# US 2024/0075446 A1 · Device for removing iron from nickel-cobalt-manganese sulfuric acid solution and method for continuously removing iron ions from nickel-cobalt-manganese sulfuric acid solution at low temperature

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0075446 A1
- Document ID: US20240075446A1
- Status: Published application
- Kind: A1
- Application number: 18/487,944
- Filed: 2023-10-16
- Published: 2024-03-07
- Earliest claimed: 2021-04-25
- Assignees: Hunan Jin Yuan New Materials Joint Stock Company Limited
- Applicants: Hunan Jin Yuan New Materials Joint Stock Company Limited
- Inventors: Xunbing LIU; Can PENG; Zhen LIU; Quncheng ZHOU; Zi WANG; Xiongwu DONG; Shanmu WU; Jianjun OUYANG
- Web page: https://patentgrep.com/patent/US20240075446A1

## CPC

- B01J 19/0066: {Stirrers (mixing per se B01F)}
- B01J 19/0086: {Processes carried out with a view to control or to change the pH-value; Applications of buffer salts; Neutralisation reactions}
- B01J 19/18: Stationary reactors having moving elements inside (B01J19/08, B01J19/26 take precedence)
- B01J 19/1862: {placed in series}
- B01J 19/1875: {internally, i.e. the mixture circulating inside the vessel such that the upwards stream is separated physically from the downwards stream(s)}
- C01G 49/00: Compounds of iron
- B01J 2219/00177: controlling the pH
- Y02P 10/20: Recycling
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A device for removing iron from a nickel-cobalt-manganese sulfuric acid solution and a method for continuously removing iron ions from a nickel-cobalt-manganese sulfuric acid solution. The device has an iron removal reactor (2) having a stirrer (3) and an iron removal reactor inner cylinder (5) and an aging reactor (9) having an aging reactor stirrer (7) and an automatic stone powder feeder (8), a mixing feed pipe (12) and a carbonate solution feed pipe (4) are arranged in an interlayer between the iron removal reactor (2) and the iron removal reactor inner cylinder (5), a mixer (1) for a preheating the device is arranged at a top of the mixing feed pipe (12), a compressed air inlet (11) and a feed inlet (10) of a solution to be subjected to iron removal are arranged in the mixer (1). Further disclosed is a method for removing iron of the device.

## Claims

### Claim 1

A device for removing iron from a nickel-cobalt-manganese sulfuric acid solution, provided with an iron removal reactor and an aging reactor, a first stirrer being arranged in the iron removal reactor, a second stirrer being arranged in the aging reactor, and the iron removal reactor being connected with the aging reactor by an overflow port connecting pipe, wherein an iron removal reactor inner cylinder is arranged in the iron removal reactor, a mixing feed pipe and a carbonate solution feed pipe are arranged in an interlayer between the iron removal reactor and the iron removal reactor inner cylinder, a mixer is arranged at a top portion of the mixing feed pipe, a compressed air inlet and a feed inlet of a solution to be subjected to iron removal are arranged in the mixer, and an automatic stone powder feeder is arranged on the aging reactor.

### Claim 2 (depends on 1)

The device for removing iron from the nickel-cobalt-manganese sulfuric acid solution according to claim 1, wherein the mixer is provided with a mixing bin, the mixing bin has a trapezoidal structure with a larger upper portion and a smaller lower portion, the lower portion of the mixing bin is provided with an electric heating portion, the compressed air inlet is arranged in a top portion of the mixing bin, the feed inlet of the solution to be subjected to iron removal is arranged in a side surface of the mixing bin, so that the solution to be subjected to iron removal is tangent to compressed air from the side surface, a diameter of an outlet in a bottom portion of the mixing bin is ½ of a diameter of the bottom portion of the mixing bin, the outlet in the bottom portion of the mixing bin is connected with the mixing feed pipe, and the mixing feed pipe penetrates through the electric heating portion.

### Claim 3 (depends on 1)

The device for removing iron from the nickel-cobalt-manganese sulfuric acid solution according to claim 1, wherein a bottom end of the mixing feed pipe is 30 cm to 40 cm away from a bottom surface of the iron removal reactor, a direction of an outlet of the mixing feed pipe is tangent to a stirring direction of the stirrer, the carbonate solution feed pipe is 30 cm to 40 cm away from the bottom surface of the iron removal reactor, and a direction of an outlet of the carbonate solution feed pipe is tangent to the stirring direction of the stirrer.

