# US 2024/0174795 A1 · High-Viscosity Biodegradable Aliphatic-Aromatic Polyester Copolymer Having Excellent Hydrolysis Resistance and Method of Preparing the Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0174795 A1
- Document ID: US20240174795A1
- Status: Published application
- Kind: A1
- Application number: 18/448,370
- Filed: 2023-08-11
- Published: 2024-05-30
- Earliest claimed: 2022-11-30
- Assignees: SK Innovation Co., Ltd.; SK Geo Centric Co., Ltd.; Kolon Industries, Inc.
- Applicants: SK Innovation Co., Ltd.; SK Geo Centric Co., Ltd.; Kolon Industries, Inc.
- Inventors: Do Young Kim; Hyun Sik Yang; Yu Hyun Kim; Ki Yup Kim; Joo Hyun Nam; Chul Soon Moon; Ji Hae Park; Sung Won Lee; Jun Haeng Lee; Ho Seung Lee
- Web page: https://patentgrep.com/patent/US20240174795A1

## CPC

- C08G 63/183: Terephthalic acids
- C08G 63/52: Polycarboxylic acids or polyhydroxy compounds in which at least one of the two components contains aliphatic unsaturation
- C08G 63/6856: {Dicarboxylic acids and dihydroxy compounds}
- C08G 63/785: {characterised by the apparatus used}
- C08G 63/916: {Dicarboxylic acids and dihydroxy compounds}
- C08K 5/29: Compounds containing {one or more} carbon-to-nitrogen double bonds
- C08L 67/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds (C08L67/06 takes precedence)
- C08G 2230/00: Compositions for preparing biodegradable polymers
- C08L 101/16: the macromolecular compounds being biodegradable
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

Provided are a biodegradable aliphatic-aromatic polyester copolymer having excellent hydrolysis resistance and high viscosity which has a carboxyl end group (CEG) content of 15 mg KOH/g or less, a ratio (Mz/Mn) of a z-average molecular weight (Mz) to a number average molecular weight (Mn) of 3 to 15, and a melt index (MI) of 5 g/10 min or less as measured under conditions of a temperature of 190° C. and a load of 2.16 kg in accordance with ASTM D 1238. A method of preparing a biodegradable aliphatic-aromatic polyester copolymer is provided, including adding a chain extender and an anti-hydrolysis agent to an aliphatic-aromatic polyester pre-copolymer over time, whereby a significant viscosity rise and improvement of hydrolysis resistance may be implemented simultaneously.

## Claims

### Claim 1

A method of preparing a biodegradable aliphatic-aromatic polyester copolymer, the method comprising:
(S1) adding an aliphatic-aromatic polyester pre-copolymer to a reactor;
(S2) adding a chain extender to the reactor comprising the aliphatic-aromatic polyester pre-copolymer to prepare a chain extended aliphatic-aromatic polyester pre-copolymer by a first polyaddition reaction of the aliphatic-aromatic polyester pre-copolymer and the chain extender; and
(S3) adding an anti-hydrolysis agent to the reactor comprising the chain extended aliphatic-aromatic polyester pre-copolymer to prepare the biodegradable aliphatic-aromatic polyester copolymer by a second reaction of the chain extended aliphatic-aromatic polyester pre-copolymer and the anti-hydrolysis agent.

### Claim 2 (depends on 1)

The method of preparing a biodegradable aliphatic-aromatic polyester copolymer of claim 1, wherein the first reaction of step (S2) is performed at 150 to 250° C.

### Claim 3 (depends on 1)

The method of preparing a biodegradable aliphatic-aromatic polyester copolymer of claim 1, wherein the first reaction of step (S2) is performed for 10 to 30 minutes.

### Claim 4 (depends on 1)

The method of preparing a biodegradable aliphatic-aromatic polyester copolymer of claim 1, wherein the second reaction of step (S3) is performed at 180 to 280° C.

### Claim 5 (depends on 1)

The method of preparing a biodegradable aliphatic-aromatic polyester copolymer of claim 1, wherein the second reaction of step (S3) is performed for 2 to 15 minutes.

### Claim 6 (depends on 1)

The method of preparing a biodegradable aliphatic-aromatic polyester copolymer of claim 1, wherein a ratio of the second reaction time of step (S3) to the first reaction time of step (S2) satisfies 0.1 to 0.5.

