# US 2024/0110265 A1 · Sintered material for aluminum die casting and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0110265 A1
- Document ID: US20240110265A1
- Status: Published application
- Kind: A1
- Application number: 18/120,258
- Filed: 2023-03-10
- Published: 2024-04-04
- Earliest claimed: 2022-10-04
- Assignees: Hyundai Motor Company; Kia Corporation
- Applicants: Hyundai Motor Company; Kia Corporation
- Inventors: Hak Soo Kim
- Web page: https://patentgrep.com/patent/US20240110265A1

## CPC

- C22C 38/22: with molybdenum or tungsten
- B22F 1/10: Metallic powder containing lubricating or binding agents; Metallic powder containing organic material
- B22F 1/16: Metallic particles coated with a non-metal (coated with lubricating or binding agents or with organic material B22F1/10)
- B22F 3/10: Sintering only
- B22F 3/1007: {Atmosphere (B22F3/1021 takes precedence)}
- B22F 3/24: After-treatment of workpieces or articles {(B22F3/1146 takes precedence)}
- C22C 33/0207: {Using a mixture of pre-alloyed powders or a master alloy}
- C22C 33/0264: {the maximum content of each alloying element not exceeding 5%}
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- B22F 2003/241: {Chemical after-treatment on the surface}
- B22F 2005/002: {Tools other than cutting tools}
- B22F 2201/013: Hydrogen
- B22F 2201/02: Nitrogen
- B22F 2201/05: Water or water vapour
- B22F 2301/35: Iron
- B22F 2998/00: Supplementary information concerning processes or compositions relating to powder metallurgy
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER

## Abstract

A sintered material for aluminum die casting can prevent the strength from being lowered even after steam treatment. The sintered material for aluminum die casting is a sintered material used as an insert at the time of aluminum die casting, and contains Cr: 0.71 to 0.97 wt %, Mo: 0.10 to 0.20 wt %, and C: 0.64 to 0.87 wt %, with the remainder being Fe and other unavoidable impurities.

## Claims

### Claim 1

A sintered material used as an insert in aluminum die casting, the sintered material comprising:
Cr: 0.71 to 0.97 wt %;
Mo: 0.10 to 0.20 wt %; and
C: 0.64 to 0.87 wt %;
wherein the remainder comprises Fe and other unavoidable impurities.

### Claim 2 (depends on 1)

The sintered material of claim 1, further comprising one or two or more selected from the group consisting of Mn, Ni and S;
wherein a total content of Mn, Ni and S is in a range of 0.15 to 0.45 wt %.

### Claim 3 (depends on 1)

The sintered material of claim 1, wherein the sintered material does not contain Cu.

### Claim 4 (depends on 1)

The sintered material of claim 1, wherein the sintered material has a yield strength of 400 MPa or more, and a fatigue strength of 150 MPa or more.

### Claim 5 (depends on 1)

The sintered material of claim 1, wherein the sintered material has a density of 6.8 to 7.2 g/cm3.

### Claim 6 (depends on 1)

The sintered material of claim 1, wherein on a surface of the sintered material, a surface protective layer made of iron oxide is formed.

### Claim 7 (depends on 6)

The sintered material of claim 6, wherein Cu is not crystallized in the surface protective layer.

### Claim 8

A method of manufacturing a sintered material for aluminum die casting, the method comprising:
preparing an iron-based pre-alloy powder containing chromium (Cr) and molybdenum (Mo);
preparing an iron-based pre-alloy mixture by mixing carbon powder, a functional additive, and a lubricant with the iron-based pre-alloy powder;
preparing a molded material by molding the iron-based pre-alloy mixture;
preparing a sintered material by sintering the molded material; and
steam-treating the sintered material;
wherein the iron-based pre-alloy powder further includes Mn, Ni, and S; and
wherein a total content of Mn, Ni and S is in a range of 0.15 to 0.45 wt %.

### Claim 9 (depends on 8)

The method of claim 8, wherein the iron-based pre-alloy powder contains Cr: 0.72 to 0.98 wt %, and Mo: 0.10 to 0.20 wt %, wherein the remainder comprises Fe and other unavoidable impurities.

### Claim 10

(canceled)

### Claim 11 (depends on 8)

The method of claim 8, wherein the iron-based pre-alloy powder does not contain Cu.

### Claim 12 (depends on 8)

The method of claim 8, wherein the iron-based pre-alloy mixture is prepared by mixing a functional additive and a lubricant with the iron-based pre-alloy powder, so that the iron-based pre-alloy mixture contains Cr: 0.71 to 0.97 wt %, Mo: 0.10 to 0.20 wt %, C: 0.63 to 0.87 wt %, functional additive: 0.10 to 0.20 wt %, and lubricant: 0.54 to 0.66 wt %, wherein the remainder comprises Fe and other unavoidable impurities.

### Claim 13 (depends on 8)

The method of claim 8, wherein the sintered material contains Cr: 0.71 to 0.97 wt %, Mo: 0.10 to 0.20 wt %, C: 0.64 to 0.87 wt %, and functional additive: 0.10 to 0.20 wt %, wherein the remainder comprises Fe and other unavoidable impurities.

### Claim 14 (depends on 8)

The method of claim 8, wherein the preparing of the sintered material comprises sintering the molded material at a temperature of 1100 to 1150° C. for 20 to 60 minutes in a nitrogen and hydrogen mixed gas atmosphere, and then air-cooling the molded material.

### Claim 15 (depends on 8)

The method of claim 8, wherein the steam-treating of the sintered material comprises treating the sintered material in a steam atmosphere at a temperature of 400 to 600° C. for 30 to 60 minutes.

### Claim 16 (depends on 15)

The method of claim 15, wherein in the steam-treating of the sintered material, on a surface of the sintered material, a surface protective layer made of iron oxide is formed.

### Claim 17 (depends on 16)

The method of claim 16, wherein in the steam-treating of the sintered material, Cu is not crystallized in the surface protective layer.

### Claim 18 (depends on 8)

The method of claim 8, wherein after the steam-treating of the sintered material, the microstructure of the sintered material is pearlite.