# US 2024/0067804 A1 · Energy-saving and environment-friendly method for preparing nanocellulose based flexible conductive film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0067804 A1
- Document ID: US20240067804A1
- Status: Published application
- Kind: A1
- Application number: 18/504,118
- Filed: 2023-11-07
- Published: 2024-02-29
- Earliest claimed: 2022-05-19
- Assignees: Zhejiang Sci-Tech University
- Applicants: Zhejiang Sci-Tech University
- Inventors: Yanjun TANG; Xingfei ZHAO
- Web page: https://patentgrep.com/patent/US20240067804A1

## CPC

- C08L 1/02: Cellulose; Modified cellulose
- H01G 11/26: characterised by their structure, e.g. multi-layered, porosity or surface features
- C08J 3/14: by precipitation from solutions {(C08J3/122 takes precedence)}
- C08J 5/18: Manufacture of films or sheets
- C08K 3/042: {Graphene or derivatives, e.g. graphene oxides}
- C08L 1/04: Oxycellulose; Hydrocellulose {, e.g. microcrystalline cellulose}
- H01G 11/30: characterised by their material
- H01G 11/36: Nanostructures, e.g. nanofibres, nanotubes or fullerenes
- H01G 11/86: specially adapted for electrodes (carbonisation or activation of carbon for the manufacture of electrodes H01G11/34)
- C08J 2301/02: Cellulose; Modified cellulose
- C08J 2301/04: Oxycellulose; Hydrocellulose
- C08J 2401/02: Cellulose; Modified cellulose
- C08J 2401/04: Oxycellulose; Hydrocellulose
- Y02E 60/13: Energy storage using capacitors
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present disclosure discloses methods for preparing a composite film based on reduced graphene oxide, cellulose nanocrystals, and cellulose nanofibers. The method mainly includes: 1. preparing a suspension mixed with graphite oxide and cellulose; 2. centrifuging the suspension obtained in the step (1) and washing the sediment after centrifuging with deionized water to obtain a solution, homogenizing the solution in a high-pressure homogenizer to obtain a suspension mixed with graphene oxide, cellulose nanocrystals, and cellulose nanofibers; and 3. drying the suspension mixed with graphene oxide, cellulose nanocrystals, and cellulose nanofibers in a petri dish, and soaking a dried film in a hydroiodic acid solution; and washing the soaked film with deionized water to obtain the composite film of reduced graphene oxide, cellulose nanocrystals, and cellulose nanofibers. The composite film obtained has a higher specific capacitance and a better cycle stability than pure reduced graphene oxide obtained under a same preparation condition.

## Claims

### Claim 1

A method for preparing a nanocellulose based flexible conductive film, comprising:
in step (a), centrifuging a suspension mixed with graphite oxide and cellulose and washing a sediment after centrifuging with water to obtain a solution, homogenizing the solution to obtain a suspension mixed with graphene oxide, cellulose nanocrystals, and cellulose nanofibers;
in step (b), drying the suspension mixed with graphene oxide, cellulose nanocrystals, and cellulose nanofibers to obtain a dried film;
reducing the dried film to obtain reduced graphene oxide, cellulose nanocrystals, and cellulose nanofibers; and
washing reduced film to obtain the nanocellulose based flexible conductive film based on the reduced graphene oxide, the cellulose nanocrystals, and the cellulose nanofibers, wherein a mass ratio of the reduced graphene oxide, the cellulose nanocrystals, and the cellulose nanofibers in the nanocellulose based flexible conductive film in the step (b) is 1:0.1-1:0.1-2.

### Claim 2 (depends on 1)

The method of claim 1, wherein the suspension mixed with graphite oxide and cellulose in step (a) is prepared by:
mixing graphite, potassium nitrate, potassium permanganate, and sulfuric acid in an ice water bath to obtain a mixture, and transferring the mixture to a warm water bath to perform reaction;
adding water to a reaction system including the mixture, increasing a temperature of the water bath, and stirring;
lowering the temperature of the water bath, adding hardwood microcrystalline cellulose, and stirring; and
terminating the reaction to obtain the suspension mixed with graphite oxide and cellulose.

### Claim 3 (depends on 2)

The method of claim 2, wherein the terminating the reaction to obtain the suspension mixed with graphite oxide and cellulose includes:
adding hydrogen peroxide solution to terminate the reaction to obtain the suspension mixed with graphite oxide and cellulose.

### Claim 4 (depends on 2)

The method of claim 2, wherein a temperature of the warm water bath is 35° C., a reaction time in the warm water bath is 0.5 h, the increased temperature of the water bath is 80° C., and the lowered temperature of the water bath is 50° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein in the step (a), a count of centrifugation and washing is 2 times, a centrifugation rate is 10,000 rpm, and a time of a single centrifugation is 10 min.

### Claim 6 (depends on 1)

The method of claim 1, wherein in the step (a), the homogenizing the solution to obtain a suspension mixed with graphene oxide, cellulose nanocrystals, and cellulose nanofibers includes:
homogenizing the solution in a high-pressure homogenizer to obtain the suspension mixed with graphene oxide, cellulose nanocrystals, and cellulose nanofibers.

### Claim 7 (depends on 6)

The method of claim 6, wherein a pressure in the high-pressure homogenizer is 60 MPa-80 MPa and a homogenization time is 0.5 h.

### Claim 8 (depends on 1)

The method of claim 1, wherein in the step (b), a drying temperature to obtain the dried film is 45° C. and a drying time to obtain the dried film is 12 h.

### Claim 9 (depends on 1)

The method of claim 1, wherein the reducing the dried film to obtain reduced graphene oxide, cellulose nanocrystals, and cellulose nanofibers in the step (b) includes:
soaking the dried film in a hydroiodic acid solution to obtain the reduced graphene oxide, the cellulose nanocrystals, and the cellulose nanofibers.

### Claim 10 (depends on 9)