# US 2024/0150179 A1 · Process for producing graphene from graphite

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0150179 A1
- Document ID: US20240150179A1
- Status: Published application
- Kind: A1
- Application number: 18/483,783
- Filed: 2023-10-10
- Published: 2024-05-09
- Earliest claimed: 2023-08-18
- Assignees: Capattery Inc.
- Applicants: Capattery Inc.
- Inventors: Susant Pattnaik; Aneeya Kumar Samantara; Satyajit Ratha
- Web page: https://patentgrep.com/patent/US20240150179A1

## CPC

- C01B 32/19: by exfoliation
- C01B 32/196: Purification
- C01B 32/225: Expansion; Exfoliation
- C01B 2204/04: Specific amount of layers or specific thickness
- C01P 2006/80: Compositional purity
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

The present disclosure provides a process for producing graphene from graphite. The process includes mechanically agitating a first dispersion comprising graphite to form an exfoliated graphene dispersion. The exfoliated graphene dispersion is separated into a supernatant layer and a sediment layer. The supernatant layer comprises exfoliated graphene and the sediment layer comprises microstructured graphite. The process further comprises subjecting the supernatant layer to sonication to obtain a graphene dispersion. The graphene is obtained from the graphene dispersion by freeze drying.

## Claims

### Claim 1

A process for producing graphene from graphite comprising steps of:
(i) mechanically agitating a first dispersion comprising graphite in an impact chamber to form an exfoliated graphene dispersion;
(ii) separating the exfoliated graphene dispersion from the impact chamber into a supernatant layer and a sediment layer, wherein the supernatant layer comprises exfoliated graphene and the sediment layer comprises microstructured graphite;
(iii) subjecting the supernatant layer to sonication to obtain a graphene dispersion at a temperature ranging from 5 degree Celsius (° C.) to −5° C.; and
(iv) separating the graphene from the graphene dispersion by freeze drying.

### Claim 2 (depends on 1)

The process as claimed in claim 1, wherein the sediment layer is recycled by repeating the steps (i) to (iv).

### Claim 3 (depends on 1)

The process as claimed in claim 1, wherein graphite of the step (i) is prepared by grinding and sieving raw graphite to a size of less than 50 microns.

### Claim 4 (depends on 3)

The process as claimed in claim 3, wherein the first dispersion is formed by dispersing graphite in a solvent with agitation.

### Claim 5 (depends on 4)

The process as claimed in claim 4, wherein the solvent comprises N,N-dimethylformamide (DMF), N-methylpyrrolidone (NMP), N,N-dimethyl acetamide (DMA), gamma-butyrolactone, dimethylsulfoxide (DMSO), 1,3-dimethyl-2-imidazolidinone, or any combinations thereof.

### Claim 6 (depends on 1)

The process as claimed in claim 1, wherein the step (i) of mechanically agitating the first dispersion comprises ball milling at a speed ranging from 200 revolutions per minute (rpm) to 400 rpm for a time period ranging from 20 to 30 hours.

### Claim 7 (depends on 1)

The process as claimed in claim 1, wherein the exfoliated graphene dispersion is separated by means of gravimetric separation.

### Claim 8 (depends on 7)

The process as claimed in claim 7, wherein the gravimetric separation comprises centrifuging the exfoliated graphene dispersion at a speed ranging from 8000 revolutions per minute (rpm) to 10000 rpm for a time ranging from 20 minutes to 1 hour.

### Claim 9 (depends on 1)

The process as claimed in claim 1, wherein the process is a batch process, a continuous process, or a semi-continuous process.

### Claim 10 (depends on 1)

The process as claimed in claim 1, wherein the graphene has a thickness ranging from 3 to 5 atomic layers.

### Claim 11 (depends on 1)

The process as claimed in claim 1, wherein the graphene has a lateral dimension ranging from 1 to 5 microns.

### Claim 12 (depends on 1)

The process as claimed in claim 1, wherein the graphene has a carbon content of more than 99%.

### Claim 13

A graphene produced from graphite using a process comprising:
(i) mechanically agitating a first dispersion comprising graphite in an impact chamber to form an exfoliated graphene dispersion;
(ii) separating the exfoliated graphene dispersion from the impact chamber into a supernatant layer and a sediment layer, wherein the supernatant layer comprises exfoliated graphene and the sediment layer comprises microstructured graphite;
(iii) subjecting the supernatant layer to sonication to obtain a graphene dispersion at a temperature ranging from 5° C. to −5° C.; and
(iv) separating the graphene from the graphene dispersion by freeze drying.

### Claim 14 (depends on 13)

The graphene as claimed in claim 13, wherein the graphene has a carbon content of more than 99%.

### Claim 15 (depends on 13)

The graphene as claimed in claim 13, wherein the graphene has a thickness ranging from 3 to 5 atomic layers.

### Claim 16 (depends on 13)

The graphene as claimed in claim 13, wherein the graphene has a lateral dimension ranging from 1 to 5 microns.