# US 2024/0174827 A1 · Heat-shrinkable films and related systems and methods

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0174827 A1
- Document ID: US20240174827A1
- Status: Published application
- Kind: A1
- Application number: 18/521,511
- Filed: 2023-11-28
- Published: 2024-05-30
- Earliest claimed: 2022-11-30
- Assignees: Klöckner Pentaplast of America, Inc.
- Applicants: Klöckner Pentaplast of America, Inc.
- Inventors: Christian Grießhammer; Hongliang Zhang
- Web page: https://patentgrep.com/patent/US20240174827A1

## CPC

- B32B 1/08: Tubular products
- C08J 5/18: Manufacture of films or sheets
- B29C 48/0018: {combined with shaping by orienting, stretching or shrinking, e.g. film blowing (B29C48/0017 takes precedence)}
- B29C 48/022: {characterised by the choice of material}
- B29C 48/08: flexible, e.g. films
- B29C 48/18: the components being layers
- B32B 7/028: Heat-shrinkability
- B32B 7/03: with respect to the orientation of features (direction of fibres or filaments B32B5/12)
- B32B 27/08: of synthetic resin
- B32B 27/36: comprising polyesters
- C08J 11/08: using selective solvents for polymer components
- B29K 2995/0049: Heat shrinkable
- B32B 2250/02: 2 layers
- B32B 2250/03: 3 layers
- B32B 2250/244: All polymers belonging to those covered by group B32B27/36
- B32B 2255/10: on synthetic resin layer or on natural or synthetic rubber layer
- B32B 2255/28: Multiple coating on one surface
- B32B 2270/00: Resin or rubber layer containing a blend of at least two different polymers
- B32B 2307/30: having particular thermal properties
- B32B 2307/4023: on the layer surface, e.g. ink
- B32B 2307/514: Oriented
- B32B 2307/736: Shrinkable
- B32B 2307/7376: Thickness
- B32B 2307/75: Printability
- B32B 2367/00: Polyesters, e.g. PET, i.e. polyethylene terephthalate
- B32B 2519/00: Labels, badges
- B32B 2597/00: Tubular articles, e.g. hoses, pipes
- C08J 2367/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds; (C08J2367/06 takes precedence)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

In various examples, the subject matter of this disclosure relates to heat-shrinkable films and systems and methods for manufacturing and recycling heat-shrinkable films. A heat-shrinkable film can include: a first layer having a first copolymerized polyester resin; and a second layer disposed on the first layer and having a second copolymerized polyester resin, wherein the heat-shrinkable film is predisposed to either (i) curl towards the first layer when heat is applied or (ii) not curl towards the second layer when heat is applied. A layer of ink can be disposed on the second layer.

## Claims

### Claim 1

A heat-shrinkable film comprising:
a first layer comprising a first copolymerized polyester resin; and
a second layer disposed on the first layer and comprising a second copolymerized polyester resin,
wherein the heat-shrinkable film is predisposed to either (i) curl towards the first layer when heat is applied or (ii) not curl towards the second layer when heat is applied.

### Claim 2 (depends on 1)

The heat-shrinkable film of claim 1, wherein the first layer and the second layer each comprises from about 5% to about 95% of a total thickness of the heat-shrinkable film.

### Claim 3 (depends on 1)

The heat-shrinkable film of claim 1, wherein the first copolymerized polyester resin and the second copolymerized polyester resin each comprise a diol component and a dicarboxylic acid component, and wherein the diol component comprises at least one of ethylene glycol, diethylene glycol, neopentyl glycol, cyclohexanedimethanol, or methyl propanediol.

### Claim 4 (depends on 3)

The heat-shrinkable film of claim 3, wherein the first copolymerized polyester resin and the second copolymerized polyester resin each comprises a functional glycol modification in which the diol component comprises at least one of diethylene glycol, neopentyl glycol, cyclohexanedimethanol, or methyl propanediol.

### Claim 5 (depends on 4)

The heat-shrinkable film of claim 4, wherein the first copolymerized polyester resin comprises a total amount of the functional glycol modification from about 15 mole % to about 40 mole %, based on a total number of moles of the diol component.

### Claim 6 (depends on 4)

The heat-shrinkable film of claim 4, wherein the second copolymerized polyester resin comprises a total amount of the functional glycol modification from about 5 mole % to about 35 mole %, based on a total number of moles of the diol component.

### Claim 7 (depends on 4)

The heat-shrinkable film of claim 4, wherein the first copolymerized polyester resin comprises a first total amount of the functional glycol modification, wherein the second copolymerized polyester resin comprises a second total amount of the functional glycol modification, and wherein the first total amount is greater than the second total amount by at least 1 mole %, based on a total number of moles of the diol component.

### Claim 8 (depends on 1)

The heat-shrinkable film of claim 1, wherein the first copolymerized polyester resin and the second copolymerized polyester resin are identical.

### Claim 9 (depends on 1)

The heat-shrinkable film of claim 1, wherein at least one of the first layer or the second layer comprises a blend of copolymerized polyester resins.

### Claim 10 (depends on 1)

The heat-shrinkable film of claim 1, further comprising a third layer disposed between the first layer and the second layer, wherein a functional glycol modification of the first layer is greater than a functional glycol modification of the third layer, and wherein the functional glycol modification of the third layer is greater than a functional glycol modification of the second layer.

