# US 2024/0116827 A1 · Self-cleaning cementitious system and method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0116827 A1
- Document ID: US20240116827A1
- Status: Published application
- Kind: A1
- Application number: 18/374,747
- Filed: 2023-09-29
- Published: 2024-04-11
- Earliest claimed: 2022-09-30
- Applicants: Purdue Research Foundation
- Inventors: Maria Mirian Velay Lizancos; Vito Francioso; Carlos Moro Martinez; Marina Garcia Lopez-Arias
- Web page: https://patentgrep.com/patent/US20240116827A1

## CPC

- C04B 41/009: {characterised by the material treated}
- C04B 28/04: Portland cements
- C04B 28/08: Slag cements
- C04B 2111/00019: {Carbon dioxide sequestration}
- C04B 2111/00827: {Photocatalysts}
- C04B 2111/2061: {Materials containing photocatalysts, e.g. TiO2, for avoiding staining by air pollutants or the like}
- C04B 2235/3232: Titanium oxides or titanates, e.g. rutile or anatase
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

The construction system includes a composition that includes Portland cement, nano-TiO2, and slag cement. The composition may also include water. The composition is cured via a CO2 curing process to produce a self-cleaning photocatalytic composite with lower carbon footprint and may be more economically manufactured than known cement-based photocatalytic composites. The unveiled synergistic effect of using slag cement and applying a CO2 curing process may reduce the porosity of the material and reduce the penetration of the pollutants that will accumulate in the surface. Thus, pollutants will be more exposed to UV light and decompose the pollutants in a greater rate. The construction system is self-cleaning in that water, such as from rainfall, may effectively clean the cured composition to reset the sequestering capabilities for the construction system to continue to remove toxic gases for the atmosphere.

## Claims

### Claim 1

A composition for a construction material comprising:
around a tenth of a percent to around eighty-three percent Portland cement by total weight of the composite;
around a tenth of a percent to five percent of a photocatalytic material by weight of the composite; and
around a tenth of a percent to around eighty-three percent slag cement by total weight of the composite;
wherein the composition is cured by a CO2 curing process.

### Claim 2 (depends on 1)

The composition of claim 1, wherein the composition further includes water between a around sixteen percent to around thirty-eight percent by total weight of the composite.

### Claim 3 (depends on 2)

The composition of claim 2, wherein the water is around thirty-five percent by total weight of the composite.

### Claim 4 (depends on 1)

The composition of claim 1, wherein the Portland cement is between around twenty percent to around sixty percent by total weight of the composite.

### Claim 5 (depends on 4)

The composition of claim 4, wherein the Portland cement is around forty-four percent by total weight of the composite.

### Claim 6 (depends on 1)

The composition of claim 1, wherein the photocatalytic material is TiO2.

### Claim 7 (depends on 6)

The composition of claim 6, wherein the TiO2 is nanostructured.

### Claim 8 (depends on 7)

The composition of claim 7, wherein the nano-TiO2 is between around one percent to around three percent by total weight of the composite.

### Claim 9 (depends on 8)

The composition of claim 8, wherein the nano-TiO2 is around one and three tenths of a percent by total weight of the composite.

### Claim 10 (depends on 1)

The composition of claim 1, wherein the slag cement is between around five percent to around fourty percent by total weight of the composite.

### Claim 11 (depends on 10)

The composition of claim 10, wherein the slag cement is around nineteen and three tenths of a percent by total weight of the composite.

### Claim 12 (depends on 1)

The composition of claim 1, wherein the composition includes around thirty-five and one half of a percent water by total weight of the composite, around forty-three and nine tenths of a percent Portland cement by total weight of the composite, around one and three tenths of a percent by weight of nano-TiO2 by total weight of the composite, and around nineteen and three tenths of a percent by weight of slag cement.

### Claim 13 (depends on 1)

The composition of claim 1, wherein the composition is photocatalytic according to UNI 11259 requirements.

### Claim 14

A method of manufacturing a composite system, the method comprising the steps of:
mixing around a tenth of a percent to around eighty-three percent Portland cement by total weight, around a tenth of a percent to around five percent of a photocatalytic material by total weight of the composite, and around a tenth of a percent to around eighty-three percent slag cement by total weight of the composite;
disposing the mixture into a predetermined position; and
CO2 curing the disposed mixture.

### Claim 15 (depends on 14)

The method of claim 14, further comprising a step of mixing water into the mixture.

### Claim 16 (depends on 14)

The method of claim 14, wherein the CO2 curing of the disposed mixture includes exposing the disposed mixture to around five percent to around thirty-five percent CO2.

### Claim 17 (depends on 16)

The method of claim 16, wherein the step of CO2 curing further includes controlling the humidity at a predetermined level.

### Claim 18 (depends on 14)

The method of claim 14, wherein the step of CO2 curing the composite system is performed in at least one of a chamber, container, and an envelope.

### Claim 19 (depends on 18)

The method of claim 18, wherein the step of CO2 curing is performed for around twelve to twenty-four hours.

### Claim 20 (depends on 16)

The method of claim 16, wherein the photocatalytic material is TiO2 provided as less than three percent by total weight of the composite.