### Claim 4 (depends on 1)

The device for removing iron from the nickel-cobalt-manganese sulfuric acid solution according to claim 1, wherein the mixing feed pipe is symmetrically arranged with the carbonate solution feed pipe.

### Claim 5 (depends on 1)

The device for removing iron from the nickel-cobalt-manganese sulfuric acid solution according to claim 1, wherein a height-diameter ratio of the iron removal reactor 2 is 1.0 to 2.5:1.

### Claim 6 (depends on 1)

The device for removing iron from the nickel-cobalt-manganese sulfuric acid solution according to claim 1, wherein the stirrer is composed of a motor and a stirring vane, the stirring vane adopts a cross-shaped double-layer stirring blade, a diameter of the stirring blade is ⅓ of a diameter of the iron removal reactor, a lowermost stirring blade is 50 cm to 80 cm away from a bottom portion of the reactor, a distance between upper and lower stirring blades is 50 cm to 115 cm, the stirrer of the aging reactor is composed of a motor and a stirring vane, the stirring vane adopts a cross-shaped double-layer stirring blade, a diameter of the stirring blade is ⅓ of a diameter of the aging reactor, a lowermost stirring blade is 50 cm to 80 cm away from a bottom portion of the reactor, and a distance between upper and lower stirring blades is 50 cm to 115 cm.

### Claim 7 (depends on 1)

The device for removing iron from the nickel-cobalt-manganese sulfuric acid solution according to claim 1, wherein the iron removal reactor inner cylinder is made into a cylindrical shape with open top and bottom portions, and fixed on an inner wall of the iron removal reactor by a support stirring frame, and a diameter of the inner cylinder is 70% to 80% of a diameter of the iron removal reactor.

### Claim 8

A method for continuously removing iron ions from a nickel-cobalt-manganese sulfuric acid solution at a low temperature by using a device for removing iron from a nickel-cobalt-manganese sulfuric acid solution, comprising the following steps of:
a. preparing carbonate: preparing a carbonate solution or slurry first, wherein a carbonate concentration is 120 g/L to 240 g/L, and a temperature is controlled to be 40° C. to 45° C.;
b. injecting a solution to be subjected to iron removal: injecting a nickel-cobalt-manganese sulfuric acid solution to be subjected to iron removal and compressed air into an iron removal reactor through a mixer with a preheating device;
c. injecting the carbonate solution: adding the prepared carbonate solution or slurry into the iron removal reactor while injecting the nickel-cobalt-manganese sulfuric acid solution to be subjected to iron removal, and controlling a PH value of a process reaction to be 2.5 to 3.5;
d. carrying out a stirring reaction: when the solution to be subjected to iron removal and the carbonate solution are injected, stirring the mixture during injecting, controlling a process temperature to be 40° C. to 45° C., and after the reactor is full, making the reaction slurry flow into the aging reactor;
e. adding stone powder: after the reaction slurry enters the aging reactor, stirring the slurry, and then adding the stone powder through an automatic feed device; and
f. filtering the solution: filtering the solution after the aging reactor is full, wherein a filter residue is an iron slag, and a filtrate is the iron-removed nickel-cobalt-manganese sulfuric acid solution.

### Claim 9 (depends on 8)

The method for continuously removing iron ions from the nickel-cobalt-manganese sulfuric acid solution at the low temperature by using the device for removing iron from the nickel-cobalt-manganese sulfuric acid solution according to claim 8, wherein in the step of injecting the iron solution to be subjected to iron removal, a flow rate of the solution is calculated according to a volume of the reactor by the following formula: flow rate=volume V of reactor m3/(2-5.5 hours), and a flow rate of the compressed air is 2 to 8 times that of the iron solution to be subjected to iron removal.

### Claim 10 (depends on 8)

The method for continuously removing iron ions from the nickel-cobalt-manganese sulfuric acid solution at the low temperature by using the device for removing iron from the nickel-cobalt-manganese sulfuric acid solution according to claim 8, wherein an addition amount of the stone powder is 0.05 to 0.5 kg/m3 solution.

### Claim 11 (depends on 8)

A nickel-cobalt-manganese sulfuric acid solution prepared by the method for continuously removing iron ions from the nickel-cobalt-manganese sulfuric acid solution at the low temperature by using the device for removing iron from the nickel-cobalt-manganese sulfuric acid solution according to claim 8.