# US 2024/0030583 A1 · Electrochemical method for fabrication of high-purity, high-conductivity corrugated waveguides

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0030583 A1
- Document ID: US20240030583A1
- Status: Published application
- Kind: A1
- Application number: 18/353,265
- Filed: 2023-07-17
- Published: 2024-01-25
- Earliest claimed: 2022-07-22
- Assignees: Faraday Technology Corp.
- Applicants: Faraday Technology, Inc.
- Inventors: Danny Xin Liu; Holly Garich; Timothy D. Hall; Earl Jennings Taylor
- Web page: https://patentgrep.com/patent/US20240030583A1

## CPC

- H01P 11/002: {Manufacturing hollow waveguides}
- C25D 1/00: Electroforming
- C25D 1/02: Tubes; Rings; Hollow bodies
- C25D 3/38: of copper
- C25D 21/12: Process control or regulation (controlling or regulating in general G05)
- H01P 3/123: with a complex or stepped cross-section, e.g. ridged or grooved waveguides (H01P3/14 takes precedence)
- H01P: WAVEGUIDES; RESONATORS, LINES, OR OTHER DEVICES OF THE WAVEGUIDE TYPE (operating at optical frequencies G02B)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

A method of manufacturing a corrugated copper microwave waveguide comprising placing a mandrel with external corrugations in an electrolyte bath substantially devoid of brighteners, accelerators, or levelers and including copper ions, sulfuric acid, chloride, and polyethylene glycol. The mandrel is placed proximate a copper anode in the bath. One or more waveforms are applied to the mandrel and anode to control electrodeposition distribution of copper to the mandrel rather than controlling the electrolyte bath chemistry. The mandrel and the resulting electroformed waveguide are removed from the electrolyte bath and the mandrel is excised (e.g., dissolved) resulting in a microwave waveguide with internal corrugations. Substantially devoid of additives (brighteners, accelerators, and/or levelers) generally means not having to repeatedly meter in additives during the electroforming process.

## Claims

### Claim 1

A method of manufacturing a corrugated copper microwave waveguide, the method comprising:
placing a mandrel with external corrugations in an electrolyte bath substantially devoid of brighteners, accelerators or levelers and including copper ions, sulfuric acid, chloride, and polyethylene glycol;
locating a copper anode in the bath proximate the mandrel;
applying one or more waveforms to the mandrel and anode to control electrodeposition distribution of copper to the mandrel rather than controlling the electrolyte bath chemistry;
removing the mandrel and the resulting electroformed copper waveguide from the electrolyte bath; and
excising the mandrel resulting in a microwave waveguide with internal corrugations.

### Claim 2 (depends on 1)

The method of claim 1 in which the waveguide internal corrugations have a sub-millimeter width.

### Claim 3 (depends on 1)

The method of claim 1 in which the waveguide internal corrugations have a sub-millimeter distance between adjacent corrugations.

### Claim 4 (depends on 1)

The method of claim 1 in which the copper anode is substantially oxygen free.

### Claim 5 (depends on 1)

The method of claim 1 in which the mandrel is made of aluminum or an aluminum alloy.

### Claim 6 (depends on 1)

The method of claim 1 in which the waveforms include a cathodic current followed by an anodic current repeated for a predetermined time.

### Claim 7 (depends on 6)

The method of claim 6 in which the cathodic current ranges from 10 to 50 mA/cm2 with cathodic current on-times that range from 0.1 to 100 ms and the anodic current ranges from 5 to 200 mA/cm2 and the anodic current on-times range from 0.1 to 10 ms.

### Claim 8 (depends on 6)

The method of claim 6 in which the predetermined time is between 24 and 48 hours.

### Claim 9 (depends on 1)

The method of claim 1 further including a waveguide thickening method.

### Claim 10 (depends on 9)

The method of claim 9 in which the thickening method includes applying a cathodic current waveform followed by an anodic current waveform for a predetermined time.

### Claim 11 (depends on 10)

The method of claim 10 in which the predetermined time is between 24-48 hours.

### Claim 12 (depends on 1)

The method of claim 1 in which the waveguide has an inner diameter of approximately 7 mm and a corrugation period of 1.38 mm.

### Claim 13 (depends on 1)

The method of claim 1 in which the corrugations are rectangular in cross section.

