# US 2024/0131483 A1 · Method of making a magnetic material and a fluidized bed mixer for making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0131483 A1
- Document ID: US20240131483A1
- Status: Published application
- Kind: A1
- Application number: 18/049,012
- Filed: 2022-10-23
- Published: 2024-04-25
- Earliest claimed: 2022-10-23
- Assignees: GM Global Technology Operations LLC
- Applicants: GM Global Technology Operations LLC
- Inventors: Qigui Wang; Yucong Wang
- Web page: https://patentgrep.com/patent/US20240131483A1

## CPC

- B01F 33/401: {Methods}
- C23C 4/12: characterised by the method of spraying
- B01F 23/69: {Mixing systems, i.e. flow charts or diagrams; Arrangements, e.g. comprising controlling means}
- B01F 23/804: {Drying the mixture}
- B01F 23/81: {Grinding the mixture}
- B01F 33/052: {the energy being electric fields for electrostatically charging of the ingredients or compositions for mixing them}
- B01F 33/40: Mixers using gas or liquid agitation, e.g. with air supply tubes
- B01F 33/409: {Parts, e.g. diffusion elements; Accessories}
- B01F 35/55: {Baffles; Flow breakers (B01F35/531 takes precedence)}
- B01J 2/16: by suspending the powder material in a gas, e.g. in fluidised beds or as a falling curtain
- B22F 1/052: characterised by a mixture of particles of different sizes or by the particle size distribution
- B22F 1/102: Metallic powder coated with organic material
- B22F 1/107: containing organic material comprising solvents, e.g. for slip casting
- B22F 1/16: Metallic particles coated with a non-metal (coated with lubricating or binding agents or with organic material B22F1/10)
- B22F 3/10: Sintering only
- B22F 9/04: starting from solid material, e.g. by crushing, grinding or milling ({C22C1/1084 takes precedence}; crushing, grinding or milling, in general, see the relevant subclasses, e.g. B02C)
- C23C 24/04: Impact or kinetic deposition of particles
- H01F 1/0571: {in the form of particles, e.g. rapid quenched powders or ribbon flakes}
- H01F 1/0577: {sintered}
- H01F 41/0293: {diffusion of rare earth elements, e.g. Tb, Dy or Ho, into permanent magnets}
- B05B 7/1486: {for spraying particulate material in dry state}
- B22F 2009/043: {by ball milling}
- B22F 2301/355: Rare Earth - Fe intermetallic alloys
- B22F 2998/10: Processes characterised by the sequence of their steps
- C22C 2202/02: Magnetic
- B01F: MIXING, e.g. DISSOLVING, EMULSIFYING OR DISPERSING (mixing paints B44D3/06)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- B05B: SPRAYING APPARATUS; ATOMISING APPARATUS; NOZZLES (spray-mixers with nozzles B01F25/72; processes for applying liquids or other fluent materials to surfaces by spraying B05D)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A fluidized bed mixer for combining a first powder with a second powder for manufacturing a magnet and a method of using the fluidized bed mixer for making the magnet. The first powder material is an alloy powder containing neodymium (Nd), iron (Fe), and boron (B), and the second powder material is an alloy powder or elemental metal powder containing one or more of dysprosium (Dy) and terbium (Tb). The fluidized bed mixer includes a fluidized bed portion in an upper portion of a mixing chamber, a cascading baffle system beneath the fluidized bed portion, and combined powder collection area beneath the cascading baffle system. The fluidized bed mixer is configured to homogenously combine a first powder material with a second powder material in such a way that particles of the second powder material adheres to and covers the outer surfaces of the particles of the first powder material.

## Claims

### Claim 1

A method of making a magnetic material comprising:
mixing a first powder material with a second powder material in a fluidized bed mixer to form a combined powder material;
milling the combined powder material; and
sintering the milled combined powder material into a solid structure.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first powder material comprises neodymium (Nd), iron (Fe), and boron (B) and the second powder material comprises one or more of dysprosium (Dy) and terbium (Tb).

### Claim 3 (depends on 2)

The method of claim 2, wherein the combined powder material includes alloy particles comprising a particle core having Nd, Fe, and B, and a particle surface coated with one or more of Dy and Tb.

