# US 2024/0043313 A1 · Alkali doped optical fiber with reduced attenuation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0043313 A1
- Document ID: US20240043313A1
- Status: Published application
- Kind: A1
- Application number: 18/226,816
- Filed: 2023-07-27
- Published: 2024-02-08
- Earliest claimed: 2022-08-05
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Sushmit Sunil Kumar Goyal; Craig Daniel Nie; Pushkar Tandon
- Web page: https://patentgrep.com/patent/US20240043313A1

## CPC

- C03B 37/01245: {by drawing and collapsing}
- C03B 37/018: by glass deposition on a glass substrate, e.g. by {inside-, modified-, plasma- or plasma modified-} chemical vapour deposition {[ICVD, MCVD, PCVD, PMCVD], i.e. by thin layer coating on the inside or outside of a glass tube or on a glass rod} (C03B37/016 takes precedence; surface treatment of glass by coating with glass C03C17/02)
- C03B 37/01262: {Depositing additional preform material as liquids or solutions, e.g. solution doping of preform tubes or rods}
- C03B 37/01453: {for doping the preform with flourine}
- C03B 37/01853: {Thermal after-treatment of preforms, e.g. dehydrating, consolidating, sintering}
- C03B 37/02718: {Thermal treatment of the fibre during the drawing process, e.g. cooling (coating C03C25/10)}
- C03B 2201/12: doped with fluorine (C03B2201/14 takes precedence)
- C03B 2201/50: doped with alkali metals
- C03B 2205/40: Monitoring or regulating the draw tension or draw rate
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

A method of manufacturing an optical fiber, the method includes drawing a first optical fiber preform at a first draw tension to produce a first alkali doped optical fiber and drawing the first optical fiber preform at a second draw tension to produce a second alkali doped optical fiber, measuring the attenuation of the first alkali doped optical fiber and the second alkali doped optical fiber such that the second alkali doped optical fiber has a lower attenuation. Additionally, the method includes setting the draw tension to the second draw tension and drawing a second optical fiber preform at the second draw tension to produce a third alkali doped optical fiber. The third alkali-doped optical fiber has an attenuation at 850 nm of about 1.50 dB/km or less and an attenuation at 1550 nm of about 0.155 dB/km or less.

## Claims

### Claim 1

A method of manufacturing an optical fiber, the method comprising:
forming an alkali-doped silica-containing glass tube;
collapsing the glass tube to form a first glass rod;
depositing silica soot on the first glass rod to form a first glass body;
depositing additional silica soot on the first glass body;
exposing the silica soot on the first glass body to a halide dopant;
exposing the silica soot on the first glass body to a reducing agent;
consolidating the silica soot on the first glass body to form a first preform precursor;
forming a first optical fiber preform from the first preform precursor;
drawing the first optical fiber preform at a first draw tension to produce a first alkali doped optical fiber and drawing the first optical fiber preform at a second draw tension to produce a second alkali doped optical fiber;
measuring the attenuation of the first alkali doped optical fiber and the second alkali doped optical fiber such that the first alkali doped optical fiber has a first measured attenuation and the second alkali doped optical fiber has a second measured attenuation, the second measured attenuation being less than the first measured attenuation;
setting the draw tension to the second draw tension; and
drawing a second optical fiber preform at the second draw tension to produce a third alkali doped optical fiber,
wherein the third alkali-doped optical fiber has an attenuation at 850 nm of about 1.50 dB/km or less and an attenuation at 1550 nm of about 0.155 dB/km or less.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first optical fiber preform and the second optical fiber preform are made by the same process.

### Claim 3 (depends on 1)

The method of claim 1, further comprising exposing silica soot of the second optical fiber preform to the halide dopant and to the reducing agent

### Claim 4 (depends on 1)

The method of claim 1, wherein the first glass rod is doped with an alkali comprising at least one of sodium, potassium, and rubidium.

### Claim 5 (depends on 1)

The method of claim 1, wherein the reducing agent is carbon monoxide (CO), silicon tetrachloride (SiCl4), chloromethane (CH3Cl), dichloromethane (CH2Cl2), chloroform (CHCl3), or mixtures thereof.

