# US 2024/0150241 A1 · Encapsulated systems for the development of self- healing building materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0150241 A1
- Document ID: US20240150241A1
- Status: Published application
- Kind: A1
- Application number: 18/280,631
- Filed: 2022-03-04
- Published: 2024-05-09
- Earliest claimed: 2021-03-07
- Assignees: National Centre for Scientific Research Demokritos
- Applicants: National Centre for Scientific Research Demokritos
- Inventors: Ioannis Karatasios; Stamatoula Papaioannou; Maria Amenta; Dimitrios Gournis; Vassilios Kilikoglou
- Web page: https://patentgrep.com/patent/US20240150241A1

## CPC

- C04B 20/1077: {Cements, e.g. waterglass}
- C04B 20/1037: {obtained otherwise than by reactions only involving carbon-to-carbon unsaturated bonds}
- C04B 20/1088: {Water}
- C04B 2111/00663: {as filling material for cavities or the like}
- C04B 2235/3206: Magnesium oxides or oxide-forming salts thereof
- C04B 2235/3208: Calcium oxide or oxide-forming salts thereof, e.g. lime
- C04B 2235/5427: millimeter or submillimeter sized, i.e. larger than 0,1 mm
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

The present invention relates to a novel method for the production of an encapsulated system for the self-healing of cracks formed within the matrix of building materials, preferably cementitious materials, such as concrete, mortar or render. Further, the invention refers to a novel encapsulated system comprising a cement-based active core and a hydrated cement-based protective shell, and to the use of said encapsulated system for the self-healing of cementitious materials such as concrete or mortar.

## Claims

### Claim at position 1

-13. (canceled)

### Claim 14

A method of producing an encapsulated system for self-healing of building materials including concrete, mortar, or render, the method comprising:
preparing core particles by the following steps:
adding cement powder in a drum of a pan-coating device;
wetting the cement powder in the drum by spraying with water in a water/cement ratio equal to 1/10 w/w for approximately 2 minutes while rotating the drum at a speed in the range of 50-70 RPM and supplying a continuous airflow at a temperature of 40-50° C., thereby forming the core particles;
removing the formed core particles from the drum and drying the core particles in an oven at 40° C. for 24 hours to provide the core particles with a diameter in the range of 0.5-10 mm; and
coating the prepared core particles with a shell by the following steps:
from the prepared core particles, selecting those core particles with a diameter in the range of 2-4 mm;
adding the selected core particles in the drum;
wetting the core particles in the drum with water or a polyvinyl alcohol water solution of 10 wt %;
rotating the drum containing the wetted core particles while supplying a continuous airflow at a temperature of 40-50° C.;
adding cement powder into the rotating drum to coat the core particles with an external cement layer and form a shell covering the core particles;
spraying the core particles covered with the external cement layer with a sodium silicate water solution of 10 wt % or a setting accelerator water solution of 12 wt % to cause the shell to become thickened and hardened;
repeating one more time the steps of adding the cement power followed by the spraying of the core particles so that the shell is further thickened and hardened;
thereafter drying the coated particles at 40° C. for 4 hours; and
storing the dried coated particles at room temperature.

### Claim 15 (depends on 14)

The method of claim 14, wherein:
during preparation of the core particles, the cement powder comprises Portland cement or belite/calcium sulfo-aluminate cement or a mixture of Portland cement and belite/calcium sulfo-aluminate cement; and further comprising mixing the cement powder with crystalline admixtures, and/or calcium oxide, and/or magnesium oxide and and/or a super plasticizer;
during the coating of the prepared core particles with the shell, the selection of the core particles with a diameter in the range of 2-4 mm is done by sieving, and the cement powder comprises Portland cement or belite/calcium sulfo-aluminate cement or a mixture of ordinary Portland cement and belite/calcium sulfo-aluminate cement.

### Claim 16 (depends on 15)

The method of claim 15, wherein during preparation of the core particles, the wetting of the cement powder comprises spraying the cement powder with tap water for approximately 2 minutes.

### Claim 17 (depends on 14)

The method of claim 14, wherein during preparation of the core particles, the cement powder comprises Portland cement or belite/calcium sulfo-aluminate cement or a mixture of Portland cement and belite/calcium sulfo-aluminate cement; and further comprising mixing the cement powder with crystalline admixtures, and/or calcium oxide, and/or magnesium oxide, and/or a super plasticizer, and grinding the resulting mixture for homogenization down to 63 microns.

