# US 2024/0157511 A1 · Method of manufacturing composite article

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0157511 A1
- Document ID: US20240157511A1
- Status: Published application
- Kind: A1
- Application number: 18/422,028
- Filed: 2024-01-25
- Published: 2024-05-16
- Earliest claimed: 2018-10-31
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company Ltd.
- Inventors: HUA-CHOU CHIANG; CHANDLER YING LAI SEE; CHUNG-CHIEH KO
- Web page: https://patentgrep.com/patent/US20240157511A1

## CPC

- B27N 3/007: {and at least partly composed of recycled material}
- B24B 29/02: designed for particular workpieces
- B24B 37/04: designed for working plane surfaces
- B24B 37/042: {operating processes therefor}
- B24B 37/10: for single side lapping
- B24B 47/12: by mechanical gearing or electric power (B24B47/16 takes precedence)
- B24B 53/017: Devices or means for dressing, cleaning or otherwise conditioning lapping tools
- B24B 55/12: Devices for exhausting mist of oil or coolant; Devices for collecting or recovering materials resulting from grinding or polishing, e.g. of precious metals, precious stones, diamonds or the like
- B27N 3/08: Moulding or pressing (presses in general B30B)
- H10P 52/00: Grinding, lapping or polishing of wafers, substrates or parts of devices
- H10P 52/403: {of conductive or resistive materials}
- H10P 72/00: Handling or holding of wafers, substrates or devices during manufacture or treatment thereof
- Y02P 80/30: Reducing waste in manufacturing processes; Calculations of released waste quantities
- B27N: MANUFACTURE BY DRY PROCESSES OF ARTICLES, WITH OR WITHOUT ORGANIC BINDING AGENTS, MADE FROM PARTICLES OR FIBRES CONSISTING OF WOOD OR OTHER LIGNOCELLULOSIC OR LIKE ORGANIC MATERIAL (containing cementitious material B28B; shaping of substances in a plastic state B29C; fibreboards made from fibrous suspensions D21J; drying F26B17/00)
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method of manufacturing a composite article includes providing a polishing pad; rubbing over the polishing pad to produce a polishing pad debris; collecting the polishing pad debris; providing a wood material; and applying a force over the wood material and the polishing pad debris to form the composite article, wherein the composite article includes the wood material and the polishing pad debris, and the rubbing of the polishing pad includes removing a portion of the polishing pad to produce the polishing pad debris.

## Claims

### Claim 1

A method of manufacturing a composite article, comprising:
rubbing a polishing pad to produce polishing pad debris;
collecting the polishing pad debris;
providing a wood material; and
applying a force over the wood material and the polishing pad debris to form the composite article including the wood material and the polishing pad debris.

### Claim 2 (depends on 1)

The method of claim 1, wherein the rubbing of the polishing pad includes grinding a semiconductor structure by the polishing pad.

### Claim 3 (depends on 2)

The method of claim 2, wherein the semiconductor structure is a substrate or a wafer.

### Claim 4 (depends on 1)

The method of claim 1, wherein the polishing pad and the polishing pad debris include polyurethane (PU).

### Claim 5 (depends on 1)

The method of claim 1, wherein a thickness of the polishing pad is reduced by the rubbing of the polishing pad.

### Claim 6 (depends on 1)

The method of claim 1, wherein the rubbing of the polishing pad includes removing a portion of the polishing pad.

### Claim 7 (depends on 1)

The method of claim 1, wherein a first content of the polishing pad debris in the composite article is less than a second content of the wood material in the composite article.

### Claim 8 (depends on 7)

The method of claim 7, wherein a ratio of the first content to the second content is about 3:7.

### Claim 9 (depends on 1)

The method of claim 1, wherein the application of the force includes compressing the wood material and the polishing pad debris to form the composite article.

### Claim 10 (depends on 1)

The method of claim 1, further comprising assembling the composite article with a plurality of wooden bars to form a pallet.

### Claim 11 (depends on 1)

The method of claim 1, wherein the composite article is in a block configuration.

### Claim 12

A method of manufacturing a composite article, comprising:
providing a polishing pad;
providing a semiconductor structure disposed above the polishing pad;
polishing the semiconductor structure by the polishing pad;
collecting polishing pad debris produced upon the polishing;
providing a wood material; and
compressing the wood material and the polishing pad debris to form the composite article,
wherein the polishing pad debris includes a portion of the polishing pad removed from the polishing pad upon the polishing.

### Claim 13 (depends on 12)

The method of claim 12, wherein the polishing pad debris is cleaned prior to the compression.

### Claim 14 (depends on 12)

The method of claim 12, further comprising:
providing a plurality of wooden bars arranged substantially in parallel to each other;
attaching the composite article to an end of one of the plurality of wooden bars.

### Claim 15 (depends on 12)

The method of claim 12, wherein the semiconductor structure is rotated relative to the polishing pad during the polishing.

### Claim 16 (depends on 12)

The method of claim 12, wherein the polishing pad is rotated relative to the semiconductor structure during the polishing.

### Claim 17 (depends on 12)

The method of claim 12, wherein the semiconductor structure and the polishing pad are rotated simultaneously during the polishing.

### Claim 18

A method of manufacturing a composite article, comprising:
rubbing a semiconductor structure by a polishing pad to produce debris, wherein the debris includes polishing pad debris and semiconductor structure debris;
cleaning the debris;
providing a wood material; and
applying a force over the wood material and the debris after the cleaning to form the composite article.

### Claim 19 (depends on 18)

The method of claim 18, wherein the cleaning of the debris includes removing the semiconductor structure debris from the debris.

### Claim 20 (depends on 18)

The method of claim 18, wherein the semiconductor structure debris in the debris after the cleaning is almost absent.