# US 2024/0043591 A1 · Optical grade moulding compositions having increased heat resistance

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0043591 A1
- Document ID: US20240043591A1
- Status: Published application
- Kind: A1
- Application number: 18/256,318
- Filed: 2021-12-08
- Published: 2024-02-08
- Earliest claimed: 2020-12-09
- Assignees: Rohm Co., Ltd.
- Applicants: Röhm GmbH
- Inventors: Rüdiger Carloff; Werner Arnold; Gerald Dietrich
- Web page: https://patentgrep.com/patent/US20240043591A1

## CPC

- C08F 220/14: Methyl esters {, e.g. methyl (meth)acrylate}
- C08F 6/003: {from polymer solutions, suspensions, dispersions or emulsions without recovery of the polymer therefrom}
- C08F 6/005: {from solid polymers}
- C08F 8/16: Lactonisation
- C08L 35/02: Homopolymers or copolymers of esters (C08L35/06, C08L35/08 take precedence)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A process can be used for manufacturing an acrylic copolymer having increased heat resistance, high transparency, and improved adhesion to metal surfaces. The process involves polymerizing a monomer mixture, optional heating of the copolymer mixture, and removing volatile components from the copolymer mixture by degassing. Moulding compositions containing this copolymer are highly suitable for manufacturing optical elements for optoelectronic devices containing acrylic and metallic or ceramic parts.

## Claims

### Claim at position 1

1: A process for the manufacturing of a moulding composition comprising a copolymer, the process comprising:
(a) polymerizing in a radical copolymerization in a polymerization reactor, a monomer mixture comprising
from 80.0 to 99.9 wt.-% of methyl methacrylate; and
from 0.1 to 20.0 wt.-% of a compound represented by formula (I)
wherein the substituent R1 is a hydrogen atom or a hydrocarbon group having from 1 to 6 carbon atoms,
optionally, from 0.0 to 19.9 wt. % of a monomer selected from the group consisting of methyl acrylate, ethyl acrylate, and styrene;
a polymerisation initiator; and
optionally, a chain transfer agent;
to form a copolymer mixture comprising the copolymer and volatile components;
(b) optionally, heating the copolymer mixture, obtained in (a) to a temperature from 100° C. to 300° C. in a heating unit; and
(c) degassing the copolymer mixture to remove the volatile components from the copolymer mixture, to form a copolymer melt in a degassing unit, the degassing unit comprising
at least one copolymer mixture feed port,
at least one melt outlet die, and
at least one degassing device, the degassing device comprising
at least one degassing zone,
at least one gas outlet, and
at least one copolymer melt outlet,
wherein
a temperature of the copolymer melt Tv, in ° C., in the last degassing zone, in relation to a direction of conveying of the copolymer melt,
a temperature of the copolymer melt 16, in ° C., entering the at least one melt outlet die, and
a total residence time t, in s, of the copolymer melt between the last degassing zone, and the at least one melt outlet die of the degassing unit,
are adjusted in such a way that the term
4.981·10−8·t·exp(0.0517·(1.5·Tv+0.5·To)/2)
is lower than 8.

### Claim at position 2 (depends on 1)

2: The process according to claim 1, wherein the term (1.5·Tv+0.5·To)/2), in ° C., of the copolymer melt in the last degassing zone of the degassing device in (c) is between 230° C. and 290° C.

### Claim at position 3 (depends on 1)

3: The process according to claim 1, wherein the total residence time t, in s, of the copolymer melt between the last degassing zone, in relation to the direction of conveying of the copolymer melt, and the at least one melt outlet die is in the range of 10 s to 200 s.

### Claim at position 4 (depends on 1)

4: The process according to claim 1, wherein the degassing unit employed in (c) further comprises at least one melt filter, located between the last degassing zone of the degassing device and the at least one melt outlet die.

### Claim at position 5 (depends on 1)

5: The process according to claim 1, wherein an absolute pressure in the last degassing zone of the degassing device, in relation to the direction of conveying of the copolymer melt, is in the range of 1 mbar to 300 mbar.

### Claim at position 6 (depends on 1)

6: The process according to claim 1, wherein the polymerization reactor in (a) is a discontinuously or continuously operated stirred tank reactor, a continuously operated tubular reactor, a discontinuously or continuously operated loop reactor, or a combination of any those, and
wherein if several reactors are employed, they are operated in parallel or are sequentially connected.