### Claim 18 (depends on 15)

The method of claim 15, wherein the super plasticizer comprises polycarboxylate.

### Claim 19 (depends on 14)

The method of claim 14, wherein during the coating of the prepared core particles with the shell: the spraying comprises spraying the core particles covered with the external cement layer with a sodium silicate water solution of 10 wt %; and further comprising spraying the dried coated particles with a sodium silicate water solution of 10 wt % and drying the sprayed coated particles at 40° C. for 4 hours before storing the dried coated particles at room temperature.

### Claim 20 (depends on 14)

The method of claim 14, wherein during the coating of the prepared core particles with the shell: the spraying comprises spraying the core particles covered with the external cement layer with a setting accelerator water solution of 12 wt %; and further comprising spraying the dried coated particles with a setting accelerator water solution of 12 wt % and drying the sprayed coated particles at 40° C. for 4 hours before storing the dried coated particles at room temperature.

### Claim 21 (depends on 15)

An encapsulated system for self-healing of building materials, including concrete, mortar or render, directly obtainable by the method of claim 15.

### Claim 22 (depends on 21)

The encapsulated system of claim 21, wherein each of the core particles has a diameter in the range of 0.5-10 mm.

### Claim 23 (depends on 22)

The encapsulated system of claim 22, wherein each of the core particles has a diameter in the range of 2-4 mm.

### Claim 24 (depends on 22)

The encapsulated system of claim 22, wherein the shell coating each of the core particles has a thickness in the range of 0.1-2 mm.

### Claim 25 (depends on 21)

The encapsulated system of claim 21, wherein the encapsulated system has a spherical or spheroid shape.

### Claim 26 (depends on 21)

An additive for building materials comprising the encapsulated system of claim 21.

### Claim 27 (depends on 21)

A building material comprising the encapsulated system of claim 21.

### Claim 28

A method of producing an encapsulated system for self-healing of building materials, comprising:
preparing core particles by:
providing cement powder in a drum configured for undergoing rotation;
wetting the cement power and supplying thereto a continuous airflow while the drum undergoes rotation, thereby forming core particles;
removing the core particles from the drum and drying the core particles to obtain core particles with a diameter in the range of 0.5-10 mm; and
coating the core particles with shells by:
adding the obtained core particles in the drum and wetting the added core particles with water or a polyvinyl alcohol water solution;
rotating the drum with the wetted core particles while supplying thereto a continuous airflow;
adding cement powder into the rotating drum to coat the core particles with an external cement layer and form a shell covering the core particles;
spraying the core particles covered with the external cement layer with a sodium silicate water solution or a setting accelerator water solution to cause the shell to become thickened and hardened;
repeating the steps of adding the cement power followed by the spraying of the core particles so that the shell is further thickened and hardened; and
thereafter drying the coated particles and storing the dried coated particles at room temperature.

### Claim 29 (depends on 28)

The method of claim 28, wherein during preparation of the core particles, the cement power is wetted by spraying with water in a water/cement ratio equal to 1/10 w/w for approximately 2 minutes while the drum is rotated at a speed in the range of 50-70 RPM and the continuous airflow is supplied at a temperature of 40-50° C.

### Claim 30 (depends on 29)

The method of claim 29, wherein the obtained core particles added to the drum have a diameter in the range of 2-4 mm.

### Claim 31 (depends on 28)

The method of claim 28, wherein during the coating of the core particles with shells:
the obtained core particles added in the drum have a diameter in the range of 2-4 mm and the polyvinyl alcohol water solution has a concentration of 10 wt %;
the continuous airflow while the drum is rotated is supplied at a temperature of 40-50° C.; and
the coated particles are dried at 40° C. for 4 hours.

### Claim 32 (depends on 31)

The method of claim 31, wherein the spraying of the core particles comprises spraying the core particles with a sodium silicate water solution of 10 wt %.

### Claim 33 (depends on 31)

The method of claim 31, wherein the spraying of the core particles comprises spraying the core particles with a setting accelerator water solution of 12 wt %.