# US 2024/0102120 A1 · Method for laser hardening of a card wire

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0102120 A1
- Document ID: US20240102120A1
- Status: Published application
- Kind: A1
- Application number: 18/263,937
- Filed: 2021-12-17
- Published: 2024-03-28
- Earliest claimed: 2021-02-02
- Assignees: Groz-Beckert KG
- Applicants: Groz-Beckert KG
- Inventors: Johannes BRUSKE; Jochen STAUSS
- Web page: https://patentgrep.com/patent/US20240102120A1

## CPC

- C21D 1/09: by direct application of electrical or wave energy; by particle radiation
- C21D 1/34: Methods of heating (C21D1/06 takes precedence)
- C21D 1/74: Methods of treatment in inert gas, controlled atmosphere, vacuum or pulverulent material
- C21D 6/00: Heat treatment of ferrous alloys
- C21D 9/0068: {for particular articles not mentioned below}
- C21D 9/26: for needles; for teeth for card-clothing
- C21D 9/52: for wires; for strips {; for rods of unlimited length}
- C21D 9/525: {for wire, for rods (C21D9/54 takes precedence)}
- D01G 15/88: formed from metal sheets or strips
- C21D 2221/02: Edge parts
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- D01G: PRELIMINARY TREATMENT OF FIBRES, e.g. FOR SPINNING (winding or unwinding, conducting or guiding laps, webs, slivers or rovings in general, sliver or roving cans, depositing in sliver or roving cabs B65H; preparation of fibres for paper-making D21)

## Abstract

A method for laser beam hardening of sections to be hardened (A) of a card wire (10) is disclosed. Thereby the card wire (10) is moved in a conveying direction through a working space (26). In the working space (26), an inert gas atmosphere is created by continuously or discontinuously introducing inert gas (G). In the working space (26), a laser beam area (27) is generated through which the sections to be hardened (A) of the card wire (10) are moved. Thereby the sections to be hardened (A) are heated. After exiting out of the laser beam area (27) the sections to be hardened (A) cool and are hardened by progressing through this temperature profile. The hardening in the inert gas atmosphere inside working space (26) avoids formation of oxide layers (scaling) and annealing colors.

## Claims

### Claim 1

A method for laser hardening of a card wire (10) comprising a base section (11) and multiple teeth (12) projecting from the base section, wherein the method comprises the following steps:
generating at least one continuous laser beam area (27) inside a working space (26);
supplying an inert gas (G) into the working space (26);
conveying the card wire (10) in a conveying direction (F) into the working space (26) such that a section to be hardened (A) of each tooth (12) is moved through the at least one continuous laser beam area (27), whereby at least one outer surface (18, 19) of each section to be hardened (A) is moved through the at least one continuous laser beam area (27), such that the section to be hardened (A) is heated; and
cooling of the section to be hardened (A).

### Claim 2 (depends on 1)

The method according to claim 1, wherein conveying the card wire (10) in the conveying direction comprises moving the card wire (10) non-stop continuously in the conveying direction (F).

### Claim 3 (depends on 2)

The method according to claim 2, wherein the card wire (10) is moved with a constant speed in the conveying direction (F).

### Claim 4 (depends on 1)

The method according to claim 1, wherein the at least one continuous laser beam area (27) has a non-circular contour having a length (x) in the conveying direction (F) and a width (y) orthogonal to the conveying direction (F) and wherein the width (y) is smaller than the length (x).

### Claim 5 (depends on 1)

The method according to claim 1, wherein the at least one continuous laser beam area (27) comprises at least one straight outer edge.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the at least one straight outer edge of the at least one continuous laser beam area (27) is oriented parallel to the conveying direction (F).

### Claim 7 (depends on 5)

The method according to claim 5, wherein an intensity of laser light in the at least one continuous laser beam area (27) changes abruptly at the at least one straight outer edge of the at least one continuous laser beam area (27).

### Claim 8 (depends on 1)

The method according to claim 1, wherein the at least one continuous laser beam area (27) is generated by at least one beam forming optic (31) that forms an incident laser beam (30) into an exiting laser beam (32), whereby the exiting laser beam forms the at least one continuous laser beam area (27).

### Claim 9 (depends on 8)

The method according to claim 8, further comprising capturing at least a part of the laser light of the exiting laser beam (32) with a beam dump (38).

### Claim 10 (depends on 9)

The method according to claim 9, further comprising cooling the beam dump (38) with a cooling medium (K).

### Claim 11 (depends on 9)

The method according to claim 9, wherein the beam dump (38) comprises at least one incident surface (39) for the exiting laser beam (32) arranged inclined relative to a travel direction of the laser light passing through the at least one continuous laser beam area (27).

### Claim 12 (depends on 1)

The method according to claim 1, wherein generating at least one continuous laser beam area (27) comprises emitting a laser beam (29) from a laser beam source (28) that comprises a wavelength of 900 nm to 1100 nm.

### Claim 13 (depends on 1)

The method according to claim 1, further comprising applying the laser light in the at least one continuous laser beam area (27) on the section to be hardened (A) for an application period of 50 ms and to 70 ms.

### Claim 14 (depends on 1)

The method according to claim 1, further comprising annealing the card wire (10) prior to moving the card wire (10) into the at least one laser beam area (27).

### Claim 15 (depends on 1)

The method according to claim 1, further comprising cleaning the card wire (10) prior to moving the card wire (10) into the at least one continuous laser beam area (27).

### Claim 16 (depends on 1)

The method according to claim 1, further comprising generating a first laser beam area (27a) and a second laser beam area (27b) that is spaced apart from the first laser beam area (27a).

### Claim 17 (depends on 16)

The method according to claim 16, further comprising moving a first outer surface (18) of the section to be hardened (A) through the first laser beam area (27a) and a second outer surface (19) opposite to the first outer surface (18) of the section to be hardened (A) through the second laser beam area (27b).

### Claim 18 (depends on 1)

The method according to claim 1, further comprising measuring the heating of the section to be hardened (A).