### Claim 4 (depends on 2)

The method of claim 2, wherein the first powder material is gravity fed into a top portion of the fluidized bed mixer and the second powder material is sprayed into the fluidized bed mixer such that the second powder material collides with the first powder material.

### Claim 5 (depends on 4)

The method of claim 4, wherein the first powder material includes one of a positive charge and a negative charge, and the second powder material includes the other of the positive charge and the negative charge.

### Claim 6 (depends on 5)

The method of claim 5, further include spraying a solvent comprising at least one of a methanol, ethanol, kerosene, and gasoline onto the first powder material and the second powder material in the fluidized bed mixer.

### Claim 7 (depends on 6)

The method of claim 6, further including injecting a flow of an inert gas into the fluidized bed mixer sufficient to maintain the first powder material and the second powder material suspended in a fluidized bed but allows the heavier combined powder material to drop out of the fluidized bed.

### Claim 8 (depends on 7)

The method of claim 7, further comprising homogenizing the combined powder material dropped out of the fluidized bed through a cascading baffle system.

### Claim 9 (depends on 8)

The method of claim 8, further comprising milling the combined powder material exiting the cascading baffle system in a rotating drum and ball miller; and spraying a solvent onto the combined powder material while milling.

### Claim 10 (depends on 9)

The method of claim 9, further comprising drying the milled combined powder material in the fluidized bed mixer prior to sintering.

### Claim 11

A fluidized bed mixer for making a magnetic material, comprising:
a housing having an interior surface defining a mixing chamber extending along a centerline;
a fluidized bed portion in an upper portion of the mixing chamber;
a cascading baffle system in a middle portion of the mixing chamber below the fluidized bed portion; and
a collection area beneath the cascading baffle system in a lower portion of the mixing chamber.

### Claim 12 (depends on 11)

The fluidized bed mixer of claim 11 further comprising:
a first powder inlet configured to gravity feed a first powder material into the fluidized bed portion; and
at least one injection nozzle configured to inject a stream of the second powder material into the fluidized bed portion such that the second powder material collides with the first powder material to form a plurality of alloy particles having a core of the first powder material and a surface coated with the second powder material.

### Claim 13 (depends on 12)

The fluidized bed mixer of claim 12 further comprising an inlet to convey a stream of inert gas to maintain the first powder material and the second powder material suspended in a fluidized bed while allowing the plurality of alloy particles to drop out of the fluidized bed.

### Claim 14 (depends on 11)

The fluidized bed mixer of claim 11, wherein the cascading baffle system comprises:
a plurality of baffle plates, wherein each of the baffle plates includes a first end attached to the interior surface of the housing and an opposite second end angled downward across the centerline of the mixing chamber, wherein the baffle plates are arranged in a descending order such that the plurality of alloy particles flows from an upper baffle plate to a lower baffle plate in a cascading order.

### Claim 15 (depends on 14)

The fluidized bed mixer of claim 14, wherein one or more of the baffle plates are perforated.

### Claim 16 (depends on 15)

The fluidized bed mixer of claim 15, further comprising at least one inert gas inlet disposed between a pair of baffle plates and an inert gas outlet located above the fluidized bed portion.

### Claim 17 (depends on 16)

The fluidized bed mixer of claim 16, further comprising a first electrostatic spray configured to charge the first powder material with one of a positive and a negative charge, and a second electrostatic spray configured to charge the second powder material with the other of the positive charge and the negative charge.

### Claim 18

A method of making a magnetic material comprising:
mixing a first powder material with a second powder material in a fluidized bed to form a combined powder material; and
mixing the combined powder material dropped out of the fluidized bed through a cascading baffle system.

### Claim 19 (depends on 18)

The method of claim 18, further comprising:
applying one of a positive charge and a negative charge to the first powder material prior entering the fluidized bed;
applying the other of the positive charge and the negative charge to the second powder material prior entering the fluidized bed; and
spraying a solvent onto the first powder material and the second powder material suspended in the fluidized bed.

### Claim 20 (depends on 19)

The method of claim 19, further comprising:
milling the combined powder material;
adding a solvent to the combined powder material while milling; and
drying the milled combined powder material in the fluidized bed mixer.