# US 2024/0174800 A1 · Melt-stable polylactide resin compositions containing phosphite esters

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0174800 A1
- Document ID: US20240174800A1
- Status: Published application
- Kind: A1
- Application number: 18/550,583
- Filed: 2022-03-28
- Published: 2024-05-30
- Earliest claimed: 2021-03-31
- Assignees: NatureWorks LLC
- Applicants: NatureWorks LLC
- Inventors: Jed Richard Randall; Samantha Leigh Thompson-Barclay; Patricia America Nancy Popescu; Patrick Kevin Hoard; Joseph David Schroeder; James Russell Valentine; Manuel A.W. Natal
- Web page: https://patentgrep.com/patent/US20240174800A1

## CPC

- C08G 63/692: containing phosphorus
- C08L 67/04: Polyesters derived from hydroxycarboxylic acids, e.g. lactones (C08L67/06 takes precedence)
- C08G 63/823: {for the preparation of polylactones or polylactides}
- C08G 63/88: Post-polymerisation treatment
- C08K 3/08: Metals
- C08K 3/32: Phosphorus-containing compounds
- C08K 5/524: Esters of phosphorous acids, e.g. of H3PO3
- C08K 5/0033: {Additives activating the degradation of the macromolecular compound}
- C08K 5/005: {Stabilisers against oxidation, heat, light, ozone}
- C08K 2003/329: {Phosphorus containing acids}
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

Polylactide resin compositions contain certain phosphite esters. The presence of the phosphite ester increases the rate of hydrolysis of the polylactide resin under conditions of moisture (including atmospheric moisture) at mildly elevated temperatures.

## Claims

### Claim 1

A polylactide resin composition comprising (a) at least one polylactide having a number-average molecular weight as measured by gel permeation chromatography against a polystyrene standard of at least 20,000 g/mol, the polylactide containing (i) 5 to 300 ppm by weight of Group 2-14 metals based on the weight of the polylactide, (ii) 0.1 to 2 parts by weight per 100 parts by weight of the polylactide of (ii-a) a polymer having multiple carboxylic acid, a number average molecular weight of at least 500 g/mol and at least one carboxylic acid group per 250 atomic mass units and/or (ii-b) a polyphosphoric acid which may be partially or completely neutralized, and/or residue thereof and (iii) no more than 0.6 parts by weight of lactide per 100 parts by weight of the polylactide, and (b) at least one phosphite ester compound having a number-average molecular weight of up to 5,000 g/mol, the phosphite ester compound containing 3 to 15% by weight phosphorus and wherein the phosphite ester compound contains, per phosphite phosphorus atom, from zero to one aryl group in which at least one ring carbon ortho to a ring carbon bonded directly to a phosphite oxygen is directly bonded to a tertiary carbon atom of a substituent group, and the polylactide resin composition containing sufficient phosphite ester compound to provide 0.01 to 32 g of phosphorus per kilogram of the polylactide in the polylactide resin composition.

### Claim 2 (depends on 1)

The polylactide resin composition of claim 1 wherein the phosphite ester compound is one or more of bis(2,4-di-t-butylphenyl)pentaerythritol diphosphite, bis(2,4-dicumylphenyl) pentaerythritol diphosphite, bis (octadecyl)pentaerythritol diphosphite, triphenyl phosphite, tridecyl phosphite, didecyl phenyl phosphite, phenyl neopentylene glycol phosphite ester and tris(4-nonylphenyl) phosphite.

