# US 2024/0069428 A1 · Reflective mask blank, reflective mask, reflective mask manufacturing method, and semiconductor device manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0069428 A1
- Document ID: US20240069428A1
- Status: Published application
- Kind: A1
- Application number: 18/039,466
- Filed: 2021-12-08
- Published: 2024-02-29
- Earliest claimed: 2020-12-22
- Assignees: Hoya Corporation
- Applicants: Hoya Corporation
- Inventors: Yohei IKEBE
- Web page: https://patentgrep.com/patent/US20240069428A1

## CPC

- G03F 1/24: Reflection masks; Preparation thereof
- C03C 17/225: {Nitrides}
- C03C 17/3636: {one layer at least containing silicon, hydrogenated silicon or a silicide}
- C03C 17/3649: {made of metals other than silver}
- C03C 17/3665: {specially adapted for use as photomask}
- C23C 14/0641: {Nitrides (C23C14/0617 takes precedence)}
- C23C 14/083: {of refractory metals or yttrium}
- C23C 14/185: {by cathodic sputtering}
- C23C 14/35: by application of a magnetic field, e.g. magnetron sputtering {(C23C14/3457 takes precedence)}
- C23C 14/46: by ion beam produced by an external ion source
- G03F 1/74: by charged particle beam [CPB], e.g. focused ion beam
- G03F 1/84: Inspecting
- C03C 2217/281: Nitrides
- C03C 2218/155: by reactive sputtering
- C03C 2218/156: by magnetron sputtering
- C03C 2218/365: Coating different sides of a glass substrate
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A reflective mask blank includes a multilayer reflective film, a first thin film, and a second thin film in this order on a main surface of a substrate, a relative reflectance R2 of the second thin film with respect to a reflectance of the multilayer reflective film in the light of 13.5 nm wavelength is 3% or more, and an extinction coefficient k1 of the first thin film in the light of 13.5 nm wavelength and a thickness d1 [nm] of the first thin film satisfy a relationship of (Formula 1). 21.5×k12×d12−52.5×k1×d1+32.1>R2 (Formula 1)

## Claims

### Claim 1

A reflective mask blank comprising:
a substrate; and
a multilayer reflective film,
a first thin film and
a second thin film,
in this order on a main surface of the substrate, wherein
a relative reflectance R2 of the second thin film relative to a reflectance of the multilayer reflective film with respect to light having a wavelength of 13.5 nm is 3% or more, and
when an extinction coefficient of the first thin film with respect to the light having a wavelength of 13.5 nm is k1 and a thickness of the first thin film is d1 [nm], a relationship of Formula 1 is satisfied.
21.5×k12×d12−52.5×k1×d1+32.1>R2 (Formula 1)

### Claim 2 (depends on 1)

The reflective mask blank according to claim 1,
wherein the relative reflectance R2 is approximately 32% or less.

### Claim 3 (depends on 1)

The reflective mask blank according to claim 1,
wherein the extinction coefficient k1 of the first thin film is approximately 0.05 or less.

### Claim 4 (depends on 1)

The reflective mask blank according to claim 1,
wherein the thickness d1 of the first thin film is 1 nm or more and 30 nm or less.

### Claim 5 (depends on 1)

The reflective mask blank according to claim 1,
wherein the first thin film contains a metal element and at least one element of oxygen and nitrogen.

### Claim 6 (depends on 1)

The reflective mask blank according to claim 1,
wherein the second thin film contains a metal element such that a phase difference between with respect to reflected light having a wavelength of 13.5 nm between the second thin film and the multilayer reflective film is between 130° to 230° and has a relative reflectance contrast of greater than 40% with respect to the first thin film.

### Claim 7 (depends on 1)

The reflective mask blank according to claim 1, further comprising
a protective film between the multilayer reflective film and the first thin film.

### Claim 8 (depends on 7)

The reflective mask blank according to claim 7,
wherein the protective film contains ruthenium.

### Claim 9

A reflective mask blank comprising:
a substrate; and
a multilayer reflective film, a first thin film, and a second thin film, in this order on a main surface of the substrate, in which a transfer pattern is formed in the first thin film and the second thin film; wherein
a relative reflectance R2 of the second thin film relative to a reflectance of the multilayer reflective film with respect to light having a wavelength of 13.5 nm is 3% or more and a phase difference between with respect to reflected light having a wavelength of 13.5 nm between the second thin film and the multilayer reflective film is between 130° to 230°, and
wherein a contrast of the first thin film and second thin film with respect to light having a wavelength of 13.5 nm is greater than 40%.

### Claim 10

A method of manufacturing a reflective mask using the reflective mask blank that comprises a substrate, a multilayer reflective film, a protective film, a first thin film, and a second thin film in this order on a main surface of the substrate, method comprising:
forming a transfer pattern in the second thin film without substantially forming the transfer pattern in the first thin film;
performing a defect inspection of the transfer pattern by using inspection light including light having a wavelength of 13.5 nm with respect to the second thin film in which the transfer pattern is formed;
performing a defect repair by irradiating defects detected by the defect inspection which exist in the transfer pattern of the second thin film with charged particles while supplying a fluorine-containing substance to the defects; and
forming another transfer pattern in the first thin film after the defect repair.

### Claim 11

(canceled)

### Claim 12

(canceled)

### Claim 13 (depends on 9)

The reflective mask blank according to claim 9,
wherein the relative reflectance R2 is approximately 32% or less.

### Claim 14 (depends on 9)

The reflective mask blank according to claim 9,
wherein an extinction coefficient k1 of the first thin film is approximately 0.05 or less.

### Claim 15 (depends on 9)

The reflective mask blank according to claim 9,
wherein a thickness d1 of the first thin film is 1 nm or more and 30 nm or less.

### Claim 16 (depends on 9)

The reflective mask blank according to claim 9,
wherein the first thin film contains a metal element and at least one element of oxygen and nitrogen.

### Claim 17 (depends on 9)

The reflective mask blank according to claim 9 further comprising
a protective film between the multilayer reflective film and the first thin film.

### Claim 18 (depends on 9)

The reflective mask blank according to claim 9 wherein when an extinction coefficient of the first thin film with respect to the light having a wavelength of 13.5 nm is k1 and a thickness of the first thin film is d1 [nm], a relationship of Formula 1 is satisfied.
21.5×k12×d12−52.5×k1×d1+32.1>R2 (Formula 1)

### Claim 19 (depends on 9)

The reflective mask blank according to claim 9,
wherein the second film comprises an alloy of one of chromium and ruthenium or tantalum and boron.

### Claim 20 (depends on 1)

The reflective mask blank according to claim 1,
wherein the second film comprises an alloy of one of chromium and ruthenium or tantalum and boron.