivatives of lignin (high-molecular-weight derivatives of lignin {C08H6/00})
- C08G 18/12: using two or more compounds having active hydrogen in the first polymerisation step
- C08G 18/18: containing secondary or tertiary amines or salts thereof
- C08G 18/4208: {containing aromatic groups}
- C08G 18/4837: {and other oxyalkylene units}
- C08G 18/6492: {Lignin containing materials; Wood resins; Wood tars; Derivatives thereof}
- C08G 18/7657: {containing two or more aromatic rings}
- C08H 6/00: {Macromolecular compounds derived from lignin, e.g. tannins, humic acids}
- C08J 9/0061: {characterized by the use of several polymeric components}
- C08J 9/141: {Hydrocarbons}
- C08K 3/22: of metals
- C08K 3/30: Sulfur-, selenium- or tellurium-containing compounds
- C08K 3/32: Phosphorus-containing compounds
- C08K 5/0066: {Flame-proofing or flame-retarding additives}
- C08K 5/521: Esters of phosphoric acids, e.g. of H3PO4
- C09K 21/12: containing phosphorus
- C08G 2101/00: Manufacture of cellular products
- C08G 2110/0025: rigid
- C08J 2201/026: Crosslinking before of after foaming
- C08J 2203/14: Saturated hydrocarbons, e.g. butane; Unspecified hydrocarbons
- C08J 2205/10: Rigid foams
- C08J 2375/06: from polyesters
- C08J 2375/12: from compounds containing nitrogen and active hydrogen, the nitrogen atom not being part of an isocyanate group
- C08J 2497/00: Characterised by the use of lignin-containing materials
- C08K 2003/2248: {of copper}
- C08K 2003/3045: {Sulfates}
- C08K 2003/321: {Phosphates}
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C07G: COMPOUNDS OF UNKNOWN CONSTITUTION (sulfonated fats, oils or waxes of undetermined constitution C07C309/62)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08H: DERIVATIVES OF NATURAL MACROMOLECULAR COMPOUNDS (polysaccharides C08B; natural rubber C08C; natural resins or their derivatives C09F; bituminous materials C10)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

Modified lignin products, processes for making them, and their use to produce rigid polyurethane or polyisocyanurate foams are disclosed. The processes comprise heating a lignin source with a nitrogen source and a starved concentration of a C1-C5 aldehyde to give a reaction mixture comprising a Mannich condensation product, neutralizing the reaction mixture, and isolating the modified lignin product. The process is performed at a mass ratio of lignin source to nitrogen source within the range of 1:1 to 1:5 and at a molar ratio of nitrogen source to C1-C5 aldehyde within the range of 3.5:1 to 1:1. Polyol blends and performance additives that contain the modified lignin products are described. Rigid foams that process well and incorporate up to 60 wt. %, based on the amount of polyol component, of the modified lignin contribute to excellent flame retardancy and low-temperature R-value performance.

## Claims

### Claim 1

A modified lignin product made by a process comprising:
(a) heating a lignin source with an amide nitrogen source and a starved concentration of a C1-C5 aldehyde in the presence of an acidic or basic catalyst at a mass ratio of lignin source to nitrogen source within the range of 1:1 to 1:5 and at a molar ratio of nitrogen source to C1-C5 aldehyde within the range of 3.5:1 to 1:1 to give a reaction mixture comprising a Mannich condensation product;
(b) neutralizing the reaction mixture from step (a) to give a neutralized reaction mixture; and
(c) isolating a modified lignin product from the neutralized reaction mixture.

### Claim 2 (depends on 1)

A performance additive comprising:
(a) a phosphorus-based flame retardant, a natural oil polyol, or a combination thereof; and
(b) 10 to 90 wt. %, based on the amount of performance additive, of the modified lignin product of claim 1.

### Claim 3 (depends on 2)

The performance additive of claim 2 wherein the phosphorus-based flame retardant is a trialkyl phosphate.

### Claim 4 (depends on 3)

The performance additive of claim 3 wherein the trialkyl phosphate is selected from the group consisting of trimethylphosphate, triethylphosphate, tri-n-butylphosphate, trioctylphosphate, and mixtures thereof.

### Claim 5 (depends on 2)

The performance additive of claim 2 further comprising a nonionic surfactant.

### Claim 6 (depends on 5)

The performance additive of claim 5 wherein the nonionic surfactant is an alkylphenol ethoxylate.

### Claim 7 (depends on 2)

The performance additive of claim 2 further comprising copper(I) oxide, copper(II) sulfate, or copper(II) phosphate in an amount within the range of 0.1 to 1 mmol of Cu per gram of the modified lignin product.

### Claim 8 (depends on 1)

A polyol blend comprising:
(a) 20 to 80 wt. % of an aromatic polyester polyol;
(b) 5 to 30 wt. % of a glycol;
(c) optionally, 5 to 30 wt. % of a natural oil polyol; and
(d) 10 to 60 wt. % of the modified lignin product of claim 1.

### Claim 9 (depends on 8)

The polyol blend of claim 8 wherein the glycol is selected from the group consisting of dipropylene glycol, diethylene glycol, PEG 300, and PEG 400, and the blend has a Brookfield viscosity measured at 25° C. of less than 3000 cP.