### Claim 3 (depends on 1)

The polylactide resin composition of claim 1 wherein the phosphite ester compound includes at least one at least one polyphosphite ester compound represented by either of structures I and II, wherein structure I is
wherein each R2, R3, R4 and R5 can be the same or different and independently selected from the group consisting of C1-20 alkyl, C3-22 alkenyl, C6-40 cycloalkyl, C7-40 cycloalkylene, C1-20 methoxy alkyl glycol ethers, C1-20 alky glycol ethers, and/or Y—OH; Y is selected from the group consisting of C2-40 alkylene, C2-40 alkyl lactone, —R6—N(R7)—R8— wherein R6, R7, and R8 are independently selected from the group consisting of hydrogen, C1-20 alkyl, C3-22 alkenyl, C6-40 cycloalkyl, C7-40 cycloalkylene, C1-20 methoxy alkyl glycol ethers, C1-20 alky glycol ethers and/or Y—OH, m is an integral value ranging from 2 to 100 and x is an integral value ranging from 1 to 1000; and structure II is
wherein R10, R11, R12, R13 and R14 can be the same or different are independently selected from the group consisting of C1-20 alkyl, C2-22 alkenyl, C6-40 cycloalkyl and C704o cycloalkenyl; Y is selected from the group consisting of C2-40 alkylene, C2-40 aliphatic carboxylic acid esters and C3-40 cycloalkylenes, n is a number from 5 to 100, u is a number from 8 to 1000, v is a number from 1 to 1000 and w is a number from 1 to 1000.

### Claim 4 (depends on 1)

The polylactide resin composition of claim 1 which contains 5 to 300 ppm tin.

### Claim 5 (depends on 1)

The polylactide resin composition of claim 1 wherein the polymer having multiple carboxylic acid groups, a number average molecular weight of at least 500 g/mol and at least one carboxylic acid group per 250 atomic mass units is present and is a homopolymer or copolymer of acrylic acid.

### Claim 6 (depends on 1)

The polylactide resin composition of claim 1 wherein the polyphosphoric acid or residue thereof is present.

### Claim 7 (depends on 1)

A method of making a polylactide resin composition of claim 1, comprising the steps of:
a) polymerizing lactide in the presence of a Group 2-14 metal-containing catalyst to produce a crude polylactide containing 5 to 300 ppm by weight of Group 2-14 metals based on the weight of the polylactide;
b) combining the crude PLA resin with a 0.1 to 2 parts by weight, per 100 parts of the polylactide, of (i) a polymer having multiple carboxylic acid groups, a number average molecular weight of at least 500 g/mol and at least one carboxylic acid group per 250 atomic mass units, and/or (ii) a polyphosphoric acid and/or residue thereof;
c) before, simultaneously with, or after step b), devolatilizing the crude polylactide resin to reduce the lactide concentration to no greater than 0.6% of the combined weight of the polylactide and the remaining lactide and then
d) after step b), combining the PLA resin at least one phosphite ester compound containing 3 to 15% by weight phosphorus and wherein the phosphite ester compound contains, per phosphite phosphorus atom, from zero to one aryl group in which at least one ring carbon ortho to a ring carbon bonded directly to a phosphite oxygen is directly bonded to a tertiary carbon atom of a substituent group, in an amount of sufficient to provide 0.01 to 32 g of phosphorus per kg of the polylactide in the polylactide resin composition.

### Claim 8 (depends on 7)

The method of claim 7 wherein the phosphite ester compound is one or more of bis(2,4-di-t-butylphenyl)pentaerythritol diphosphite, bis(2,4-dicumylphenyl) pentaerythritol diphosphite, bis (octadecyl)pentaerythritol diphosphite, triphenyl phosphite, tridecyl phosphite, didecyl phenyl phosphite, phenyl neopentylene glycol phosphite ester and tris(4-nonylphenyl) phosphite.

### Claim 9 (depends on 7)

The method of claim 7 wherein the phosphite ester compound includes at least one at least one polyphosphite ester compound represented by either of structures I and II, wherein structure I is
wherein each R2, R3, R4 and R5 can be the same or different and independently selected from the group consisting of C1-20 alkyl, C3-22 alkenyl, C6-40 cycloalkyl, C7-40 cycloalkylene, C1-20 methoxy alkyl glycol ethers, C1-20 alky glycol ethers, and/or Y—OH; Y is selected from the group consisting of C2-40 alkylene, C2-40 alkyl lactone, —R6—N(R7)—R8— wherein R6, R7, and R8 are independently selected from the group consisting of hydrogen, C1-20 alkyl, C3-22 alkenyl, C6-40 cycloalkyl, C7-40 cycloalkylene, C1-20 methoxy alkyl glycol ethers, C1-20 alky glycol ethers and/or Y—OH, m is an integral value ranging from 2 to 100 and x is an integral value ranging from 1 to 1000; and structure II is
wherein R10, R11, R12, R13 and R14 can be the same or different are independently selected from the group consisting of C1-20 alkyl, C2-22 alkenyl, C6-40 cycloalkyl and C704o cycloalkenyl; Y is selected from the group consisting of C2-40 alkylene, C2-40 aliphatic carboxylic acid esters and C3-40 cycloalkylenes, n is a number from 5 to 100, u is a number from 8 to 1000, v is a number from 1 to 1000 and w is a number from 1 to 1000.

