# US 2024/0150900 A1 · Cavitation corrosion resistant damping composite metal material structure of cross-flow component and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0150900 A1
- Document ID: US20240150900A1
- Status: Published application
- Kind: A1
- Application number: 18/386,662
- Filed: 2023-11-03
- Published: 2024-05-09
- Earliest claimed: 2022-11-03
- Assignees: Hohai University
- Applicants: Hohai University
- Inventors: Hongbing YAO; Yuanhang ZHOU; Wenlong LI; Wenjie SHI; Wei SU; Jiang YUE; Xiang HE; Yuanyuan XIANG; Weihua ZHU
- Web page: https://patentgrep.com/patent/US20240150900A1

## CPC

- C23C 24/103: {Coating with metallic material, i.e. metals or metal alloys, optionally comprising hard particles, e.g. oxides, carbides or nitrides}
- B23K 26/356: by shock processing
- B23K 26/362: Laser etching
- B32B 3/00: Layered products comprising a layer with external or internal discontinuities or unevennesses, or a layer of non-planar shape; Layered products comprising a layer having particular features of form
- B32B 3/02: characterised by features of form at particular places, e.g. in edge regions {(non-uniform thickness B32B3/263)}
- B32B 3/06: for securing layers together; for attaching the product to another member, e.g. to a support {, or to another product, e.g. groove/tongue, interlocking}
- B32B 3/10: characterised by a discontinuous layer, i.e. formed of separate pieces of material
- B32B 3/12: characterised by a layer of regularly- arranged cells, e.g. a honeycomb structure
- B32B 3/263: {characterised by a layer having non-uniform thickness}
- B32B 3/266: {characterised by an apertured layer, the apertures going through the whole thickness of the layer, e.g. expanded metal, perforated layer, slit layer regular cells B32B3/12}
- B32B 3/30: characterised by a layer formed with recesses or projections, e.g. {hollows, grooves, protuberances, ribs (apertured layer B32B3/266; layer with cavities or internal voids B32B3/26)}
- B32B 15/01: all layers being exclusively metallic {(making layered metal workpieces by pressure cladding B23K20/22; making coatings with a metallic material characterised by its composition C23C30/00)}
- B32B 15/017: {one layer being formed of aluminium or an aluminium alloy, another layer being formed of an alloy based on a non ferrous metal other than aluminium}
- B32B 15/04: comprising metal as the main or only constituent of a layer, {which is} next to another layer of {the same or of} a {different material (next to a bituminous or tarry layer B32B11/08; next to a water-setting substance layer B32B13/06; next to a glass layer B32B17/061; next to a cellulosic plastic layer B32B23/042)}
- B32B 15/043: {of metal (B32B15/01 takes precedence)}
- B32B 15/20: comprising aluminium or copper {(B32B15/016 and B32B15/017 take precedence)}
- C22C 19/002: {with copper as the next major constituent}
- C22C 19/03: based on nickel
- C22C 30/00: Alloys containing less than 50% by weight of each constituent
- C22C 32/0063: {based on SiC}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/44: with molybdenum or tungsten
- C22F 3/00: Changing the physical structure of non-ferrous metals or alloys by special physical methods, e.g. treatment with neutrons
- C23C 4/00: Coating by spraying the coating material in the molten state, e.g. by flame, plasma or electric discharge (build-up welding B23K, e.g. B23K5/18, B23K9/04)
- C23C 4/01: Selective coating, e.g. pattern coating, without pre-treatment of the material to be coated
- C23C 4/02: Pretreatment of the material to be coated, e.g. for coating on selected surface areas
- C23C 4/06: Metallic material
- C23C 4/067: containing free particles of non-metal elements, e.g. carbon, silicon, boron, phosphorus or arsenic
- C23C 4/08: containing only metal elements (C23C4/073 takes precedence)
- C23C 4/10: Oxides, borides, carbides, nitrides or silicides; Mixtures thereof
- C23C 4/11: Oxides
- C23C 4/18: After-treatment
- C23C 24/106: {Coating with metal alloys or metal elements only}
- C23C 28/021: {including at least one metal alloy layer}
- C23C 28/023: {only coatings of metal elements only}
- C23C 28/027: {including at least one metal matrix material comprising a mixture of at least two metals or metal phases or metal matrix composites, e.g. metal matrix with embedded inorganic hard particles, CERMET, MMC.}
- C23C 28/028: {Including graded layers in composition or in physical properties, e.g. density, porosity, grain size}
- C23C 28/04: only coatings of inorganic non-metallic material
- C23C 28/048: {with layers graded in composition or physical properties}
- C23C 28/30: {Coatings combining at least one metallic layer and at least one inorganic non-metallic layer}
- C23C 28/32: {including at least one pure metallic layer}
- C23C 28/321: {with at least one metal alloy layer}
- C23C 28/322: {only coatings of metal elements only}
- C23C 28/324: {with at least one metal matrix material layer comprising a mixture of at least two metals or metal phases or a metal-matrix material with hard embedded particles, e.g. WC-Me}
- C23C 28/325: {with layers graded in composition or in physical properties}
- C23C 28/36: {including layers graded in composition or physical properties}
- C23C 28/44: {characterized by a measurable physical property of the alternating layer or system, e.g. thickness, density, hardness}
- C23C 30/00: Coating with metallic material characterised only by the composition of the metallic material, i.e. not characterised by the coating process (C23C26/00, C23C28/00 take precedence)
- C23C 30/005: {on hard metal substrates}
- C23F 4/00: Processes for removing metallic material from surfaces, not provided for in group C23F1/00 or C23F3/00
- C23F 17/00: Multi-step processes for surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by subclass C21D or C22F or class C25 (coating for obtaining at least two superposed coatings either by methods not provided for in a single one of main groups C23C2/00 - C23C26/00, or by combinations of methods providedfor in subclasses C23C and C25D, C23C28/00)
- Y02P 10/25: Process efficiency
- Y10T 428/12451: Macroscopically anomalous interface between layers
- Y10T 428/12458: having composition, density, or hardness gradient
- Y10T 428/12472: Microscopic interfacial wave or roughness
- Y10T 428/12771: Transition metal-base component
- Y10T 428/12778: Alternative base metals from diverse categories
- Y10T 428/12903: Cu-base component
- Y10T 428/1291: Next to Co-, Cu-, or Ni-base component
- Y10T 428/12917: Next to Fe-base component
- Y10T 428/12931: Co-, Fe-, or Ni-base components, alternative to each other
- Y10T 428/12937: Co- or Ni-base component next to Fe-base component
- Y10T 428/12944: Ni-base component
- Y10T 428/12951: Fe-base component
- Y10T 428/12958: Next to Fe-base component
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An anti-cavitation damping composite metal structure for a flow passage component and a preparation method thereof are provided. The preparation method includes: cladding a gradient functional material layer by layer on a substrate of a flow passage component; forming periodic structures on a surface of each layer of the gradient functional material through etching by an ultrafast laser to absorb a part of an impact load energy caused by cavitation of the flow passage component, where the layers of the gradient functional material form a gradient coating with a toughness increasing layer by layer and a hardness decreasing layer by layer from bottom to top; and forming nano twins on a surface layer by a laser shock peening technique, and implanting a residual compressive stress to further improve anti-cavitation resistance of a surface.

