# US 2024/0004284 A1 · Pellicle membrane with improved properties

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0004284 A1
- Document ID: US20240004284A1
- Status: Published application
- Kind: A1
- Application number: 17/854,133
- Filed: 2022-06-30
- Published: 2024-01-04
- Earliest claimed: 2022-06-30
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company
- Inventors: Pei-Cheng Hsu; Wei-Hao Lee; Ting-Pi Sun; Chia-Tung Kuo; Huan-Ling Lee; Hsin-Chang Lee; Chin-Hsiang Lin
- Web page: https://patentgrep.com/patent/US20240004284A1

## CPC

- G03F 1/64: characterised by the frames, e.g. structure or material, including bonding means therefor
- B82Y 40/00: Manufacture or treatment of nanostructures
- G03F 1/48: Protective coatings
- G03F 1/62: Pellicles, e.g. pellicle assemblies, e.g. having membrane on support frame; Preparation thereof
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

A pellicle assembly includes a pellicle membrane with a nanotube layer formed from thick nanotube bundles. The pellicle membrane can be formed with multiple layers and has a combination of long lifetime, high transmittance, low deflection, and small pore size. A conformal coating may applied to an outer surface of the pellicle membrane. The conformal coating protects the pellicle membrane from damage that can occur due to heat and hydrogen plasma created during EUV exposure.

## Claims

### Claim 1

A method of forming a pellicle assembly, comprising:
reducing a thickness of an initial membrane to obtain a first nanotube layer for a pellicle membrane, wherein the initial membrane is formed from thick nanotube bundles which are formed from 25 or more nanotubes; and
affixing the pellicle membrane to a mounting frame to obtain the pellicle assembly.

### Claim 2 (depends on 1)

The method of claim 1, wherein each thick nanotube bundle has an average diameter of 25 nanometers or greater.

### Claim 3 (depends on 1)

The method of claim 1, wherein each thick nanotube bundle is formed from multi-wall nanotubes.

### Claim 4 (depends on 1)

The method of claim 1, wherein the pellicle membrane further comprises a second nanotube layer, wherein the second nanotube layer is formed from thin nanotube bundles.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first nanotube layer is placed between two nanotube layers that are formed from thin nanotube bundles.

### Claim 6 (depends on 1)

The method of claim 1, wherein the thick nanotube bundles comprise carbon nanotubes, boron nitride nanotubes, silicon carbide nanotubes, molybdenum disulfide nanotubes, molybdenum diselenide nanotubes, tungsten disulfide nanotubes, or tungsten diselenide nanotubes.

### Claim 7 (depends on 1)

The method of claim 1, wherein a conformal coating is applied to at least an outer surface of the pellicle membrane.

### Claim 8 (depends on 7)

The method of claim 7, wherein the conformal coating comprises B, BN, B4C, B2O3, B6Si, SiN, Si3N4, SiN2, SiC, SiZr, SiCxNy, Nb, NbN, NbSi, NbSiN, Nb2O5, NbTixNy, NbC, Nb5Si3, ZrNx, ZrYxOy, ZrF, ZrF4, ZrSi2, YN, Y2O3, YF, Mo, MO2N, MoSi, MoSi2, MoSiN, MoC2, MoC, MoS2, MoN, Ru, RuNb, RuSiN, RuO2, TiN, TiCxNy, HfO2, HfNx, HfF4, VN, Rh, Pt, Pd, W, Cr, Ni, Fe, Co, Ag, Au, Zr, Y, or a composite thereof.

### Claim 9 (depends on 7)

The method of claim 7, wherein the coating is in the form of a continuous film, nano-grains, nano-particles, or nano-sheets.

### Claim 10 (depends on 1)

The method of claim 1, wherein the thickness of the initial membrane is reduced by applying pressure.

### Claim 11 (depends on 1)

The method of claim 1, wherein the thickness of the initial membrane is reduced by:
stretching the initial membrane using a stretching frame to obtain an extended membrane;
affixing a mounting frame to a portion of the extended membrane; and
separating the mounting frame and the portion of the extended membrane from the remainder of the extended membrane, to obtain the pellicle assembly.

### Claim 12 (depends on 11)

The method of claim 11, wherein the initial membrane is stretched biaxially.

### Claim 13 (depends on 1)

The method of claim 1, further comprising annealing the initial membrane while stretching the initial membrane.

### Claim 14 (depends on 13)

The method of claim 13, wherein the initial membrane is annealed at a temperature of about 200° C. to about 800° C.

### Claim 15 (depends on 13)

The method of claim 13, further comprising flowing an inert gas past the initial membrane during the stretching.

### Claim 16

A method of forming a pellicle assembly, comprising:
reducing a thickness of an initial membrane to obtain a first nanotube layer for a pellicle membrane, wherein the initial membrane is formed from nanotube bundles which are formed from multi-wall nanotubes and which have an average diameter of 25 nanometers or greater;
combining the first nanotube layer with a second nanotube layer formed from thin nanotube bundles to form the pellicle membrane; and
affixing the pellicle membrane to a mounting frame to obtain the pellicle assembly.

### Claim 17 (depends on 16)

The method of claim 16, wherein the thick nanotube bundles are formed from at least 25 nanotubes.

### Claim 18

A method for processing a semiconductor wafer substrate, comprising:
receiving a semiconductor wafer substrate;
forming a photoresist layer on the semiconductor wafer substrate;
exposing the photoresist layer to radiation from a reflective photomask in an exposure tool;
wherein the radiation passes through a pellicle membrane that comprises at least one nanotube membrane layer formed from thick nanotube bundles.

### Claim 19 (depends on 18)

The method of claim 18, wherein each thick nanotube bundle has a diameter of 25 nanometers or greater, or wherein the thick nanotube bundles are formed from at least 25 nanotubes.

### Claim 20 (depends on 18)

The method of claim 18, wherein the exposure tool is an EUV lithography system or an EUV lithography system having a numerical aperture of greater than 0.5.