### Claim at position 7 (depends on 1)

7: The process according to claim 1, wherein the degassing device in (c) is selected from the group consisting of a degassing extruder, degassing kneader, and one or several flash chambers.

### Claim at position 8 (depends on 1)

8: The process according to claim 1, wherein the copolymer comprises
from 80.0 to 99.5 wt.-% of repeating units derived from methyl methacrylate;
from 0.5 to 20.0 wt.-% of repeating units derived from the compound represented by formula (I)
wherein the substituent R1 is a hydrogen atom or a hydrocarbon group having from 1 to 6 carbon atoms; and,
optionally, from 0.0 to 19.5 wt-% of repeating units derived from methyl acrylate, ethyl acrylate, or styrene.

### Claim at position 9 (depends on 1)

9: A moulding composition, obtainable by the process according to claim 1, the moulding composition comprising the copolymer, the copolymer comprising
from 80.0 to 99.9 wt-% of repeating units derived from methyl methacrylate; and
from 0.1 to 20.0 wt.-% of repeating units derived from the compound represented by formula (I)
wherein the substituent R1 is a hydrogen atom or a hydrocarbon group having from 1 to 6 carbon atoms;
optionally, from 0.0 to 19.9 wt.-% of repeating units derived from methyl acrylate, ethyl acrylate, or styrene; and
not more than 1.5 wt.-% of repeating units represented by formula (II)
wherein the substituents R2 and R3 are independently a hydrogen atom or a hydrocarbon group having from 1 to 6 carbon atoms.

### Claim at position 10 (depends on 9)

10: The moulding composition according to claim 9, wherein the moulding composition comprises
not more than 1,400 ppm of methanol, and/or
not more than 1,800 ppm of methacrylic acid, and/or
not more than 5,000 ppm of methyl methacrylate.

### Claim at position 11 (depends on 9)

11: The moulding composition according to claim 9, wherein the copolymer has a weight average molecular weight, determined by GPC, of from 60,000 g/mol to 400,000 g/mol.

### Claim at position 12 (depends on 9)

12: The moulding composition according to claim 9, wherein a ratio of the weight of repeating units represented by formula (II) (II)
to
the weight of repeating units derived from the compound represented by formula (I)
is below 0.2.

### Claim at position 13 (depends on 9)

13: The moulding composition according to claim 9, further comprising at least one additive selected from the group consisting of UV absorbers, UV stabilizers, anti-oxidants, colourants, flow improver, scattering aids, lubricants, processing colour stabilizers, demoulding aids, and a combination of any of those.

### Claim at position 14 (depends on 9)

14: A moulded article, obtainable from the moulding composition according to claim 9, by a process selected from the group consisting of injection moulding and extrusion.

### Claim at position 15 (depends on 14)

15: The moulded article according to claim 14, wherein the moulded article is a component of an optoelectronic device; optical element; lamp cover, light guide, optical lens, or black coloured pillar trim.

### Claim at position 16 (depends on 1)

16: The process according to claim 1, wherein the monomer mixture comprises:
from 85.0 to 98.0 wt.-% of the methyl methacrylate;
from 2.0 to 8.0 wt.-% of the compound represented by formula (I); and
from 0.0 to 7.0 wt.-% of the monomer selected from the group consisting of methyl acrylate, ethyl acrylate, and styrene.

### Claim at position 17 (depends on 1)

17: The process according to claim 1, wherein the temperature of the copolymer melt Tv, the temperature of the copolymer melt To, and the total residence time t, are adjusted in such a way that the term
4.981·10−8·t·exp(0.0517·(1.5·Tv+0.5·To)/2)
is lower than 2.

### Claim at position 18 (depends on 9)

18: The moulding composition according to claim 9, wherein the copolymer comprises:
from 85.0 to 98.0 wt-% of the repeating units derived from methyl methacrylate;
from 2.0 to 8.0 wt.-% of the repeating units derived from the compound represented by formula (I);
from 0.0 to 7.0 wt.-% of the repeating units derived from methyl acrylate, ethyl acrylate, or styrene; and
not more than 1.0 wt.-% of the repeating units represented by formula (II).

### Claim at position 19 (depends on 10)

19: The moulding composition according to claim 10, wherein the moulding composition comprises:
not more than 1,000 ppm of methanol, and/or
not more than 1,500 ppm of methacrylic acid, and/or
not more than 4,000 ppm of methyl methacrylate.

### Claim at position 20 (depends on 15)

20: The moulded article according to claim 15, wherein the moulded article is a light emitting diode, an optical sensor, or a solar cell.