# US 2024/0097141 A1 · Electrode for secondary battery, secondary battery provided with same, and method for manufacturing electrode for secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0097141 A1
- Document ID: US20240097141A1
- Status: Published application
- Kind: A1
- Application number: 17/766,938
- Filed: 2020-11-24
- Published: 2024-03-21
- Earliest claimed: 2019-11-27
- Assignees: Vehicle Energy Japan Inc.
- Applicants: Vehicle Energy Japan Inc.
- Inventors: Motonari KIFUNE
- Web page: https://patentgrep.com/patent/US20240097141A1

## CPC

- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/75: Wires, rods or strips
- H01M 4/139: Processes of manufacture
- H01M 4/625: {Carbon or graphite}
- H01M 10/052: Li-accumulators
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- Y10T 29/53135: Storage cell or battery
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present disclosure provides an electrode for a secondary battery capable of measuring the width of a first mixture layer and the width of a second mixture layer when the first mixture layer and the second mixture layer are stacked and formed on the surface of a metal foil. A positive electrode body (electrode for a secondary battery) includes a strip-like positive electrode foil and a positive electrode mixture layer provided on the positive electrode foil. The positive electrode mixture layer includes a first positive electrode mixture layer provided on the positive electrode foil and a second positive electrode mixture layer provided on the first positive electrode mixture layer. The first positive electrode mixture layer has a width greater than a width of the second positive electrode mixture layer.

## Claims

### Claim 1

An electrode for a secondary battery comprising:
a strip-like metal foil; and
a mixture layer provided on the metal foil,
wherein:
the mixture layer includes a first mixture layer provided on the metal foil and a second mixture layer provided on the first mixture layer,
the first mixture layer has a width greater than a width of the second mixture layer,
the first mixture layer and the second mixture layer contain carbon particles,
a content of the carbon particles of the first mixture layer is higher than a content of the carbon particles of the second mixture layer, and
the first mixture layer has a smaller L* value in a L*a*b* color system by 4 or larger as compared to the second mixture layer.

### Claim 2

(canceled)

### Claim 3 (depends on 1)

The electrode for a secondary battery according to claim 1, wherein an average particle diameter of the carbon particles of the first mixture layer is smaller than an average particle diameter of the carbon particles of the second mixture layer.

### Claim 4

(canceled)

### Claim 5 (depends on 1)

A secondary battery comprising the electrode for a secondary battery according to claim 1 as a positive electrode.

### Claim 6

A method for manufacturing an electrode for a secondary battery including a mixture layer provided on a strip-like metal foil, the mixture layer including a first mixture layer provided on the metal foil and a second mixture layer provided on the first mixture layer, the method comprising:
applying a first mixture slurry and a second mixture slurry, each containing carbon particles, in a stacked state over the metal foil to form a first mixture slurry layer on the metal foil and to form a second mixture slurry layer on the first mixture slurry layer, the second mixture slurry having a content of the carbon particles at least 4% by weight higher than a content of the carbon particles of the first mixture slurry, the second mixture slurry layer having a width less than a width of the first mixture slurry layer;
drying the first mixture slurry layer and the second mixture slurry layer to form the first mixture layer and the second mixture layer; and
converting an image obtained by detecting light emitted to and reflected on the metal foil, the first mixture layer, and the second mixture layer into values in a L*a*b* color system for each pixel, detecting a boundary portion between the first mixture layer and the second mixture layer where a difference in L* value is 4 or larger, and measuring a width of the first mixture layer and a width of the second mixture layer simultaneously.