### Claim 10 (depends on 7)

The method of claim 7 wherein the polylactide resin composition contains 5 to 300 ppm tin.

### Claim 11 (depends on 7)

The method of claim 7 wherein in step b the crude PLA resin is combined with the polymer having multiple carboxylic acid groups, a number average molecular weight of at least 500 g/mol and at least one carboxylic acid group per 250 atomic mass units.

### Claim 12

The method of 7 wherein in step b) the crude PLA resin is combined with the polyphosphoric acid.

### Claim 13

A polylactide resin composition comprising (a) at least one polylactide having a number-average molecular weight as measured by gel permeation chromatography against a polystyrene standard of at least 20,000 g/mol having dissolved or dispersed therein (b) at least one polyphosphite ester compound containing 3.5 to 15% by weight phosphorus and being represented by either of structures I and II, wherein structure I is
wherein each R2, R3, R4 and R5 can be the same or different and independently selected from the group consisting of C1-20 alkyl, C3-22 alkenyl, C6-40 cycloalkyl, C7-40 cycloalkylene, C1-20 methoxy alkyl glycol ethers, C1-20 alky glycol ethers, and/or Y—OH; Y is selected from the group consisting of C2-40 alkylene, C2-40 alkyl lactone, —R6—N(R7)—R8— wherein R6, R7, and R8 are independently selected from the group consisting of hydrogen, C1-20 alkyl, C3-22 alkenyl, C6-40 cycloalkyl, C7-40 cycloalkylene, C1-20 methoxy alkyl glycol ethers, C1-20 alky glycol ethers and/or Y—OH, m is an integral value ranging from 2 to 100 and x is an integral value ranging from 1 to 1000; and structure II is
wherein R10, R11, R12, R13 and R14 can be the same or different are independently selected from the group consisting of C1-20 alkyl, C2-22 alkenyl, C6-40 cycloalkyl and C704o cycloalkenyl; Y is selected from the group consisting of C2-40 alkylene, C2-40 aliphatic carboxylic acid esters and C3-40 cycloalkylenes, n is a number from 5 to 100, u is a number from 8 to 1000, v is a number from 1 to 1000 and w is a number from 1 to 1000,
is (i) a linear or branched C2 to C24 alkylene group; (ii) a residue, after removal of hydroxyl groups, of a glycol ether or a glycol polyether, a homopolymer or copolymer of ethylene glycol, and/or propylene glycol having 4 or more ether units and formula weights (after removal of hydroxyl groups) of up to 1000 g/mol; and (iii) an o-, m-, or p-dialkyl cyclohexane, in which the alkyl groups have 1 to 4 carbon atoms.

### Claim 14 (depends on 13)

A process for hydrolyzing a polylactide resin, comprising immersing a polylactide composition of claim 13 in liquid water at a temperature of 25° C. to 80° C.

### Claim 15 (depends on 13)

A process for hydrolyzing a polylactide resin, comprising immersing a polylactide composition of claim 13 in liquid water at a temperature of 25° C.to 80° C.

### Claim 16 (depends on 13)

A process for hydrolyzing a polylactide resin, comprising contacting the polylactide composition of claim 13 in air having relative humidity of at least 50% at a temperature of 35° C. to 80° C.

### Claim 17 (depends on 1)

A method for treating a subterranean formation comprising a) introducing a treatment fluid containing a liquid phase and particles of the polylactide composition of claim 1 into the subterranean formation, such that a mass of the particles is deposited in the subterranean formation, and then b) hydrolyzing the deposited particles in the subterranean formation by exposing the deposited particles to an aqueous medium and an elevated temperature such that the deposited particles lose at least 50% of their starting mass due to hydrolysis.