# US 2024/0124692 A1 · Polyolefin resins for containers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0124692 A1
- Document ID: US20240124692A1
- Status: Published application
- Kind: A1
- Application number: 18/397,894
- Filed: 2023-12-27
- Published: 2024-04-18
- Earliest claimed: 2018-08-21
- Assignees: LiquiForm Group LLC
- Applicants: LiquiForm Group LLC
- Inventors: Gregory Carpenter; Theodore Tekip; Kirk Maki; Mark Blystone
- Web page: https://patentgrep.com/patent/US20240124692A1

## CPC

- C08L 23/04: Homopolymers or copolymers of ethene
- C08L 23/06: Polyethylene
- B29C 49/0006: {for heating or cooling}
- B29C 49/06: Injection blow-moulding
- B29C 49/0871: {radial stretch ratio, i.e. hoop or tangential stretch ratio}
- B29C 49/0872: {axial stretch ratio}
- B29C 49/12: Stretching rods
- B29C 49/46: characterised by using particular environment or blow fluids other than air
- B29C 49/58: Blowing means
- C08F 110/02: Ethene
- B29C 2049/465: {being incompressible}
- B29C 2049/4664: {staying in the final article}
- B29C 2049/7834: {Pressure increase speed, e.g. dependent on stretch or position}
- B29C 2049/7866: {of the blowing medium}
- B29C 2049/7879: {Stretching, e.g. stretch rod}
- B29C 2949/0715: the preform having one end closed
- B29C 2949/0861: Other specified values, e.g. values or ranges
- B29C 2949/0872: Weight
- B29C 2949/22: at neck portion
- B29C 2949/24: at flange portion
- B29C 2949/26: at body portion
- B29C 2949/28: at bottom portion
- B29K 2023/065: {HDPE, i.e. high density polyethylene}
- B29K 2995/0018: having particular optical properties, e.g. fluorescent or phosphorescent
- B29K 2995/0063: Density
- B29L 2031/712: {Containers; Packaging elements or accessories, Packages (closures therefor B29L2031/56; ink or toner cartridges B29L2031/7678; squeeze tubes B29L2023/20; suitcases B29L2031/7418)}
- B29L 2031/7158: {Bottles}
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L 2207/062: HDPE
- C08L 2314/02: Ziegler natta catalyst
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

A high-density polyethylene (HDPE) resin configured to be molded into a preform that can be biaxially expanded within a cavity of a container mold by introducing an incompressible fluid under pressure into the preform to stretch the preform to assume a shape of a surrounding mold cavity of the container mold. The HDPE resin has: a melt flow index of between 0.3 and 10.0 grams per 10 minutes at a temperature of 190° C. under 2.16 kilograms of load; a polydispersity index of 4-24; and a density of 0.943-0.965 grams per cubic centimeter.

## Claims

### Claim 1

A process for simultaneously forming and filling a container, the process comprising:
providing a preform comprising a high-density polyethylene (HDPE) resin in a mold cavity of a container mold wherein the HDPE resin has
a melt flow index of 0.3-10.0 grams per 10 minutes at a temperature of 190° C. under 2.16 kilograms of load through an extrusion plastometer test fixture with die orifice diameter of 2.0955 mm and length of 8.000 mm;
a polydispersity index of 4-24; and
a density of 0.943-0.965 grams per cubic centimeter; and
introducing an incompressible fluid under pressure into the preform to stretch the preform into a container filled with the incompressible fluid, the container having a shape of the mold cavity of the container mold.

### Claim 2 (depends on 1)

The process of claim 1 wherein:
the HDPE resin is from a chromium catalyst system; and
the HDPE resin has a melt flow index of 0.3 to 1 gram per 10 minutes at a temperature of 190° C. under 2.16 kilograms of load through an extrusion plastometer test fixture with a die orifice diameter of 2.0955 mm and a length of 8.000 mm.

### Claim 3 (depends on 1)

A container formed from the process of claim 1, wherein a ratio of a volume of the incompressible fluid encapsulated to a mass of the container formed from the HDPE resin is up to 60 ml per gram.

### Claim 4 (depends on 2)

A container formed from the process of claim 2, wherein a ratio of a volume of the incompressible fluid encapsulated to a mass of the container formed from the HDPE resin is up to 60 ml per gram.

### Claim 5 (depends on 2)

A container formed from the process of claim 2, wherein a ratio of a volume of the incompressible fluid encapsulated to a mass of the container formed from the HDPE resin is as high as 98 ml per gram.

### Claim 6 (depends on 1)

The process of claim 1, wherein the HDPE resin is from a Ziegler-Natta catalyst system.

### Claim 7 (depends on 6)

The process of claim 6, wherein the Ziegler-Natta catalyst system is multimodal.

### Claim 8 (depends on 1)

The process of claim 1, wherein the melt flow index is 0.3-4.0 grams per 10 minutes at a temperature of 190° C. under 2.16 kilograms of load through an extrusion plastometer test fixture with a die orifice diameter of 2.0955 mm and a length of 8.000 mm.

### Claim 9 (depends on 1)

The process of claim 1, wherein the melt flow index is 0.3-2.0 grams per 10 minutes at a temperature of 190° C. under 2.16 kilograms of load through an extrusion plastometer test fixture with a die orifice diameter of 2.0955 mm and a length of 8.000 mm.

### Claim 10 (depends on 1)

The process of claim 1, wherein the HDPE resin has a polydispersity index of 7-24.

### Claim 11 (depends on 1)

The process of claim 1, wherein the HDPE resin has a polydispersity index of 9-24.

### Claim 12 (depends on 1)

The process of claim 1, wherein the HDPE resin is a multimodal resin having a polydispersity index of 7 to 24.

### Claim 13 (depends on 1)

The process of claim 1, wherein the incompressible fluid is introduced at a incompressible fluid flow rate of from 0.5 L/sec to 6.0 L/sec.

### Claim 14 (depends on 1)

The process of claim 1, wherein the incompressible fluid is introduced at a temperature of from 9° C. to 85° C.

### Claim 15 (depends on 1)

The process of claim 1, further comprising axially stretching the preform with a rod.