# US 2024/0018013 A1 · Method for preparing nickel sulfate from ferronickel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0018013 A1
- Document ID: US20240018013A1
- Status: Published application
- Kind: A1
- Application number: 18/374,630
- Filed: 2023-09-28
- Published: 2024-01-18
- Earliest claimed: 2021-08-25
- Assignees: Guangdong Brunp Recycling Technology Co., Ltd.; Hunan Brunp Recycling Technology Co., Ltd.; Hunan Brunp Ev Recycling Co., Ltd.
- Applicants: Guangdong Brunp Recycling Technology Co., Ltd.; Hunan Brunp Recycling Technology Co., Ltd.; Hunan Brunp Ev Recycling Co., Ltd.
- Inventors: Haijun Yu; Yinghao Xie; Aixia Li; Xuemei Zhang; Changdong Li
- Web page: https://patentgrep.com/patent/US20240018013A1

## CPC

- C01G 53/10: Sulfates
- C01G 49/02: Oxides; Hydroxides {(C01G49/0018 takes precedence)}
- C01G 49/06: Ferric oxide [Fe2O3]
- C01G 53/01: Preparation or separation involving a liquid-liquid extraction, an adsorption or an ion-exchange
- C01G 99/003: {Preparation involving a liquid-liquid extraction, an adsorption or an ion-exchange}
- Y02P 10/20: Recycling
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present disclosure discloses a method for preparing nickel sulfate from ferronickel, including: S1: in a high-pressure oxygen environment, mixing crushed ferronickel with sulfuric acid, introducing a carbon monoxide gas to allow a reaction, and conducting solid-liquid separation (SLS) to obtain a filtrate and a filter residue; S2: adding an oxidizing agent and a precipitating agent successively to the filtrate, controlling a pH of the filtrate, and conducting SLS to obtain a nickel-containing filtrate and an iron hydroxide precipitate; and S3: subjecting the nickel-containing filtrate to extraction and back-extraction to obtain a nickel sulfate solution. In the present disclosure, the carbon monoxide gas is introduced under high-pressure acidic conditions to first react with nickel and iron to form nickel tetracarbonyl and iron pentacarbonyl, and the nickel tetracarbonyl and iron pentacarbonyl are oxidized by oxygen and then smoothly react with sulfuric acid to form nickel sulfate and iron sulfate.

## Claims

### Claim 1

A method for preparing nickel sulfate from ferronickel, comprising the following steps:
S1: in a high-pressure oxygen environment, mixing crushed ferronickel with sulfuric acid, introducing a carbon monoxide gas to allow a reaction, and conducting solid-liquid separation to obtain a filtrate and a filter residue, the reaction is conducted in a closed space, the carbon monoxide gas is introduced through a bottom of the crushed ferronickel, and a volume concentration of the carbon monoxide gas in the closed space is controlled at ≤2.5%; the reaction is conducted at 40° C. to 200° C.; the sulfuric acid has a concentration of 3 mol/L to 8 mol/L;
S2:adding an oxidizing agent to the filtrate, and then adding a precipitating agent, controlling a pH of the filtrate, and conducting solid-liquid separation to obtain a nickel-containing filtrate and an iron hydroxide precipitate; and
S3: subjecting the nickel-containing filtrate to extraction and back-extraction to obtain a nickel sulfate solution; a process of the extraction and back-extraction comprises: adding an extracting agent to the nickel-containing filtrate for nickel extraction to obtain a nickel-containing organic phase, and adding a sulfuric acid solution to the nickel-containing organic phase for nickel back-extraction to obtain the nickel sulfate solution; the extracting agent is one or more selected from the group consisting of P204, P507, DEHPA, and Cyanex272.

### Claim 2 (depends on 1)

The method according to claim 1, wherein in S1, the reaction is conducted at a pressure of 3.0 MPa to 6.5 MPa.

### Claim 3 (depends on 1)

The method according to claim 1, wherein in S2, the oxidizing agent is one or more selected from the group consisting of hydrogen peroxide, compressed air, chlorine, and sodium chlorate.

### Claim 4 (depends on 1)

The method according to claim 1, wherein in S2, the precipitating agent is one or more selected from the group consisting of ammonia water, sodium hydroxide, sodium carbonate, and sodium bicarbonate.

### Claim 5 (depends on 1)

The method according to claim 1, wherein in S2, the pH is 3 to 3.5.