- Number: US 2024/0006589 A1
- Document ID: US20240006589A1
- Status: Published application
- Kind: A1
- Application number: 18/468,737
- Filed: 2023-09-18
- Published: 2024-01-04
- Earliest claimed: 2019-06-12
- Assignees: SK On Co., Ltd.
- Applicants: SK On Co., Ltd.
- Inventors: Jae Yun MIN; Jeong A. KIM; Sung Jun PARK; Da Bin CHUNG; Jae Kyu JIN; Ji Hwan CHOI
- Web page: https://patentgrep.com/patent/US20240006589A1

## CPC

- H01M 4/366: {as layered products}
- H01M 4/364: {as mixtures}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/622: {being polymers}
- H01M 4/625: {Carbon or graphite}
- H01M 4/626: {Metals}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A secondary battery comprising a positive electrode current collector, a first positive electrode mixture layer disposed on the positive electrode current collector and including a first positive electrode active material and a binder, and a second positive electrode mixture layer disposed on the first positive electrode mixture layer and including a second positive electrode active material and a binder. A nickel content of the second positive electrode active material is 80% by weight or less of a nickel content of the first positive electrode active material. By providing a secondary battery including a positive electrode of a multi-layer structure that includes positive electrode active materials having different contents of nickel, a secondary battery capable of improving high-temperature characteristics while maintaining energy density may be provided.

## Claims

### Claim 1

A secondary battery comprising:
a positive electrode comprising:
a positive electrode current collector;
a first positive electrode mixture layer disposed on the positive electrode current collector and including a first positive electrode active material and a binder; and
a second positive electrode mixture layer disposed on the first positive electrode mixture layer and including a second positive electrode active material and a binder,
wherein a nickel content of the second positive electrode active material is 80% by weight or less of a nickel content of the first positive electrode active material.

### Claim 2 (depends on 1)

The secondary battery of claim 1, wherein the first positive electrode active material contains 42% by weight or more of nickel.

### Claim 3 (depends on 1)

The secondary battery of claim 1, wherein the second positive electrode active material contains 37% by weight or less of nickel.

### Claim 4 (depends on 1)

The secondary battery of claim 1, wherein the second positive electrode active material is contained in an amount of 50% by weight or less of the first positive electrode active material and the second positive electrode active material.

### Claim 5 (depends on 1)

The secondary battery of claim 1, wherein a thickness of the first positive electrode mixture layer is 30 μm to 100 μm.

### Claim 6 (depends on 1)

The secondary battery of claim 1, wherein a thickness of the second positive electrode mixture layer is 1 μm to 50 μm.

### Claim 7 (depends on 1)

The secondary battery of claim 1, wherein the first positive electrode active material is at least one selected from LiNi0.7Co0.15Mn0.15O2, LiNi0.8Co0.1Mn0.1O2, LiNi0.9Co0.05Mn0.05O2, and LiNi0.8Co0.15Al0.05O2.

### Claim 8 (depends on 1)

The secondary battery of claim 1, wherein the second positive electrode active material is at least one selected from LiNi(⅓)Co(⅓)Mn(⅓)O2, LiNi0.4Co0.3Mn0.3O2, LiNi0.5Co0.2Mn0.3O2, LiNi0.6Co0.2Mn0.2O2, and LiNi0.7Co0.15Mn0.15O2.

### Claim 9 (depends on 1)

The secondary battery of claim 1, wherein the binder is at least one selected from polyvinylidene fluoride (PVDF), polyvinyl alcohol, carboxymethylcellulose (CMC), starch, hydroxypropyl cellulose, regenerated cellulose, polyvinylpyrrolidone, tetrafluoroethylene, polyethylene, polypropylene, ethylene-propylene-diene terpolymer (EPDM), sulfonated EPDM, styrene butylene rubber (SBR), hydrogenated nitrile butadiene rubber (H-NBR), fluorine rubber, styrene monomer (SM), Butadiene (BD), butyl acrylate (BA), mussel protein, a polyolefin-based binder, and a silane-based binder.

### Claim 10 (depends on 1)

The secondary battery of claim 1, wherein the first positive electrode mixture layer and the second positive electrode mixture layer further comprise a conductive material.

### Claim 11 (depends on 10)

The secondary battery of claim 10, wherein the conductive material is at least one selected from multi-wall CNT, single-wall CNT or the like; natural graphite, artificial graphite or the like; carbon black, acetylene black, ketjen black, channel black, furnace black, lamp black, or carbon black of summer black; a carbon fiber, a metal fiber, or the like; a metal powder of carbon fluoride, aluminum and nickel powder, a conductive whisker of zinc oxide and potassium titanate, a conductive metal oxide of titanium oxide, and a polyphenylene derivative.