### Claim 11 (depends on 1)

The heat-shrinkable film of claim 1, further comprising a third layer comprising the first copolymerized polyester resin, wherein the second layer is disposed between the first layer and the third layer, and wherein the third layer is thinner than the first layer.

### Claim 12 (depends on 1)

The heat-shrinkable film of claim 1, further comprising a layer of ink disposed on the second layer.

### Claim 13 (depends on 12)

The heat-shrinkable film of claim 12, further comprising a primer layer disposed between the layer of ink and the second layer, wherein the primer layer is configured to dissolve in a caustic soda.

### Claim 14

A shrink sleeve comprising:
a heat-shrinkable film forming a tube shape and comprising:
a first layer comprising a first copolymerized polyester resin; and
a second layer disposed on the first layer and comprising a second copolymerized polyester resin; and
a layer of ink disposed on the second layer,
wherein a particle of the heat-shrinkable film is predisposed to either (i) curl towards the first layer when heat is applied or (ii) not curl towards the second layer when heat is applied.

### Claim 15 (depends on 14)

The shrink sleeve of claim 14, wherein the layer of ink is on an inner surface of the tube shape.

### Claim 16 (depends on 14)

The shrink sleeve of claim 14, wherein the shrink sleeve is configured to shrink around a container when heat is applied by at least one of steam, hot-air, microwave energy, or infrared radiation.

### Claim 17 (depends on 14)

The shrink sleeve of claim 14, wherein the first copolymerized polyester resin and the second copolymerized polyester resin each comprises a diol component and a dicarboxylic acid component, and wherein the diol component comprises at least one of ethylene glycol, diethylene glycol, neopentyl glycol, cyclohexanedimethanol, or methyl propanediol.

### Claim 18 (depends on 17)

The shrink sleeve of claim 17, wherein the first copolymerized polyester resin and the second copolymerized polyester resin each comprises a functional glycol modification in which the diol component comprises at least one of diethylene glycol, neopentyl glycol, cyclohexanedimethanol, or methyl propanediol.

### Claim 19 (depends on 18)

The shrink sleeve of claim 18, wherein the first copolymerized polyester resin comprises a total amount of the functional glycol modification from about 15 mole % to about 40 mole %, based on a total number of moles of the diol component.

### Claim 20 (depends on 18)

The shrink sleeve of claim 18, wherein the second copolymerized polyester resin comprises a total amount of the functional glycol modification from about 5 mole % to about 35 mole %, based on a total number of moles of the diol component.

### Claim 21 (depends on 18)

The shrink sleeve of claim 18, wherein the first copolymerized polyester resin comprises a first total amount of the functional glycol modification, wherein the second copolymerized polyester resin comprises a second total amount of the functional glycol modification, and wherein the first total amount is greater than the second total amount by at least 1 mole %, based on a total number of moles of the diol component.

### Claim 22 (depends on 14)

The shrink sleeve of claim 14, wherein at least one of the first layer or the second layer comprises a blend of copolymerized polyester resins.

### Claim 23

A method of manufacturing a heat-shrinkable film, the method comprising:
coextruding a heat-shrinkable film comprising (i) a first layer comprising a first copolymerized polyester resin and (ii) a second layer disposed on the first layer and comprising a second copolymerized polyester resin,
wherein the film is predisposed to either (i) curl towards the first layer when heat is applied or (ii) not curl towards the second layer when heat is applied.

### Claim 24 (depends on 23)

The method of claim 23, wherein the heat-shrinkable film is coextruded at a temperature from about 200° C. to about 300° C., and wherein coextruding the heat-shrinkable film comprises casting the heat-shrinkable film through a die and onto a chill roll.

### Claim 25 (depends on 23)

The method of claim 23, further comprising stretching the heat-shrinkable film in a tenter frame to a stretch ratio from about 1.5 to about 7.

### Claim 26 (depends on 25)

The method of claim 25, wherein the heat-shrinkable film comprises a glass transition temperature, and wherein the stretching is performed at a temperature from about the glass transition temperature to the glass transition temperature plus about 20° C.

### Claim 27

A method of recycling a heat-shrinkable film, the method comprising:
obtaining particles of a heat-shrinkable film comprising:
a first layer comprising a first copolymerized polyester resin; and
a second layer disposed on the first layer and comprising a second copolymerized polyester resin; and
a layer of ink disposed on the second layer; and
immersing the particles in a liquid bath,
wherein the particles are predisposed to either (i) curl towards the first layer when heat is applied or (ii) not curl towards the second layer when heat is applied.

### Claim 28 (depends on 27)

The method of claim 27, wherein the particles comprise a length from about 1 mm to about 50 mm.

### Claim 29 (depends on 27)

The method of claim 27, wherein the liquid bath comprises:
a temperature from about 55° C. to about 95° C.;
a caustic soda in an amount from about 0.1% to about 5%, by weight; and
a detergent in an amount from about 0.1% to about 3%, by weight.

### Claim 30 (depends on 27)

The method of claim 27, wherein the particles of the heat-shrinkable film comprise a primer layer disposed between the layer of ink and the second layer, wherein the primer layer is configured to dissolve in a caustic soda.