# US 2024/0133028 A1 · Electrolyte and Method for Cobalt Electrodeposition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0133028 A1
- Document ID: US20240133028A1
- Status: Published application
- Kind: A1
- Application number: 18/277,695
- Filed: 2022-02-08
- Published: 2024-04-25
- Earliest claimed: 2021-02-18
- Assignees: aveni
- Applicants: Aveni
- Inventors: Hermine Marie Berthon; Mikailou Thiam; Dominique Suhr; Yeeseul Kim; Céline Pascale Doussot
- Web page: https://patentgrep.com/patent/US20240133028A1

## CPC

- C25D 5/02: Electroplating of selected surface areas
- C25D 3/12: of nickel or cobalt
- C25D 3/18: Heterocyclic compounds
- C25D 7/12: Semiconductors
- C25D 7/123: {Semiconductors first coated with a seed layer or a conductive layer}
- C25D 5/48: After-treatment of electroplated surfaces
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

The present invention relates to a method for fabricating cobalt interconnects and an electrolyte enabling it to be implemented. The electrolyte of pH less than 4.0 comprises cobalt ions, chloride ions and organic additives, including an alpha-hydroxy carboxylic acid and an amine chosen from polyethyleneimine or benzotriazole.

## Claims

### Claim 1

Electrolyte for the electrodeposition of cobalt characterized in that the electrolyte is an aqueous solution comprising from 1 to 5 g/L of cobalt II ions, from 1 to 10 g/L of chloride ions, a strong acid in a sufficient quantity to obtain a pH comprised between 1.8 and 4.0, and organic additives including at least one first additive chosen from alpha-hydroxy carboxylic acids and mixtures thereof and at least one second additive chosen from polyethyleneimines and benzotriazole.

### Claim 2 (depends on 1)

Electrolyte according to claim 1, characterized in that the total concentration of organic additives in the electrolyte is comprised between 5 ppm and 50 ppm.

### Claim 3 (depends on 1)

Electrolyte according to claim 1, characterized in that the concentration of the second additive is comprised between 1 ppm and 10 ppm.

### Claim 4 (depends on 1)

Electrolyte according to claim 1, characterized in that it does not contain any sulphur compound.

### Claim 5 (depends on 1)

Electrolyte according to claim 1, characterized in that its pH is comprised between 1.8 and 2.6.

### Claim 6 (depends on 5)

Electrolyte according to claim 5, characterized in that the first additive is chosen from citric acid, tartaric acid, malic acid, mandelic acid and glyceric acid.

### Claim 7 (depends on 1)

Electrolyte according to claim 1, characterized in that its conductivity is comprised between 2 mS/cm and 10 mS/cm.

### Claim 8 (depends on 5)

Electrolyte according to claim 5, characterized in that it does not contain boric acid.

### Claim 9 (depends on 1)

Electrochemical method for deposition on a substrate provided with a conductive surface comprising a flat part and cavities, by filling said cavities bottom-up, said method comprising:
a step of contacting the conductive surface with an electrolyte according to claim 1,
an electrical step of polarizing the conductive surface for a sufficient duration to perform a cobalt deposition on the surface.

### Claim 10 (depends on 9)

Electrochemical method for depositing cobalt according to claim 9, characterized in that the duration is sufficient to perform the filling of the cavities and the coating of the flat part by a cobalt deposit having a thickness ranging from 50 nm to 400 nm.

### Claim 11 (depends on 9)

Electrochemical method for depositing cobalt according to claim 9, characterized in that the polarization step is immediately followed by a polishing step combining chemical and mechanical attack of the cobalt deposit obtained at the end of the polarization step.

### Claim 12 (depends on 9)

Method according to claim 9, wherein the cavities have a width at their opening of less than 100 nm, preferably comprised between 10 and 50 nm and a depth comprised between 50 nm and 250 nm.

### Claim 13 (depends on 9)

Method according to claim 9, wherein the cobalt deposit obtained at the end of the polarization step has an impurity content less than 1000 atomic ppm.

### Claim 14 (depends on 9)

Method according to claim 9, wherein the cobalt deposit obtained at the end of the electrodeposition step comprises a mean void percentage of less than 10% by volume or by area, without undergoing a heat treatment at a temperature ranging from 50° C. to 500° C.

### Claim 15 (depends on 9)

Method according to claim 9, wherein the cobalt deposition rate is comprised between 0.1 nm/s and 3.0 nm/s when the intensity of the polarization current ranges from 8.5 mA/cm2 to 18.5 mA/cm2.

### Claim 16 (depends on 9)

Method according to claim 9, wherein the resistivity of the cobalt deposit obtained at the end of the polarization step is less than 30 μ∩·cm without undergoing a heat treatment at a temperature ranging from 50° C. to 500° C.

### Claim 17 (depends on 9)

Method according to claim 9, wherein the substrate is obtained by successive deposits of SiO2, tantalum nitride and cobalt.

### Claim 18 (depends on 17)

Method according to claim 17, characterized in that the cobalt is deposited on tantalum nitride by chemical vapor deposition (CVD) or by atomic layer deposition (ALD).