# US 2024/0101470 A1 · Window manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0101470 A1
- Document ID: US20240101470A1
- Status: Published application
- Kind: A1
- Application number: 18/217,972
- Filed: 2023-07-03
- Published: 2024-03-28
- Earliest claimed: 2022-09-28
- Assignees: Samsung Display Co., Ltd.
- Applicants: Samsung Display Co., LTD.
- Inventors: JINSU NAM; YONGKYU KANG; SEUNGHO KIM
- Web page: https://patentgrep.com/patent/US20240101470A1

## CPC

- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 23/0055: {by ion implantation}
- C03C 23/0065: {by microwave radiation}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A window manufacturing method includes preparing a glass substrate including alkali ions, providing a strengthening material on a surface of the glass substrate, and strengthening the surface of the glass substrate. The strengthening the surface of the glass substrate includes irradiating the strengthening material disposed on the glass substrate with high-frequency waves, and the strengthening material includes a salt including ion exchange target ions, which are ion-exchangeable with the alkali ions included in the glass substrate, and a high-frequency reactive material.

## Claims

### Claim 1

A window manufacturing method comprising:
preparing a glass substrate including alkali ions;
providing a strengthening material on a surface of the glass substrate; and
strengthening the surface of the glass substrate,
wherein the strengthening the surface of the glass substrate includes irradiating the strengthening material disposed on the glass substrate with high-frequency waves, and
the strengthening material includes a salt including ion exchange target ions, which are ion-exchangeable with the alkali ions included in the glass substrate, and a high-frequency reactive material.

### Claim 2 (depends on 1)

The window manufacturing method of claim 1, wherein the strengthening the surface of the glass substrate further comprises ion-exchanging the alkali ions and the ion exchange target ions with each other.

### Claim 3 (depends on 1)

The window manufacturing method of claim 1, wherein the irradiating the strengthening material with high-frequency waves comprises generating, by the high-frequency reactive material, heat in response to the high-frequency waves.

### Claim 4 (depends on 1)

The window manufacturing method of claim 1, wherein the high-frequency reactive material comprises high-frequency reactive ceramic.

### Claim 5 (depends on 4)

The window manufacturing method of claim 4, wherein the high-frequency reactive ceramic comprises at least one selected from Al2O3, ZrO2, TiO2, Co2O3, MnO2, NiO, CuO, MgO, SiO2, high-frequency reactive glass, dielectric ceramic expressed as ABO3, SiC, and doped Si,
wherein A is at least one selected from Ca, La, Sr, Ba, and Mg, and
B is at least one selected from Zn, Al, and Ti.

### Claim 6 (depends on 4)

The window manufacturing method of claim 4, wherein the high-frequency reactive ceramic comprises at least one selected from SiC, and doped Si.

### Claim 7 (depends on 4)

The window manufacturing method of claim 4, wherein the high-frequency reactive material further comprises a high-frequency reactive polymer.

### Claim 8 (depends on 7)

The window manufacturing method of claim 7, wherein the high-frequency reactive polymer comprises at least one selected from acrylonitrile butadiene styrene (ABS) copolymer, acetal, epoxy, melamine, phenylformaldehyde, polycarbonate, polyester, polyamide, polyurethane, polyvinyl chloride (PVC), thermoplastic elastomer (TPE), and silicon (Si).

### Claim 9 (depends on 1)

The window manufacturing method of claim 1, wherein the strengthening material has a form of slurry, paste, or a sheet.

### Claim 10 (depends on 1)

The window manufacturing method of claim 1, wherein the providing the strengthening material, and the strengthening the surface of the glass substrate are each performed in a non-immersion manner.

### Claim 11 (depends on 1)

The window manufacturing method of claim 1, further comprising:
removing the strengthening material from the glass substrate, the surface of which is strengthened.

### Claim 12 (depends on 1)

The window manufacturing method of claim 1, wherein the strengthening the surface of the glass substrate further comprises applying conductive heat, from an outside, to the glass substrate and the strengthening material disposed on the glass substrate, simultaneously with the irradiating the strengthening material with high-frequency waves.

### Claim 13 (depends on 1)

The window manufacturing method of claim 1, further comprising providing a high-frequency susceptor to be adjacent to the glass substrate and the strengthening material disposed on the glass substrate,
wherein the strengthening further includes irradiating the high-frequency susceptor with high-frequency waves, simultaneously with the irradiating the strengthening material disposed on the glass substrate with high-frequency waves, and
the high-frequency susceptor generates heat in response to the high-frequency waves radiated thereto.

### Claim 14 (depends on 1)

The window manufacturing method of claim 1, further comprising providing a high-frequency susceptor directly on the strengthening material disposed on the glass substrate,
wherein the strengthening further includes irradiating the high-frequency susceptor with high-frequency waves, simultaneously with the irradiating the strengthening material disposed on the glass substrate with high-frequency waves, and
the high-frequency susceptor generates heat in response to the high-frequency waves radiated thereto.

### Claim 15 (depends on 14)

The window manufacturing method of claim 14, further comprising:
providing a heat-loss preventing material directly on the high-frequency susceptor.

### Claim 16

A window manufacturing method comprising:
preparing a glass substrate;
providing a strengthening material including a high-frequency reactive material on a surface of the glass substrate; and
strengthening the surface of the glass substrate by irradiating the strengthening material disposed on the glass substrate with high-frequency waves.

### Claim 17 (depends on 16)

The window manufacturing method of claim 16, wherein the strengthening the surface of the glass substrate comprises generating, by the high-frequency reactive material, heat in response to the high-frequency waves.

### Claim 18 (depends on 16)

The window manufacturing method of claim 16, wherein the high-frequency reactive material comprises at least one selected from SiC and doped Si.

### Claim 19

A window manufacturing method comprising:
preparing a glass substrate;
providing a strengthening material including a high-frequency wave reaction material on a surface of the glass substrate; and
strengthening the glass substrate by irradiating the strengthening material disposed on the glass substrate with high-frequency waves,
wherein the strengthening material includes high-frequency reactive ceramic,
the high-frequency reactive ceramic includes at least one selected from Al2O3, ZrO2, TiO2, Co2O3, MnO2, NiO, CuO, MgO, SiO2, high-frequency reactive glass, dielectric ceramic expressed as ABO3, SiC, and doped Si,
wherein A is at least one selected from Ca, La, Sr, Ba, and Mg, and
B is at least one selected from Zn, Al, and Ti.

### Claim 20 (depends on 19)

The window manufacturing method of claim 19, wherein the strengthening material further comprises a high-frequency reactive polymer, and
the polymer includes at least one selected from acrylonitrile butadiene styrene copolymer (ABS), acetal, epoxy, melamine, phenylformaldehyde, polycarbonate, polyester, polyamide, polyurethane, polyvinyl chloride (PVC), thermoplastic elastomer (TPE), and silicon (Si).