# US 2024/0158681 A1 · Metal nitrate based compositions for use as phase change materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0158681 A1
- Document ID: US20240158681A1
- Status: Published application
- Kind: A1
- Application number: 18/395,418
- Filed: 2023-12-22
- Published: 2024-05-16
- Earliest claimed: 2021-04-06
- Assignees: Sunamp Limited
- Applicants: Sunamp Limited
- Inventors: Andrew John BISSELL; David OLIVER; Colin Richard PULHAM; Emily Jane GODDARD; Gylen ODLING; Kate FISHER
- Web page: https://patentgrep.com/patent/US20240158681A1

## CPC

- C09K 5/063: {Materials absorbing or liberating heat during crystallisation; Heat storage materials}
- Y02E 60/14: Thermal energy storage
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

There is disclosed herein metal nitrate hydrates as phase change materials (PCMs). More particularly, there is disclosed herein metal nitrate hydrate PCMs containing group II metal nitrates as nucleation agents. A further disclosure herein is the combination of multiple chemical species in the PCM formulation which act together to induce nucleation of metal nitrate PCMs. Furthermore, physical mechanisms by which nucleation of metal nitrate hydrate based PCMs and crystallisation rate increased are disclosed.

## Claims

### Claim 1

A method of preparing a phase-change material (PCM) composition, comprising:
heating a mixture of metal nitrate components consisting essentially of calcium nitrate tetrahydrate, a nucleation agent, and, optionally, copper nitrate, zinc nitrate, iron nitrate, or a hydrate thereof, above a melting transition temperature of one or more of the metal nitrate components and mixing to form the PCM composition as a single pourable liquid,
wherein the nucleation agent consists essentially of a mixture of magnesium nitrate or a hydrate thereof, and/or strontium nitrate or a hydrate thereof; and
wherein an anhydrous metal nitrate and/or a metal nitrate hydrate of a lower hydration number than is present in the PCM composition is used in place of one or more metal nitrate hydrate(s) forming the composition, and
wherein the method also comprises an addition of water to form a final PCM composition.

### Claim 2

A method of preparing a phase-change material (PCM) composition, comprising:
heating a mixture of metal nitrate components consisting essentially of calcium nitrate tetrahydrate, a nucleation agent, and, optionally, copper nitrate, zinc nitrate, iron nitrate, or a hydrate thereof, above a melting transition temperature of one or more of the metal nitrate components and mixing to form the PCM composition as a single pourable liquid,
wherein the nucleation agent consists essentially of a mixture of magnesium nitrate or a hydrate thereof, and/or strontium nitrate or a hydrate thereof;
wherein a metal nitrate hydrate with a higher hydration number than is present in the PCM composition is used in place of one or more metal nitrate hydrate(s) forming the final PCM composition.

### Claim 3 (depends on 2)

The method of claim 2, wherein the final PCM composition is further formed by removing excess water by heating the composition.

### Claim 4 (depends on 2)

The method of claim 2, wherein the final PCM composition is further formed by exposing the composition to reduced pressure.

### Claim 5 (depends on 2)

The method of claim 2, wherein the final PCM composition is further formed by an addition of one or more anhydrous metal nitrates to the combination, or an addition of one or more anhydrous metal nitrate salts to the combination.

### Claim 6

A method of preparing a phase-change material (PCM) composition, comprising:
heating a mixture of metal nitrate components consisting essentially of calcium nitrate tetrahydrate, a nucleation agent, and, optionally, copper nitrate, zinc nitrate, iron nitrate, or a hydrate thereof above a melting transition temperature of one or more of the metal nitrate components and mixing to form the PCM composition as a single pourable liquid,
wherein the nucleation agent consists essentially of a mixture of magnesium nitrate or a hydrate thereof, and/or strontium nitrate or a hydrate thereof,
wherein a metal nitrate solution is used in place of one or more metal nitrate hydrate(s) forming a final PCM composition;
wherein the forming the final PCM composition further includes:
i) removing excess water by heating the composition;
ii) exposing the composition to reduced pressure;
iii) an addition of one or more anhydrous metal nitrates to the combination;
iv) an addition of one or more anhydrous metal nitrate salts to the combination; or
v) a combination thereof.

### Claim 7

A method of preparing a phase-change material (PCM) composition, comprising:
heating a mixture of metal nitrate components consisting essentially of calcium nitrate tetrahydrate, a nucleation agent, and, optionally, copper nitrate, zinc nitrate, iron nitrate, or a hydrate thereof above a melting transition temperature of one or more of the metal nitrate components and mixing to form the PCM composition as a single pourable liquid,
wherein the nucleation agent consists essentially of a mixture of: magnesium nitrate or a hydrate thereof, and/or strontium nitrate or a hydrate thereof; and
wherein one or more of the metal nitrate and/or metal nitrate hydrates is produced by reaction.

### Claim 8 (depends on 7)

The method of claim 7, wherein the reaction is neutralization of nitric acid by the corresponding basic metal salt in the presence of the correct amount of water to achieve the PCM composition.

### Claim 9 (depends on 7)

The method of claim 7, wherein the reaction is neutralization of nitric acid by the corresponding metal bases in the presence of excess water relative to the PCM composition.

### Claim 10 (depends on 9)

The method of claim 9, wherein the final PCM composition is further formed by removing excess water by heating the composition.

### Claim 11 (depends on 9)

The method of claim 9, wherein the final PCM composition is further formed by exposing the composition to reduced pressure.

### Claim 12 (depends on 9)

The method of claim 9, wherein the final PCM composition is further formed by an addition of one or more anhydrous metal nitrates to the combination, or an addition of one or more anhydrous metal nitrate salts to the combination.

### Claim 13

A method of preparing a phase-change material (PCM) composition, comprising:
heating a mixture of metal nitrate components consisting essentially of calcium nitrate tetrahydrate, a nucleation agent, and, optionally, copper nitrate, zinc nitrate, iron nitrate, or a hydrate thereof above a melting transition temperature of one or more of the metal nitrate components and mixing to form the PCM composition as a single pourable liquid,
wherein the nucleation agent consists essentially of a mixture of magnesium nitrate or a hydrate thereof, and/or strontium nitrate or a hydrate thereof; and
wherein any anion other than nitrate is removed by ion exchange, or precipitation with an appropriate metal salt followed by physical separation.