## Claims

### Claim 1

A preparation method of an anti-cavitation damping composite metal structure for a flow passage component, comprising: cladding a gradient functional material layer by layer on a substrate of the flow passage component; and forming a plurality of periodic structures on a surface of each layer of the gradient functional material through etching by an ultrafast laser to absorb a part of an impact load energy caused by a cavitation of the flow passage component, wherein the each layer of the gradient functional material together forms a gradient coating with a toughness increasing layer by layer and a hardness decreasing layer by layer from outside to inside.

### Claim 2 (depends on 1)

The preparation method of the anti-cavitation damping composite metal structure for the flow passage component according to claim 1, wherein the preparation method comprises the following steps:
step S1: polishing the substrate made of high-manganese aluminum bronze, and forming first periodic structures of the plurality of periodic structures on the substrate made of the high-manganese aluminum bronze through the etching by a picosecond green laser, wherein a spacing between the first periodic structures is an integer multiple of a wavelength of a stress wave applied onto a surface of the flow passage component;
step S2: cladding a nickel copper layer by a semiconductor laser on a surface of the substrate made of the high-manganese aluminum bronze, polishing the nickel copper layer, and forming second periodic structures of the plurality of periodic structures on the nickel copper layer through the etching by the picosecond green laser, wherein a spacing between the second periodic structures is an integer multiple of the wavelength of the stress wave applied onto the surface of the flow passage component;
step S3: cladding a hard alloy layer on a surface of the nickel copper layer by the semiconductor laser, polishing the hard alloy layer, and forming third periodic structures of the plurality of periodic structures on the hard alloy layer through the etching by the picosecond green laser, wherein a spacing between the third periodic structures is an integer multiple of the wavelength of the stress wave applied onto the surface of the flow passage component; and
step S4: cladding a ceramic alloy layer on a surface of the hard alloy layer by the semiconductor laser through coaxial powder feeding to form a gradient damping composite coating.

