# US 2024/0174551 A1 · Ion exchangeable glass compositions having improved mechanical durability

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0174551 A1
- Document ID: US20240174551A1
- Status: Published application
- Kind: A1
- Application number: 18/517,504
- Filed: 2023-11-22
- Published: 2024-05-30
- Earliest claimed: 2022-11-28
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Xiaoju Guo; Peter Joseph Lezzi; Jian Luo
- Web page: https://patentgrep.com/patent/US20240174551A1

## CPC

- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 2203/10: Melting processes
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A glass composition includes: from 55 mol % to 70 mol % SiO2; from 12.5 mol % to 17.25 mol % Al2O3; from 0.1 mol % to 3.5 mol % P2O5; from 0 mol % to 5.5 mol % B2O3; from 6 mol % to 10 mol % Li2O; from 3 mol % to 10 mol % Na2O; from 0 mol % to 3 mol % TiO2; from 0 mol % to 3 mol % WO3; and from 0 mol % to 3 mol % Y2O3. The sum of Al2O3 and B2O3 in the glass composition may be from 12.5 mol % to 22.5 mol %. The sum of TiO2, WO3, and Y2O3 in the glass composition may be from 0.2 mol % to 3 mol %.

## Claims

### Claim 1

A glass composition comprising:
greater than or equal to 55 mol % and less than or equal to 70 mol % SiO2;
greater than or equal to 12.5 mol % and less than or equal to 17.25 mol % Al2O3;
greater than or equal to 0.1 mol % and less than or equal to 3.5 mol % P2O5;
greater than or equal to 0 mol % and less than or equal to 5.5 mol % B2O3;
greater than or equal to 6 mol % and less than or equal to 10 mol % Li2O;
greater than or equal to 3 mol % and less than or equal to 10 mol % Na2O;
greater than or equal to 0 mol % and less than or equal to 3 mol % TiO2;
greater than or equal to 0 mol % and less than or equal to 3 mol % WO3; and
greater than or equal to 0 mol % and less than or equal to 3 mol % Y2O3, wherein
Al2O3+B2O3 is greater than or equal to 12.5 mol % and less than or equal to 22.5 mol %, and
TiO2+WO3+Y2O3 is greater than or equal to 0.2 mol % and less than or equal to 3 mol %.

### Claim 2 (depends on 1)

The glass composition of claim 1, wherein TiO2+WO3+Y2O3 is greater than or equal to 0.4 mol % and less than or equal to 3 mol %.

### Claim 3 (depends on 1)

The glass composition of claim 1, wherein Al2O3+B2O3 is greater than or equal to 13.5 mol % and less than or equal to 21.5 mol %.

### Claim 4 (depends on 1)

The glass composition of claim 1, wherein the glass composition comprises greater than or equal to 0.1 mol % and less than or equal to 5.25 mol % B2O3.

### Claim 5 (depends on 1)

The glass composition of claim 1, wherein the glass composition comprises greater than or equal to 13 mol % and less than or equal to 17 mol % Al2O3.

### Claim 6 (depends on 1)

The glass composition of claim 1, wherein R2O is greater than or equal to 9 mol % and less than or equal to 20 mol %, R2O being the sum of Li2O, Na2O, and K2O.

### Claim 7 (depends on 1)

The glass composition of claim 1, wherein the glass composition comprises greater than 0 mol % and less than or equal to 1 mol % K2O.

### Claim 8 (depends on 1)

The glass composition of claim 1, wherein the glass composition comprises greater than 0 mol % and less than or equal to 3 mol % TiO2.

### Claim 9 (depends on 1)

The glass composition of claim 1, wherein the glass composition comprises greater than 0 mol % and less than or equal to 3 mol % WO3.

### Claim 10 (depends on 1)

The glass composition of claim 1, wherein the glass composition comprises greater than 0 mol % and less than or equal to 3 mol % Y2O3.

### Claim 11 (depends on 1)

The glass composition of claim 1, wherein the glass composition has a KIc fracture toughness as measured by a chevron notch short bar method greater than or equal to 0.7 MPa·m1/2.

### Claim 12

A glass article comprises:
greater than or equal to 55 mol % and less than or equal to 70 mol % SiO2;
greater than or equal to 12.5 mol % and less than or equal to 17.25 mol % Al2O3;
greater than or equal to 0.1 mol % and less than or equal to 3.5 mol % P2O5;
greater than or equal to 0 mol % and less than or equal to 5.5 mol % B2O3;
greater than or equal to 6 mol % and less than or equal to 10 mol % Li2O;
greater than or equal to 3 mol % and less than or equal to 10 mol % Na2O;
greater than or equal to 0 mol % and less than or equal to 3 mol % TiO2;
greater than or equal to 0 mol % and less than or equal to 3 mol % WO3; and
greater than or equal to 0 mol % and less than or equal to 3 mol % Y2O3, wherein
Al2O3+B2O3 is greater than or equal to 12.5 mol % and less than or equal to 22.5 mol %, and
TiO2+WO3+Y2O3 is greater than or equal to 0.2 mol % and less than or equal to 3 mol %.

### Claim 13 (depends on 12)

The glass article of claim 12, wherein TiO2+WO3+Y2O3 is greater than or equal to 0.4 mol % and less than or equal to 3 mol %.

### Claim 14 (depends on 12)

The glass article of claim 12, wherein Al2O3+B2O3 is greater than or equal to 13.5 mol % and less than or equal to 21.5 mol %.

### Claim 15 (depends on 12)

The glass article of claim 12, wherein the glass article comprises greater than or equal to 0.1 mol % and less than or equal to 5.25 mol % B2O3.

### Claim 16 (depends on 12)

The glass article of claim 12, wherein the glass article comprises greater than or equal to 13 mol % and less than or equal to 17 mol % Al2O3.

### Claim 17 (depends on 12)

The glass article of claim 12, wherein R2O is greater than or equal to 9 mol % and less than or equal to 20 mol %, R2O being the sum of Li2O, Na2O, and K2O.

### Claim 18 (depends on 12)

The glass article of claim 12, wherein the glass article is an ion exchanged glass article.

### Claim 19 (depends on 18)

The glass article of claim 18, wherein the ion exchanged glass article comprises a peak surface compressive stress greater than or equal to 450 MPa, a depth of layer greater than or equal to 5 μm, and a maximum central tension greater than or equal to 50 MPa, as measured at an article thickness of 0.8 mm.

### Claim 20

A method of forming a glass article, the method comprising:
heating a glass composition, the glass composition comprising:
greater than or equal to 55 mol % and less than or equal to 70 mol % SiO2;
greater than or equal to 12.5 mol % and less than or equal to 17.25 mol % Al2O3;
greater than or equal to 0.1 mol % and less than or equal to 3.5 mol % P2O5;
greater than or equal to 0 mol % and less than or equal to 5.5 mol % B2O3;
greater than or equal to 6 mol % and less than or equal to 10 mol % Li2O;
greater than or equal to 3 mol % and less than or equal to 10 mol % Na2O;
greater than or equal to 0 mol % and less than or equal to 3 mol % TiO2;
greater than or equal to 0 mol % and less than or equal to 3 mol % WO3; and
greater than or equal to 0 mol % and less than or equal to 3 mol % Y2O3, wherein
Al2O3+B2O3 is greater than or equal to 12.5 mol % and less than or equal to 22.5 mol %, and
TiO2+WO3+Y2O3 is greater than or equal to 0.2 mol % and less than or equal to 3 mol %; and
cooling the glass composition to form the glass article.