### Claim 10 (depends on 8)

The polyol blend of claim 8 wherein the blend is prepared by high-shear mixing of the modified lignin product, glycol, aromatic polyester polyol, and optional natural oil polyol at or about room temperature.

### Claim 11 (depends on 1)

A rigid polyurethane (PU) or polyisocyanurate (PIR) foam comprising a reaction product of an aromatic polyester polyol, a glycol, a polyisocyanate, a urethane catalyst, a foam-stabilizing surfactant, a blowing agent, and the modified lignin product of claim 1.

### Claim 12 (depends on 11)

The foam of claim 11 wherein the modified lignin product is isolated by concentrating the neutralized reaction mixture.

### Claim 13 (depends on 11)

The foam of claim 11 comprising 10 to 60 wt. %, based on the amount of polyol components, of the modified lignin product.

### Claim 14 (depends on 2)

A rigid polyurethane (PU) or polyisocyanurate (PIR) foam comprising a reaction product of an aromatic polyester polyol, a glycol, a polyisocyanate, a urethane catalyst, a foam-stabilizing surfactant, a blowing agent, and the performance additive of claim 2.

### Claim 15 (depends on 8)

A rigid polyurethane (PU) or polyisocyanurate (PIR) foam comprising a reaction product of a polyisocyanate, a urethane catalyst, a foam-stabilizing surfactant, a blowing agent, and the polyol blend of claim 8.

### Claim 16

A modified lignin product made by a process comprising:
(a) heating a lignin source with a urea nitrogen source and a starved concentration of a C1-C5 aldehyde in the presence of an acidic or basic catalyst at a mass ratio of lignin source to nitrogen source within the range of 1:1 to 1:5 and at a molar ratio of nitrogen source to C1-C5 aldehyde within the range of 3.5:1 to 1:1 to give a reaction mixture comprising a Mannich condensation product;
(b) neutralizing the reaction mixture from step (a) to give a neutralized reaction mixture; and
(c) isolating a modified lignin product from the neutralized reaction mixture.

### Claim 17 (depends on 16)

A performance additive comprising:
(a) a phosphorus-based flame retardant, a natural oil polyol, or a combination thereof; and
(b) 10 to 90 wt. %, based on the amount of performance additive, of the modified lignin product of claim 16.

### Claim 18 (depends on 17)

The performance additive of claim 17 wherein the phosphorus-based flame retardant is a trialkyl phosphate.

### Claim 19 (depends on 17)

The performance additive of claim 17 wherein the trialkyl phosphate is selected from the group consisting of trimethylphosphate, triethylphosphate, tri-n-butylphosphate, trioctylphosphate, and mixtures thereof.

### Claim 20 (depends on 17)

The performance additive of claim 17 further comprising a nonionic surfactant.

### Claim 21 (depends on 17)

The performance additive of claim 17 further comprising copper(I) oxide, copper(II) sulfate, or copper(II) phosphate in an amount within the range of 0.1 to 1 mmol of Cu per gram of the modified lignin product.

### Claim 22 (depends on 16)

A polyol blend comprising:
(a) 20 to 80 wt. % of an aromatic polyester polyol;
(b) 5 to 30 wt. % of a glycol;
(c) optionally, 5 to 30 wt. % of a natural oil polyol;
(d) 10 to 60 wt. % of the modified lignin product of claim 16.

### Claim 23

A modified lignin product made by a process comprising:
(a) heating a lignin source with a urea nitrogen source and a starved concentration of formaldehyde in the presence of an acidic or basic catalyst at a mass ratio of lignin source to nitrogen source within the range of 1:1 to 1:5 and at a molar ratio of nitrogen source to C1-C5 aldehyde within the range of 3.5:1 to 1:1 to give a reaction mixture comprising a Mannich condensation product;
(b) neutralizing the reaction mixture from step (a) to give a neutralized reaction mixture; and
(c) isolating a modified lignin product from the neutralized reaction mixture
wherein the mass ratio of lignin source to urea to formaldehyde is about 1.0 to about 1.2 to about 0.56.

### Claim 24 (depends on 23)

A performance additive comprising:
(a) a phosphorus-based flame retardant, a natural oil polyol, or a combination thereof; and
(b) 10 to 90 wt. %, based on the amount of performance additive, of the modified lignin product of claim 23.

### Claim 25 (depends on 24)

The performance additive of claim 24 wherein the phosphorus-based flame retardant is a trialkyl phosphate.

### Claim 26 (depends on 24)

The performance additive of claim 24 wherein the trialkyl phosphate is selected from the group consisting of trimethylphosphate, triethylphosphate, tri-n-butylphosphate, trioctylphosphate, and mixtures thereof.

### Claim 27 (depends on 24)

The performance additive of claim 24 further comprising a nonionic surfactant.

### Claim 28 (depends on 24)

The performance additive of claim 24 further comprising copper(I) oxide, copper(II) sulfate, or copper(II) phosphate in an amount within the range of 0.1 to 1 mmol of Cu per gram of the modified lignin product.

### Claim 29 (depends on 23)

A polyol blend comprising:
(a) 20 to 80 wt. % of an aromatic polyester polyol;
(b) 5 to 30 wt. % of a glycol;
(c) optionally, 5 to 30 wt. % of a natural oil polyol;
(d) 10 to 60 wt. % of the modified lignin product of claim 23.