### Claim 3 (depends on 2)

The preparation method of the anti-cavitation damping composite metal structure for the flow passage component according to claim 2, wherein the step S1 comprises:
polishing the substrate made of the high-manganese aluminum bronze with 200-2,000 grit sandpaper, and forming the first periodic structures on the substrate made of the high-manganese aluminum bronze through the etching by the picosecond green laser with a power of 30 W in a three-dimensional (3D) galvanometer scanning mode at a scanning speed of 100 mm/s, wherein the first periodic structures are pyramid structures with the spacing of 2.7 mm.

### Claim 4 (depends on 2)

The preparation method of the anti-cavitation damping composite metal structure for the flow passage component according to claim 2, wherein the step S2 comprises:
cladding the nickel copper layer on the surface of the substrate made of the high-manganese aluminum bronze by the semiconductor laser with a power of 700 W and a scanning speed of 8 mm/s, using a circular spot with a diameter of 2 mm and a defocusing amount of 11 mm through the coaxial powder feeding at a powder feeding rate of 8.5 g/min, with Ar as a protective gas, wherein the nickel copper layer is prepared from a mixed powder comprising 60% Ni, 33% Cu, and 7% Fe; and polishing the nickel copper layer, and forming the second periodic structures on the nickel copper layer through the etching by the picosecond green laser with a power of 30 W in a 3D galvanometer scanning mode at a scanning speed of 100 mm/s, wherein the second periodic structures are pyramid structures with the spacing of 2.7 mm.

### Claim 5 (depends on 2)

The preparation method of the anti-cavitation damping composite metal structure for the flow passage component according to claim 2, wherein the step S3 comprises:
cladding the hard alloy layer on the surface of the nickel copper layer by the semiconductor laser with a power of 1,500 W and a scanning speed of 15 mm/s, using a circular spot with a diameter of 2 mm and a defocusing amount of 11 mm, at a powder feeding rate of 17 g/min, with Ar as a protective gas, wherein the hard alloy layer is prepared from a mixed powder comprising 0.03% C, 0.7% Si, 1.25% Mn, 17.6% Cr, 19.5% Ni, 2.25% Mo, and 58.67% Fe; and polishing the hard alloy layer, and forming the third periodic structures on the hard alloy layer through the etching by the picosecond green laser with a power of 30 W in a 3D galvanometer scanning mode at a scanning speed of 100 mm/s, wherein the third periodic structures are pyramid structures with the spacing of 2.7 mm.

### Claim 6 (depends on 2)

The preparation method of the anti-cavitation damping composite metal structure for the flow passage component according to claim 2, wherein the step S4 comprises:
cladding the ceramic alloy layer on the surface of the hard alloy layer by the semiconductor laser with a power of 2,500 W and a scanning speed of 200 mm/s, using a circular spot with a diameter of 2 mm and a defocusing amount of 11 mm, through the coaxial powder feeding at a powder feeding rate of 10 g/min, with Ar as a protective gas, wherein the ceramic alloy layer is prepared from a mixed powder comprising 42% Ni, 42% Fe, 3% B, 3% Si, and 10% SiC, thereby forming a surface ceramic alloy layer.

### Claim 7 (depends on 2)

The preparation method of the anti-cavitation damping composite metal structure for the flow passage component according to claim 2, further comprising: step S5: strengthening the ceramic alloy layer by a laser shock peening technique, refining grains in the ceramic alloy layer to form nano twins on a surface of the ceramic alloy layer, and implanting a residual compressive stress layer.

### Claim 8 (depends on 7)

The preparation method of the anti-cavitation damping composite metal structure for the flow passage component according to claim 7, wherein the step S5 comprises: taking a black tape as an absorption layer and water as a restraint layer with a thickness of 2 mm; and using a circular Gaussian spot with a diameter of 3 mm, a spot overlapping ratio of 50%, a single pulse energy of 5-10 J, and a pulse width of 10 ns.

### Claim 9 (depends on 1)

An anti-cavitation damping composite metal structure for a flow passage component, formed by the preparation method of the anti-cavitation damping composite metal structure for the flow passage component according to claim 1.

