# US 2024/0157676 A1 · Building boards with increased surface strength

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0157676 A1
- Document ID: US20240157676A1
- Status: Published application
- Kind: A1
- Application number: 18/419,682
- Filed: 2024-01-23
- Published: 2024-05-16
- Earliest claimed: 2013-12-30
- Assignees: Saint-Gobain Placo
- Applicants: Saint-Gobain Placo SAS
- Inventors: Robin Daniel Fisher; Devang Umesh Khariwala; Jeffrey Hamilton Peet; Peter Mayer
- Web page: https://patentgrep.com/patent/US20240157676A1

## CPC

- B32B 13/08: of paper or cardboard
- E04C 2/043: {of plaster (E04C2/049 takes precedence)}
- B32B 2255/12: on paper layer
- B32B 2255/26: Polymeric coating
- B32B 2307/54: Yield strength; Tensile strength
- B32B 2419/00: Buildings or parts thereof
- B32B 2607/00: Walls, panels
- Y10T 428/24488: Differential nonuniformity at margin
- Y10T 428/24496: Foamed or cellular component
- Y10T 428/24612: Composite web or sheet
- Y10T 428/249968: Of hydraulic-setting material
- Y10T 428/273: of coating
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- E04C: STRUCTURAL ELEMENTS; BUILDING MATERIALS (for bridges E01D; specially designed for insulation or other protection E04B; elements used as building aids E04G; for mining E21; for tunnels E21D; structural elements with broader range of application than for building engineering F16, particularly F16S)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Disclosed is a building board construction with increased surface strength. More specifically, increased nail pull strength is achieved via the application of an external surface coating. The surface coating is ideally applied to a paper faced gypsum building board. In one possible embodiment, the coating is formed from a water soluble polymer.

## Claims

### Claim at position 1

1-42. (canceled)

### Claim 43

A gypsum-based building board with enhanced nail pull strength, the composite building board comprising:
first and second liners each having an interior face, the first liner comprising paper having an exterior face forming an outer face of the building board;
a set gypsum plaster core positioned between and bonded with the interior face of the first liner and the interior face of the second liner; and
a coating of a coating polymer on the exterior face of the first liner, the coating having a tensile modulus above 500 psi and an elongation at break of greater than 500% at room temperature and improving a nail pull strength of the building board relative to an identical building board without the coating.

### Claim 44 (depends on 43)

The gypsum-based building board according to claim 43, wherein the coating comprises less than 10 grams of coating polymer per square foot of the outer face.

### Claim 45 (depends on 43)

The gypsum-based building board according to claim 43, wherein the coating comprises in the range of 0.5-10 grams of coating polymer per square foot of the outer face.

### Claim 46 (depends on 43)

The gypsum-based building board according to claim 43, wherein the coating comprises less than 2 grams of coating polymer per square foot of the outer face and the nail pull strength is greater than 10% higher than an identical building board without the polymer-based spray coating.

### Claim 47 (depends on 43)

The gypsum-based building board according to claim 43, wherein the coating polymer comprises a polymer selected from acrylics and acrylic copolymers, vinyl acetate polymers and copolymers, styrene-butadiene polymers and copolymers, and polyvinyl alcohols.

### Claim 48 (depends on 43)

The gypsum-based building board according to claim 43, wherein the coating polymer comprises one of the following:
a copolymer containing vinyl acetate and ethylene;
a copolymer containing styrene and butadiene; or
a poly vinyl alcohol.

### Claim 49 (depends on 43)

The gypsum-based building board according to claim 43, wherein the coating polymer has a glass transition temperature below 30 degrees Celsius.

### Claim 50 (depends on 43)

The gypsum-based building board according to claim 43, wherein the coating polymer has a glass transition temperature above 5 degrees Celsius and below 25 degrees Celsius.

### Claim 51 (depends on 43)

The gypsum-based building board according to claim 43, wherein the coating is less than 100 microns thick.

### Claim 52 (depends on 43)

The gypsum-based building board according to claim 43, wherein the coating is in the range of 10-100 microns in thickness.

### Claim 53 (depends on 43)

The gypsum-based building board according to claim 43, wherein the coating is less than 50 microns thick.

### Claim 54 (depends on 43)

The gypsum-based building board according to claim 43, wherein the coating polymer has an elongation at break greater than 500% and up to 10,000%.

### Claim 55 (depends on 43)

The gypsum-based building board according to claim 43, wherein the coating polymer has a tensile modulus above 500 psi and up to 10,000 psi.

### Claim 56 (depends on 43)

The gypsum-based building board according to claim 43, wherein the coating polymer has an elongation at break of between greater than 500% and up to 10,000% and a tensile modulus above 500 psi and up to 10,000 psi.

### Claim 57 (depends on 56)

The gypsum-based building board according to claim 56, wherein the coating polymer comprises at least one of the following:
a copolymer containing vinyl acetate and ethylene;
a copolymer containing styrene and butadiene;
or a poly vinyl alcohol.

### Claim 58 (depends on 43)

The gypsum-based building board according to claim 43, wherein the coating polymer comprises one of the following:
a copolymer containing styrene and butadiene; and
a poly vinyl alcohol.

### Claim 59 (depends on 43)

The gypsum-based building board according to claim 43, wherein the coating is a spray coating.

### Claim 60

A gypsum-based building board with enhanced nail pull strength, the gypsum-based building board comprising:
an exterior paper face forming an outer face of the building board;
a set gypsum plaster core positioned beneath the exterior paper face; and
a coating of a coating polymer on an outer surface of the exterior paper face of the building board, the coating having a tensile modulus above 500 psi and an elongation at break of greater than 500% at room temperature and improving a nail pull strength of the building board relative to an identical building board without the coating by at least 10%.

### Claim 61 (depends on 60)

The gypsum-based building board according to claim 60, wherein the coating comprises in the range of 0.5-10 grams of polymer per square foot of the outer face.

### Claim 62 (depends on 60)

The gypsum-based building board according to claim 60, wherein the coating polymer comprises a polymer selected from acrylics and acrylic copolymers, vinyl acetate polymers and copolymers, styrene-butadiene polymers and copolymers, and polyvinyl alcohols.