# US 2024/0006601 A1 · Cathode active material, method for its manufacture, and use

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0006601 A1
- Document ID: US20240006601A1
- Status: Published application
- Kind: A1
- Application number: 18/036,828
- Filed: 2021-11-05
- Published: 2024-01-04
- Earliest claimed: 2020-11-13
- Assignees: BASF SE; The Board of Trustees of the Leland Stanford Junior University
- Applicants: BASF SE; The Board of Trustees of the Leland Stanford Junior University
- Inventors: Tobias Maximilian Teufl; Jordan K Lampert; Heino Sommer; William C. Chueh; William E. Gent
- Web page: https://patentgrep.com/patent/US20240006601A1

## CPC

- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- C01G 53/50: of the type (MnO2)n-, e.g. Li(NixMn1-x)O2 or Li(MyNixMn1-x-y)O2
- C01G 53/56: of the type (MnO3)2-, e.g. Li2(NixMn1-x)O3 or Li2(MyNixMn1-x-y)O3
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2004/82: two phases having the same anion, e.g. both oxidic phases
- C01P 2004/84: one phase coated with the other
- C01P 2006/40: Electric properties
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Process for making a composite oxide according to the formula x·Li2Ni1-y1-y2Mny1M1y2O3·(1−x)·LiNi1-zM2zO2 wherein x is in the range of from 0.01 to 0.5, z is in the range of from zero to 0.5, M1 is selected from Ti, Zr, Sn, Ge, Ta, Nb, Sb, W, and Mo, and combinations of at least two of the foregoing, M2 is at least one of Co, Al, Mg, Fe, or Mn, or a combination of at least two of the foregoing, 0.1≤y1≤0.75, zero≤y2≤0.05, said process comprising the following steps: (a) providing a particulate hydroxide, oxide or oxyhydroxide of TM where TM has the general formula x·Ni1-y1-y2Mny1M1y·(1−x)Ni1-zM2z, or the respective species without M1 and/or M2, (b) adding a source of lithium, (c) treating the mixture obtained from step (b) thermally under an atmosphere comprising oxygen in two steps: (c) heating the mixture obtained from step (b) to 680 to 800° C. in an atmosphere containing in the range of from 10 to 100 vol-% oxygen, and, (e) heating the intermediate from step (c) to 450 to 580° C. in an atmosphere containing at least 90 vol-% oxygen.

## Claims

### Claim at position 1

-14. (canceled)

### Claim 15

Process for making a cobalt-free composite oxide according to the formula x·Li2Ni1-yMnyO3·(1−x)·LiNiO2 wherein x is in the range of from 0.1 to 0.5, 0.1≤y≤0.75, said process comprising the following steps:
(a) providing a particulate hydroxide, oxide or oxyhydroxide of TM where TM has the general formula x·Ni1-yMny·(1−x)Ni,
(b) adding a source of lithium and, optionally, at least one oxide, hydroxide, or oxyhydroxide of Mn, in a molar ratio of Li:(Ni+Mn) of from 0.9:1 to 1.1:1,
(c) heating the mixture obtained from step (b) to 680 to 800° C. in an atmosphere containing oxygen,
(d) adding source of lithium, and
(e) heating the mixture obtained from step (d) to 450 to 580° C. in an atmosphere containing at least 90 vol % oxygen.

### Claim 16 (depends on 15)

Process according to claim 15 wherein 0.15≤y≤0.6.

### Claim 17 (depends on 15)

Process according to claim 15 wherein steps (c) (and (e) are performed under a forced flow of gas.

### Claim 18 (depends on 15)

Process according to claim 15 wherein the source of lithium is selected from lithium hydroxide, lithium carbonate, lithium nitrate, and lithium oxide.

### Claim 19 (depends on 15)

Process according to claim 15 wherein x is in the range of from 0.1 to 0.3.

### Claim 20 (depends on 15)

Process according to claim 15 wherein said process comprises an additional step (f) subsequent to step (e), and wherein said step (f) is selected from coating steps and wet treatment steps.

### Claim 21

Particulate cobalt-free composite oxide of the composition x·Li2Ni1-yMnyO3·(1−x)·LiNiO2 wherein x is in the range of from 0.01 to 0.5, 0.1≤y≤0.75.

### Claim 22 (depends on 21)

Particulate composite oxide according to claim 21 wherein 0.15≤y≤0.6.

### Claim 23 (depends on 21)

Particulate composite oxide according to claim 21 wherein x is in the range of from 0.1 to 0.3.

### Claim 24 (depends on 21)

Particulate composite oxide according to claim 21 wherein cations in both the Li2Ni1-yMnyO3 and the LiNiO2 domains exhibit a substantially layered ordering, where the Li2Ni1-yMnyO3 domains display alternating Li and Li1/3[Ni1-yMny]⅔ cation layers, and the LiNiO2 domains display alternating Ni and Li cation layers, and wherein Li1/3[Ni1-yMny]⅔ cation layers in the Li2Ni1-yMnyO3 domains exhibit substantially a honeycomb-type cation ordering wherein the Li cations have no other Li cations as their nearest cation neighbors within the same cation layer.

### Claim 25 (depends on 21)

Cathode comprising
(A) at least one particulate composite oxide according to claim 21,
(B) carbon in electrically conductive form,
(C) at least one binder.

### Claim 26 (depends on 25)

Electrochemical cell comprising a cathode according to claim 25.