# US 2024/0166776 A1 · Use of proton-form zeolite catalyst to produce light-polyisobutylene

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0166776 A1
- Document ID: US20240166776A1
- Status: Published application
- Kind: A1
- Application number: 18/517,947
- Filed: 2023-11-22
- Published: 2024-05-23
- Earliest claimed: 2022-11-23
- Assignees: Braskem S.A.
- Applicants: Braskem S.A.
- Inventors: Richard Caulkins; Jiahan Xie; Alicia Brasselle; Richard Opfer; Dan Xie; Maria Giuliana Torraga Uchiyama; Marcio Henrique Dos Santos Andrade; João Capistrano Nobre De Abreu; Danniel Panza; Mauricio Silveira Cadore; Suzana Kupidlowski Boaventura; Jan Kalfus
- Web page: https://patentgrep.com/patent/US20240166776A1

## CPC

- C07C 2/12: with crystalline alumino-silicates {or with catalysts comprising} molecular sieves
- C08F 10/10: Isobutene
- C08F 4/12: of boron, aluminium, gallium, indium, thallium or rare earths
- C07C 2529/08: of the faujasite type, e.g. type X or Y
- C07C 2531/08: Ion-exchange resins
- C08F 2410/06: Catalyst characterized by its size
- C08F 2500/02: Low molecular weight, e.g. <100,000 Da.
- C08F 2500/17: Viscosity
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

A method of forming a light-polyisobutylene may include polymerizing isobutene or an isobutene-containing monomer mixture in presence of a proton-form zeolite catalyst to form a light-polyisobutylene. A light-polyisobutylene may be formed by the method of polymerizing isobutene or an isobutene-containing monomer mixture in presence of a proton-form zeolite catalyst.

## Claims

### Claim 1

A method of forming a light-polyisobutylene, comprising:
polymerizing isobutene or an isobutene-containing monomer mixture in presence of a proton-form zeolite catalyst to form a light-polyisobutylene.

### Claim 2 (depends on 1)

The method of claim 1, wherein the light-polyisobutylene has a viscosity of 3-120 cst at 37.8° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the light-polyisobutylene has a viscosity of 0.5-120 cst at 37.8° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the light-polyisobutylene has a formula (IB)n where n ranges from 2 to 9 and has a molecular weight (Mn) ranging from 110-500 g/mol.

### Claim 5 (depends on 4)

The method of claim 4, wherein n ranges from 4 to 8.

### Claim 6 (depends on 1)

The method of claim 1, wherein the light-polyisobutylene has a polydispersity index of less than 1.2.

### Claim 7 (depends on 1)

The method of claim 1, wherein the proton-form zeolite catalyst is a crystalline microporous aluminosilicate.

### Claim 8 (depends on 7)

The method of claim 7, wherein the microporous aluminosilicate has a pore size greater than 4.85 angstrom.

### Claim 9 (depends on 1)

The method of claim 1, further comprising:
calcining a zeolite catalyst to form the proton-form zeolite catalyst.

### Claim 10 (depends on 9)

The method of claim 9, wherein the zeolite catalyst comprises ferrierite (FER), mordenite (MOR), tschernichite (BEA), faujasite (FAU) or any other zeolite with pore size greater than 4.85 Angstrom.

### Claim 11 (depends on 10)

The method of claim 10, wherein the zeolite catalyst has a framework selected from the group consisting of AET, AFI, AFO, AFR, AFS, AFY, ATO, ATS, BEC, Boggsite (BOG), BOZ, BPH, CAN, CFI, CON, CSV, CTH, DFO, DON, EMT, EON, ETR, EUO, EZT, GME, GON, IFO, IFR, IFW, IMF, IRR, ISV, ITG, ITH, ITR, ITT, IWR, IWS, IWV, IWW, JSR, LTF, LTL, MAZ, MEI, MEL, MFS, MOZ, MSE, MTT, MTW, MWW, NES, OBW, OFF, OKO, OSI, OSO, PCS, POS, RWY, SAF, SAO, SBE, SBS, SBT, SEW, SFE, SFF, SFG, SFH, SFN, SFO, SFS, SOR, SOV, SSF, SSY, STF, STI, STW, SVY, SYT, TER, TON, TUN, UOV, USI, UTL, UWY, VET, VFI, and YFI.

### Claim 12 (depends on 9)

The method of claim 9, wherein the calcining occurs at a temperature ranging between 400 and 600° C.

### Claim 13 (depends on 9)

The method of claim 9, wherein the calcining occurs for a time ranging between 4 and 18 h.

### Claim 14 (depends on 1)

A light-polyisobutylene formed by the method of claim 1.