# US 2024/0010539 A1 · Method of making high quality glass products from high viscosity melts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0010539 A1
- Document ID: US20240010539A1
- Status: Published application
- Kind: A1
- Application number: 18/470,909
- Filed: 2023-09-20
- Published: 2024-01-11
- Earliest claimed: 2021-03-22
- Assignees: Schott AG
- Applicants: Schott AG
- Inventors: Hildegard Römer; Michael Hahn; Stefan Rosner; Volker Trinks; Rainer Eichholz; Christoph Bergmann; Armin Vogl; Jörg Hessenkemper; Horst Blei; Klaus Schönberger; Sybille Haas; Guido Räke; Stefan Schmitt; Christoph Berndhäuser; Olaf Claussen; Christopher Klein; Wolfgang Schmidbauer
- Web page: https://patentgrep.com/patent/US20240010539A1

## CPC

- C03B 5/03: Tank furnaces
- C03B 5/023: {by microwave heating}
- C03B 5/027: by passing an electric current between electrodes immersed in the glass bath, i.e. by direct resistance heating
- C03B 5/225: Refining (C03B5/18 takes precedence {; Refining agents C03C1/004})
- C03B 5/235: Heating the glass (C03B5/02, C03B5/18, C03B5/225 take precedence)
- C03B 5/24: Automatically regulating the melting process
- C03B 5/43: Use of materials for furnace walls, e.g. fire-bricks
- C03C 3/091: containing aluminium
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A method of making glass products includes: heating material to obtain a glass melt; heating the glass melt in a melting tank having a melting tank bottom, the glass melt having a melt volume, a melt surface, and a viscosity of 102 dPas at a temperature above 1580° C. The glass melt is heated such that at least some of the glass melt has a viscosity of 102.5 dPas or less. An amount of thermal energy introduced directly into the melt volume is more than 60% of a total amount of thermal energy introduced into the glass melt. A maximum difference between a temperature at a location on the melt surface and a temperature at a location at the melting tank bottom vertically underneath the location on the melt surface is such that a difference in glass melt densities is less than 0.05 g/cm3 per meter distance between the locations.

## Claims

### Claim 1

A method of making high quality glass products from high viscosity melts, the method comprising:
heating glass raw material to obtain a glass melt;
heating the glass melt in a melting tank, the melting tank having a melting tank bottom, and the glass melt having a glass melt volume and a melt surface, wherein the glass melt is heated using one or more heat sources such that at least a part of the glass melt has a viscosity of 102.5 dPas or less, wherein heating the glass melt includes heating the melt surface and/or directly heating the glass melt volume, wherein an amount of thermal energy introduced directly into the glass melt volume is more than 60% of a total amount of thermal energy introduced into the glass melt in the melting tank, wherein a maximum difference between a temperature at a location on the melt surface and a temperature at a location at the melting tank bottom vertically underneath the location on the melt surface is such that a difference in glass melt densities corresponding to the temperatures is less than 0.05 g/cm3 per meter distance between the location on the melt surface and the location at the melting tank bottom, wherein the glass melt has a viscosity of 102 dPas at a temperature above 1580° C.;
removing bubbles from the glass melt;
withdrawing the glass melt from the melting tank at a rate of 2.0 t per m3 melt volume per 24 h or less; and
obtaining a glass product having less than 20 bubbles per kg of glass.

### Claim 2 (depends on 1)

The method of claim 1, wherein a glass melt density at a hottest location on the glass melt surface is smaller or larger than at the location at the melting tank bottom.

### Claim 3 (depends on 1)

The method of claim 1, wherein a minimum viscosity within the glass melt volume is not less than 10 dPas.

### Claim 4 (depends on 1)

The method of claim 1, wherein a temperature dependence of a glass melt density in a temperature range of from T4 to T2 is at least 9.0 mg/cm3 per 100° C., wherein T4 is a temperature where the glass has a viscosity of 104 dPas and T2 is a temperature where the glass has a viscosity of 102 dPas.

### Claim 5 (depends on 4)

The method of claim 4, wherein the temperature dependence of the glass melt density in the temperature range of from T4 to T2 is up to 19 mg/cm3 per 100° C.

### Claim 6 (depends on 1)

The method of claim 1, wherein a distance between a hottest location on the melt surface and a location at the melting tank bottom vertically underneath the hottest location is less than 1250 mm.

### Claim 7 (depends on 6)

The method of claim 6, wherein the distance between the hottest location on the melt surface and the location at the melting tank bottom vertically underneath the hottest location is at least 750 mm.

### Claim 8 (depends on 1)

The method of claim 1, wherein an amount of heating energy obtained from burning fossil fuels is less than 1.0% relative to a total amount of heat introduced into the glass melt.

### Claim 9 (depends on 1)

The method of claim 1, wherein an amount of heating energy introduced into the glass melt by heating the melt surface is less than 40.0% relative to a total amount of heat introduced into the glass melt.

### Claim 10 (depends on 1)

The method of claim 1, wherein heating the melt surface includes heating the melt surface using one or more microwave heaters, and/or burning bio-fuel and/or hydrogen.

### Claim 11 (depends on 1)

The method of claim 1, wherein directly heating the glass melt volume includes electrode heating.

### Claim 12 (depends on 1)

The method of claim 1, wherein the glass melt has a Vogel-Fulcher-Tammann (VFT) constant B in a range of from 5,000 to 9,000 K and to in a range of from 75° C. to 240° C.

### Claim 13

A glass product having less than 20 bubbles per kg of glass, wherein the glass has a viscosity of 102 dPas at a temperature above 1580° C., the glass having a temperature dependence of glass melt density in a temperature range of from T4 to T2 of at least 9.0 mg/cm3 per 100° C., wherein T4 is a temperature where the glass has a viscosity of 104 dPas and T2 is a temperature where the glass has a viscosity of 102 dPas.

### Claim 14 (depends on 13)

The glass product of claim 13, wherein the glass melt has a Vogel-Fulcher-Tammann (VFT) constant B in a range of from 5,000 to 9,000 K and T0 in a range of from 75° C. to 240° C.

### Claim 15 (depends on 13)

The glass product of claim 13, wherein the temperature dependence of the glass melt density in the temperature range of from T4 to T2 is up to 19.0 mg/cm3 per 100° C.

### Claim 16 (depends on 13)

The glass product of claim 13, wherein the glass has a coefficient of thermal expansion in a temperature range of from 20° C. to 300° C. of from 3.0 ppm/K to 8.5 ppm/K.

### Claim 17 (depends on 13)

The glass product of claim 13, wherein the glass product is produced by a method comprising:
heating glass raw material to obtain a glass melt;
heating the glass melt in a melting tank, the melting tank having a melting tank bottom, and the glass melt having a glass melt volume and a melt surface, wherein the glass melt is heated using one or more heat sources such that at least a part of the glass melt has a viscosity of 102.5 dPas or less, wherein heating the glass melt includes heating the melt surface and/or directly heating the glass melt volume, wherein an amount of thermal energy introduced directly into the glass melt volume is more than 60% of a total amount of thermal energy introduced into the glass melt in the melting tank, wherein a maximum difference between a temperature at a location on the melt surface and a temperature at a location at the melting tank bottom vertically underneath the location on the melt surface is such that a difference in glass melt densities corresponding to the temperatures is less than 0.05 g/cm3 per meter distance between the location on the melt surface and the location at the melting tank bottom;
removing bubbles from the glass melt;
withdrawing the glass melt from the melting tank at a rate of 2.0 t per m3 melt volume per 24 h or less; and
obtaining the glass product.