### Claim 7 (depends on 1)

The method of preparing a biodegradable aliphatic-aromatic polyester copolymer of claim 1, wherein the chain extender comprises a diisocyanate compound.

### Claim 8 (depends on 1)

The method of preparing a biodegradable aliphatic-aromatic polyester copolymer of claim 1, wherein the chain extender is comprised at 0.1 to 1 part by weight with respect to 100 parts by weight of the aliphatic-aromatic polyester pre-copolymer.

### Claim 9 (depends on 1)

The method of preparing a biodegradable aliphatic-aromatic polyester copolymer of claim 1, wherein the anti-hydrolysis agent comprises a carbodiimide compound.

### Claim 10 (depends on 1)

The method of preparing a biodegradable aliphatic-aromatic polyester copolymer of claim 1, wherein the anti-hydrolysis agent is comprised at 0.01 to 0.5 parts by weight with respect to 100 parts by weight of the aliphatic-aromatic polyester pre-copolymer.

### Claim 11 (depends on 1)

The method of preparing a biodegradable aliphatic-aromatic polyester copolymer of claim 1, wherein a weight ratio of the anti-hydrolysis agent to the chain extender satisfies 0.1 to 1.

### Claim 12 (depends on 1)

The method of preparing a biodegradable aliphatic-aromatic polyester copolymer of claim 1, wherein the aliphatic-aromatic polyester pre-copolymer has a melt index (MI) of 20 g/10 min or more as measured under conditions of a temperature of 190° C. and a load of 2.16 kg in accordance with ASTM D 1238.

### Claim 13 (depends on 1)

The method of preparing a biodegradable aliphatic-aromatic polyester copolymer of claim 1, wherein a ratio (Mz/Mzi) of a z-average molecular weight of the biodegradable aliphatic-aromatic polyester copolymer (Mz) to the z-average molecular weight aliphatic-aromatic polyester pre-copolymer (Mzi) is 1.5 to 3.5.

### Claim 14

A biodegradable aliphatic-aromatic polyester copolymer which has a carboxyl end group (CEG) content of 15 mg KOH/g or less, a ratio (Mz/Mn) of a z-average molecular weight (Mz) to a number average molecular weight (Mn) of 3 to 15, and a melt index (MI) of 5 g/10 min or less as measured under conditions of a temperature of 190° C. and a load of 2.16 kg in accordance with ASTM D 1238.

### Claim 15 (depends on 14)

The biodegradable aliphatic-aromatic polyester copolymer of claim 14, wherein the biodegradable aliphatic-aromatic polyester copolymer has a weight average molecular weight (Mw) of 120,000 g/mol to 250,000 g/mol.

### Claim 16 (depends on 15)

The biodegradable aliphatic-aromatic polyester copolymer of claim 15, wherein the biodegradable aliphatic-aromatic polyester copolymer has the z-average molecular weight (Mz) of 250,000 g/mol to 900,000 g/mol.

### Claim 17 (depends on 14)

The biodegradable aliphatic-aromatic polyester copolymer of claim 14, wherein the biodegradable aliphatic-aromatic polyester copolymer has a ratio (Mz/Mw) of the z-average molecular weight (Mz) to the weight average molecular weight (Mw) of 2 to 7.

### Claim 18 (depends on 14)

The biodegradable aliphatic-aromatic polyester copolymer of claim 14, wherein the biodegradable aliphatic-aromatic polyester copolymer is one or a combination of two or more selected from the group consisting of polybutylene adipate terephthalate (PBAT), polybutylene succinate butylene terephthalate (PBAST), polybutylene sebacate terephthalate (PBSeT) and mixtures thereof.

### Claim 19

A method for reducing greenhouse gas emissions by preparing a biodegradable aliphatic-aromatic polyester copolymer, the method comprising:
(S1) adding an aliphatic-aromatic polyester pre-copolymer to a reactor;
(S2) adding a chain extender to the reactor comprising the aliphatic-aromatic polyester pre-copolymer to prepare a chain extended aliphatic-aromatic polyester pre-copolymer by a first polyaddition reaction of the aliphatic-aromatic polyester pre-copolymer and the chain extender; and
(S3) adding an anti-hydrolysis agent to the reactor comprising the chain extended aliphatic-aromatic polyester pre-copolymer to prepare the biodegradable aliphatic-aromatic polyester copolymer by a second reaction of the chain extended aliphatic-aromatic polyester pre-copolymer and the anti-hydrolysis agent.