### Claim 10 (depends on 9)

The anti-cavitation damping composite metal structure for the flow passage component according to claim 9, wherein the preparation method comprises the following steps:
step S1: polishing the substrate made of high-manganese aluminum bronze, and forming first periodic structures of the plurality of periodic structures on the substrate made of the high-manganese aluminum bronze through the etching by a picosecond green laser, wherein a spacing between the first periodic structures is an integer multiple of a wavelength of a stress wave applied onto a surface of the flow passage component;
step S2: cladding a nickel copper layer by a semiconductor laser on a surface of the substrate made of the high-manganese aluminum bronze, polishing the nickel copper layer, and forming second periodic structures of the plurality of periodic structures on the nickel copper layer through the etching by the picosecond green laser, wherein a spacing between the second periodic structures is an integer multiple of the wavelength of the stress wave applied onto the surface of the flow passage component;
step S3: cladding a hard alloy layer on a surface of the nickel copper layer by the semiconductor laser, polishing the hard alloy layer, and forming third periodic structures of the plurality of periodic structures on the hard alloy layer through the etching by the picosecond green laser, wherein a spacing between the third periodic structures is an integer multiple of the wavelength of the stress wave applied onto the surface of the flow passage component; and
step S4: cladding a ceramic alloy layer on a surface of the hard alloy layer by the semiconductor laser through coaxial powder feeding to form a gradient damping composite coating.

### Claim 11 (depends on 10)

The anti-cavitation damping composite metal structure for the flow passage component according to claim 10, wherein the step S1 comprises:
polishing the substrate made of the high-manganese aluminum bronze with 200-2,000 grit sandpaper, and forming the first periodic structures on the substrate made of the high-manganese aluminum bronze through the etching by the picosecond green laser with a power of 30 W in a three-dimensional (3D) galvanometer scanning mode at a scanning speed of 100 mm/s, wherein the first periodic structures are pyramid structures with the spacing of 2.7 mm.

### Claim 12 (depends on 10)

The anti-cavitation damping composite metal structure for the flow passage component according to claim 10, wherein the step S2 comprises:
cladding the nickel copper layer on the surface of the substrate made of the high-manganese aluminum bronze by the semiconductor laser with a power of 700 W and a scanning speed of 8 mm/s, using a circular spot with a diameter of 2 mm and a defocusing amount of 11 mm through the coaxial powder feeding at a powder feeding rate of 8.5 g/min, with Ar as a protective gas, wherein the nickel copper layer is prepared from a mixed powder comprising 60% Ni, 33% Cu, and 7% Fe; and polishing the nickel copper layer, and forming the second periodic structures on the nickel copper layer through the etching by the picosecond green laser with a power of 30 W in a 3D galvanometer scanning mode at a scanning speed of 100 mm/s, wherein the second periodic structures are pyramid structures with the spacing of 2.7 mm.

### Claim 13 (depends on 10)

The anti-cavitation damping composite metal structure for the flow passage component according to claim 10, wherein the step S3 comprises:
cladding the hard alloy layer on the surface of the nickel copper layer by the semiconductor laser with a power of 1,500 W and a scanning speed of 15 mm/s, using a circular spot with a diameter of 2 mm and a defocusing amount of 11 mm, at a powder feeding rate of 17 g/min, with Ar as a protective gas, wherein the hard alloy layer is prepared from a mixed powder comprising 0.03% C, 0.7% Si, 1.25% Mn, 17.6% Cr, 19.5% Ni, 2.25% Mo, and 58.67% Fe; and polishing the hard alloy layer, and forming the third periodic structures on the hard alloy layer through the etching by the picosecond green laser with a power of 30 W in a 3D galvanometer scanning mode at a scanning speed of 100 mm/s, wherein the third periodic structures are pyramid structures with the spacing of 2.7 mm.

### Claim 14 (depends on 10)

The anti-cavitation damping composite metal structure for the flow passage component according to claim 10, wherein the step S4 comprises:
cladding the ceramic alloy layer on the surface of the hard alloy layer by the semiconductor laser with a power of 2,500 W and a scanning speed of 200 mm/s, using a circular spot with a diameter of 2 mm and a defocusing amount of 11 mm, through the coaxial powder feeding at a powder feeding rate of 10 g/min, with Ar as a protective gas, wherein the ceramic alloy layer is prepared from a mixed powder comprising 42% Ni, 42% Fe, 3% B, 3% Si, and 10% SiC, thereby forming a surface ceramic alloy layer.

### Claim 15 (depends on 10)

The anti-cavitation damping composite metal structure for the flow passage component according to claim 10, further comprising: step S5: strengthening the ceramic alloy layer by a laser shock peening technique, refining grains in the ceramic alloy layer to form nano twins on a surface of the ceramic alloy layer, and implanting a residual compressive stress layer.

### Claim 16 (depends on 15)

The anti-cavitation damping composite metal structure for the flow passage component according to claim 15, wherein the step S5 comprises: taking a black tape as an absorption layer and water as a restraint layer with a thickness of 2 mm; and using a circular Gaussian spot with a diameter of 3 mm, a spot overlapping ratio of 50%, a single pulse energy of 5-10 J, and a pulse width of 10 ns.