# US 2024/0131580 A1 · Silver powder and method of producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0131580 A1
- Document ID: US20240131580A1
- Status: Published application
- Kind: A1
- Application number: 18/546,779
- Filed: 2022-03-02
- Published: 2024-04-25
- Earliest claimed: 2021-03-10
- Assignees: Dowa Electronics Materials Co., Ltd.
- Applicants: DOWA Electronics Materials Co., Ltd.
- Inventors: Kaori TOKUSADA; Hikaru HAYASHIDA
- Web page: https://patentgrep.com/patent/US20240131580A1

## CPC

- B22F 1/05: Metallic powder characterised by the size or surface area of the particles
- B22F 1/052: characterised by a mixture of particles of different sizes or by the particle size distribution
- B07B 9/00: Combinations of apparatus for screening or sifting or for separating solids from solids using gas currents; General arrangement of plant, e.g. flow sheets
- B22F 1/105: containing inorganic lubricating or binding agents, e.g. metal salts
- B22F 9/04: starting from solid material, e.g. by crushing, grinding or milling ({C22C1/1084 takes precedence}; crushing, grinding or milling, in general, see the relevant subclasses, e.g. B02C)
- B22F 9/18: with reduction of metal compounds
- B22F 9/24: starting from liquid metal compounds, e.g. solutions
- C22C 1/0466: {Alloys based on noble metals}
- C22C 5/06: Alloys based on silver
- B07B 7/08: using centrifugal force (centrifuges B04B; cyclones B04C)
- B07B 7/0865: {using the coanda effect of the moving gas stream}
- B22F 1/107: containing organic material comprising solvents, e.g. for slip casting
- B22F 2009/044: {by jet milling}
- B22F 2301/255: Silver or gold
- B22F 2304/058: Particle size above 300 nm up to 1 micrometer
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B07B: SEPARATING SOLIDS FROM SOLIDS BY SIEVING, SCREENING, SIFTING OR BY USING GAS CURRENTS; SEPARATING BY OTHER DRY METHODS APPLICABLE TO BULK MATERIAL, e.g. LOOSE ARTICLES FIT TO BE HANDLED LIKE BULK MATERIAL (wet separating processes, sorting by processes using fluent material in the same way as liquid B03; combinations of dry separating apparatus with wet separating apparatus B03B; using liquids B03B, B03D; sorting by magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high voltage electric fields B03C; centrifuges or vortex apparatus for carrying out physical processes B04; hand sorting, postal sorting, sorting by switching or other devices actuated in response to detection or measurement of some feature of articles or samples of material B07C)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

Provided are a silver powder having powder physical properties enabling reduction of volume resistivity after firing and a method of producing this silver powder. The silver powder has a tap density of 4.8 g/mL or more, a TAP/D50 value (value determined by dividing the tap density (g/mL) by the volume-based median diameter (μm)) of not less than 7 and not more than 15, and a specific surface area of not less than 0.75 m2/g and not more than 1.3 m2/g.

## Claims

### Claim 1

A silver powder having:
a tap density of 4.8 g/mL or more;
a TAP/D50 value that is a value determined by dividing the tap density, in units of g/mL, by volume-based median diameter, in units of μm, of not less than 7 and not more than 15; and
a specific surface area of not less than 0.75 m2/g and not more than 1.3 m2/g.

### Claim 2 (depends on 1)

The silver powder according to claim 1, wherein the TAP/D50 value is not less than 7 and not more than 10.

### Claim 3 (depends on 1)

The silver powder according to claim 1, wherein the median diameter is not less than 0.32 μm and not more than 1 μm.

### Claim 4 (depends on 3)

The silver powder according to claim 3, wherein the median diameter is not less than 0.4 μm and not more than 0.8 μm.

### Claim 5

A method of producing a silver powder comprising:
a milling step of using high-pressure airflow to accelerate and mill a silver powder produced by a wet reduction method; and
a classification step of classifying the silver powder, performed after the milling step, wherein
the milling step is performed with the silver powder having a concentration of 0.2 kg/m3 or less, and
the classifying is performed such that after the classification step, the silver powder has powder physical properties of:
a tap density of 4.8 g/mL or more;
a TAP/D50 value that is a value determined by dividing the tap density by volume-based median diameter, in units of μm, of not less than 7 and not more than 15; and
a specific surface area of not less than 0.75 m2/g and not more than 1.3 m2/g.

### Claim 6 (depends on 5)

The method of producing a silver powder according to claim 5, wherein
a milling device in the milling step, a classifying device in the classification step, and a collecting device are connected in series in this order,
an exhaust ventilator is connected at a downstream side of the collecting device and performs suction such that silver powder that has been supplied to the milling device is pneumatically conveyed to the collecting device, and
powder concentration determined by dividing a supply rate of silver powder in the milling step by an airflow rate of the exhaust ventilator is 0.08 kg/m3 or less.

### Claim 7 (depends on 2)

The silver powder according to claim 2, wherein the median diameter is not less than 0.32 μm and not more than 1 μm.

### Claim 8 (depends on 7)