# US 2024/0149379 A1 · Manufacturing method of gallium nitride substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0149379 A1
- Document ID: US20240149379A1
- Status: Published application
- Kind: A1
- Application number: 18/492,220
- Filed: 2023-10-23
- Published: 2024-05-09
- Earliest claimed: 2022-11-01
- Assignees: Disco Corporation
- Applicants: Disco Corporation
- Inventors: Asahi NOMOTO
- Web page: https://patentgrep.com/patent/US20240149379A1

## CPC

- B23K 26/53: for modifying or reforming the material inside the workpiece, e.g. for producing break initiation cracks
- B23K 26/0676: {into dependently operating sub-beams, e.g. an array of spots with fixed spatial relationship or for performing simultaneously identical operations}
- B28D 5/0011: {with preliminary treatment, e.g. weakening by scoring}
- B28D 5/0094: {the supporting or holding device being of the vacuum type}
- B23K 26/0622: by shaping pulses
- B23K 26/0626: {Energy control of the laser beam (B23K26/0622 takes precedence)}
- B23K 26/082: Scanning systems, i.e. devices involving movement of the laser beam relative to the laser head
- B23K 26/0823: {Devices involving rotation of the workpiece}
- B28D 5/0064: {Devices for the automatic drive or the program control of the machines}
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B28D: WORKING STONE OR STONE-LIKE MATERIALS

## Abstract

A manufacturing method of a gallium nitride (GaN) substrate includes a peeling layer forming step of forming a peeling layer at a depth, which corresponds to a thickness of the gallium nitride substrate to be manufactured, by relatively moving a GaN ingot and a focal point of a laser beam of a wavelength, which transmits through GaN, along a direction of a crystal orientation of the GaN ingot as represented by the below-described formula (1) with the focal point positioned inside the GaN ingot, and a peeling step of peeling the GaN substrate from the GaN ingot using the peeling layer as a start point. The peeling layer forming step is set such that the laser beam is split to form a plurality of focal points and straight lines connecting the individual split focal points each extend along a direction parallel to the direction of the crystal orientation represented by the below-described formula (1). 1 1 2 0 Formula (1)

## Claims

### Claim 1

A manufacturing method of a gallium nitride substrate from a gallium nitride ingot having a first surface and a second surface on a side opposite to the first surface, the method comprising:
a holding step of holding the gallium nitride ingot,
a peeling layer forming step of forming a peeling layer at a depth, which corresponds to a thickness of the gallium nitride substrate to be manufactured, by relatively moving the gallium nitride ingot and a focal point of a laser beam of a wavelength, which transmits through gallium nitride, along a direction of a crystal orientation of the gallium nitride ingot as represented by a below-described formula (1) with the focal point positioned inside the gallium nitride ingot from the first surface; and
a peeling step of peeling the gallium nitride substrate from the gallium nitride ingot using the peeling layer as a start point, wherein
the peeling layer forming step is set such that the laser beam is split to form a plurality of focal points and straight lines connecting the individual split focal points each extend along a direction parallel to the direction of the crystal orientation represented by the below-described formula (1).
1 1 2 0 Formula (1)

### Claim 2 (depends on 1)

The manufacturing method according to claim 1, wherein, in the peeling layer forming step, at least one of the straight lines connecting the individual split focal points is set so as to intersect a direction along which the gallium nitride ingot and the focal points are relatively moved and extend along the direction parallel to the direction of the crystal orientation represented by the formula (1).

### Claim 3 (depends on 1)

The manufacturing method according to claim 1, wherein, in the peeling layer forming step, a relative moving speed between the gallium nitride ingot and the focal points is set such that straight lines connecting adjacent processing marks formed by relatively moving the gallium nitride ingot and the focal points are each formed along the direction of the crystal orientation represented by the formula (1).