### Claim 14 (depends on 1)

The method of claim 1 in which applying the one or more waveforms to the mandrel and anode to control electrodeposition of copper to the mandrel conformally deposits the copper to the mandrel without dog bone features.

### Claim 15 (depends on 1)

The method of claim 1 in which applying the one or more waveforms to the mandrel and anode to control electrodeposition of the copper to the mandrel results in keyholes through the waveguide internal corrugations.

### Claim 16 (depends on 1)

The method of claim 1 in which excising the mandrel includes dissolving the mandrel using a hot concentrated caustic solution.

### Claim 17 (depends on 1)

The method of claim 1 in which the copper anode has an RRR value of approximately 100 and the copper waveguide has an RRR value of between 490 and 860.

### Claim 18

A method of manufacturing a corrugated copper microwave waveguide, the method comprising:
placing a mandrel with external corrugations in an electrolyte bath substantially devoid of chemical agents which decrease copper electrode deposit purity and/or resistivity and/or which result in outgassing;
locating a copper anode in the bath proximate the mandrel;
applying repeated cathodic current and anodic current waveforms to the mandrel and anode to electrodeposit a conformal copper electroform to the mandrel;
removing the mandrel and the resulting conformal electroform from the electrolyte bath; and
dissolving the mandrel resulting in a microwave waveguide with internal corrugations.

### Claim 19 (depends on 18)

The method of claim 18 in which the waveguide internal corrugations have a sub-millimeter width.

### Claim 20 (depends on 18)

The method of claim 18 in which the waveguide internal corrugations have a sub-millimeter distance between adjacent corrugations.

### Claim 21 (depends on 18)

The method of claim 18 in which the copper anode is substantially oxygen free.

### Claim 22 (depends on 18)

The method of claim 18 in which the mandrel is made of aluminum or an aluminum alloy.

### Claim 23 (depends on 18)

The method of claim 18 in which the waveforms include a cathodic current followed by an anodic current repeated for a predetermined time.

### Claim 24 (depends on 23)

The method of claim 23 in which the cathodic current ranges from 10 to 50 mA/cm2 with cathodic current on-times that range from 0.1 to 100 ms and the anodic current ranges from 5 to 200 mA/cm2 and the anodic current on-times range from 0.1 to 10 ms.

### Claim 25 (depends on 23)

The method of claim 23 in which the predetermined time is between 24 and 48 hours.

### Claim 26 (depends on 18)

The method of claim 18 further including the waveguide thickening method.

### Claim 27 (depends on 26)

The method of claim 26 in which the thickening method includes applying a cathodic current waveform followed by an anodic current waveform for a predetermined time resulting in a smooth surface.

### Claim 28 (depends on 27)

The method of claim 27 in which the thickening method includes a cathodic current range of 30 to 100 mA/cm2 and cathodic on-time of 10 to 50 ms and an anodic current range of 50 to 100 mA/cm2 and anodic on-time of 1 to 5 ms.

### Claim 29 (depends on 27)

The method of claim 27 in which the predetermined time is between 24-48 hours.

### Claim 30 (depends on 18)

The method of claim 18 in which the waveguide has an inner diameter of approximately 7 mm, and a corrugation period of 1.38 mm.

### Claim 31 (depends on 18)

The method of claim 18 in which the corrugations are rectangular in cross section.

### Claim 32 (depends on 18)

The method of claim 18 in which applying the one or more waveforms to the mandrel and anode to control electrodeposition of copper to the mandrel conformally deposits the copper to the mandrel without dog bone features.

### Claim 33 (depends on 18)

The method of claim 18 in which applying the one or more waveforms to the mandrel and anode to control electrodeposition of the copper to the mandrel results in keyholes through the waveguide internal corrugations.

### Claim 34 (depends on 18)

The method of claim 18 in which excising the mandrel includes dissolving the mandrel using a hot concentrated caustic solution.

### Claim 35 (depends on 18)

The method of claim 18 in which the copper anode has an RRR value of approximately 100 and the copper waveguide has an RRR value of between 490 and 860.

### Claim 36 (depends on 18)

The method of claim 18 in which the bath is devoid of brighteners, accelerators, and levelers.

### Claim 37 (depends on 36)

The method of claim 36 in which the bath includes copper ions.

### Claim 38 (depends on 37)

The method of claim 37 in which the bath includes an ionic conductivity medium and one or more recrystallization mediums.

### Claim 39 (depends on 38)