### Claim 6 (depends on 1)

The method of claim 1, further comprising drawing the second optical fiber preform at a draw tension of about 60 grams to about 90 grams.

### Claim 7 (depends on 1)

The method of claim 1, wherein the attenuation at 850 nm is about 1.45 dB/km or less.

### Claim 8 (depends on 7)

The method of claim 7, wherein the attenuation at 850 nm is about 1.40 dB/km or less.

### Claim 9 (depends on 1)

The method of claim 1, wherein the attenuation at 1550 nm is about 0.150 dB/km or less.

### Claim 10 (depends on 9)

The method of claim 9, wherein the attenuation at 1550 nm is about 0.145 dB/km or less.

### Claim 11

A method of manufacturing an optical fiber, the method comprising:
forming an alkali-doped silica-containing glass tube;
collapsing the glass tube to form a glass rod;
depositing silica soot on the glass rod to form a glass body;
depositing additional silica soot on the glass body;
exposing the silica soot on the glass body to a halide dopant;
exposing the silica soot on the glass body to a reducing agent;
consolidating the silica soot on the glass body to form a preform precursor;
forming an optical fiber preform from the preform precursor;
drawing the optical fiber preform into an alkali-doped optical fiber at a draw tension of about 60 grams to about 90 grams; and
exposing the alkali-doped optical fiber to a cooling apparatus for a duration of about 0.05 seconds or greater, the cooling apparatus being downstream of a draw furnace and operating within a range between about 900° C. and about 1300° C.,
wherein the alkali-doped optical fiber has an attenuation at 850 nm of about 1.50 dB/km or less and an attenuation at 1550 nm of about 0.155 dB/km or less.

### Claim 12 (depends on 11)

The method of claim 11, wherein the glass rod is doped with an alkali comprising at least one of sodium, potassium, and rubidium.

### Claim 13 (depends on 11)

The method of claim 11, wherein the reducing agent is carbon monoxide (CO), silicon tetrachloride (SiCl4), chloromethane (CH3Cl), dichloromethane (CH2Cl2), chloroform (CHCl3), or mixtures thereof.

### Claim 14 (depends on 13)

The method of claim 13, wherein the reducing agent is carbon monoxide (CO) or silicon tetrachloride (SiCl4).

### Claim 15 (depends on 11)

The method of claim 11, wherein the alkali-doped optical fiber is exposed to the cooling apparatus for a duration from about 0.05 seconds to about 2 seconds.

### Claim 16 (depends on 11)

The method of claim 11, wherein the silica soot on the glass body is exposed to the halide dopant and the reducing agent simultaneously.

### Claim 17 (depends on 16)

The method of claim 16, wherein the reducing agent is incorporated with a carrier gas to form a mixed gas, the mixed gas comprising between about 500 ppm and about 20,000 ppm of the reducing agent.

### Claim 18 (depends on 17)

The method of claim 17, wherein the mixed gas comprises between about 2000 ppm and about 5500 ppm of the reducing agent.

### Claim 19 (depends on 16)

The method of claim 16, wherein the halide is fluorine.

### Claim 20

A method of manufacturing an optical fiber, the method comprising:
forming an alkali-doped silica-containing glass tube;
collapsing the glass tube to form a glass rod;
depositing silica soot on the glass rod to form a glass body;
depositing additional silica soot on the glass body;
exposing the silica soot on the glass body to a halide dopant;
exposing the silica soot on the glass body to a reducing agent;
consolidating the silica soot on the glass body to form a preform precursor;
forming an optical fiber preform from the preform precursor;
drawing a first portion of the optical fiber preform into a first alkali-doped optical fiber at a first draw tension; and
drawing a second portion of the optical fiber preform into a second alkali-doped optical fiber at a second draw tension,
wherein the first draw tension is higher than the second draw tension, and
wherein the second alkali-doped optical fiber has an attenuation at 850 nm of about 1.50 dB/km or less and an attenuation at 1550 nm of about 0.155 dB/km or less.