# US 2024/0003367 A1 · Weld joint and production method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0003367 A1
- Document ID: US20240003367A1
- Status: Published application
- Kind: A1
- Application number: 18/253,839
- Filed: 2021-09-09
- Published: 2024-01-04
- Earliest claimed: 2020-11-26
- Assignees: Jfe Steel Corporation; Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
- Applicants: Jfe Steel Corporation; Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
- Inventors: Atsushi TAKADA; Peng HAN; Masamichi SUZUKI
- Web page: https://patentgrep.com/patent/US20240003367A1

## CPC

- B23K 9/16: making use of shielding gas
- B23K 35/0261: {Rods, electrodes or wires}
- B23K 35/30: with the principal constituent melting at less than 1550°C
- B23K 35/3073: {with Mn as next major constituent}
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/58: with more than 1.5% by weight of manganese
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

Provided is a weld joint having high strength and excellent hot crack resistance and low-temperature toughness. High Ni steel plates containing 6.5 mass % to 10.0 mass % of Ni are welded to form a weld metal to obtain a weld joint. The weld metal has a chemical composition containing Mn: 13.0% to 25.0%, Cr: 3.8% or less, Ni: 1.0% to 12.0%, Mo: 0.1% to 5.0%, N: % or less, and O: 0.100% or less, and the strength of the weld metal is adjusted so that the yield strength BYS of each steel plate and the 0.2% proof stress WPS of the weld metal satisfy [WPS]≤[BYS]−100 MPa (1) and the tensile strength BTS of the steel plate and the tensile strength WTS of the weld metal satisfy [WTS]≤[BTS]+100 MPa (2).

## Claims

### Claim 1

A weld joint comprising steel plates and a weld metal, the weld joint formed by welding the steel plates through the weld metal,
the steel plates comprising a steel plate chemical composition containing, in mass %,
C: 0.02% to 0.20%,
Si: 0.05% to 0.50%,
Mn: 0.10% to 1.80%,
P: 0.030% or less,
S: 0.030% or less,
Ni: 6.5% to 10.0%,
N: 0.010% or less, and
O: 0.010% or less,
with a balance consisting of Fe and inevitable impurities, the weld metal comprising:
a weld metal chemical composition containing, in mass %,
C: 0.10% to 0.80%,
Si: 0.10% to 1.00%,
Mn: 13.0% to 25.0%,
P: 0.030% or less,
S: 0.030% or less,
Ni: 1.0% to 12.0%,
Cr: 0.4% to 3.8%,
Mo: 0.1% to 5.0%,
N: 0.080% or less, and
O: 0.100% or less,
with a balance consisting of Fe and inevitable impurities; and
tensile properties of a 0.2% proof stress WPS of 400 MPa or more and a tensile strength WTS of 660 MPa or more,
a yield strength BYS of the steel plate and the 0.2% proof stress WPS of the weld metal satisfying the following formula (1), and
a tensile strength BTS of the steel plate and the tensile strength WTS of the weld metal satisfying the following formula (2):
[WPS]≤[BYS]−100 MPa (1)
[WTS]≤[BTS]+100 MPa (2)
where WPS is the 0.2% proof stress of the weld metal in MPa, WTS is the tensile strength of the weld metal in MPa, BYS is the yield strength of the steel plate in MPa, and BTS is the tensile strength of the steel plate in MPa.

### Claim 2 (depends on 1)

The weld joint according to claim 1, wherein the weld metal chemical composition further contains, in mass %, one or more selected from the following (i) and (ii): (i) one or more selected from the group consisting of V: 1.0% or less, Ti: 1.0% or less, Nb: 1.0% or less, and W: 1.0% or less; and (ii) one or more selected from the group consisting of Cu: 2.0% or less, Al: 1.0% or less, Ca: 0.010% or less, and REM: 0.020% or less.

### Claim 3 (depends on 1)

The weld joint according to claim 1, wherein the steel plate chemical composition further contains, in mass %, one or more selected from the following (iii) and (iv): (iii) one or more selected from the group consisting of Cu: 0.5% or less, Al: 0.1% or less, Cr: 1.0% or less, Mo: 1.0% or less, V: 0.2% or less, Nb: 0.2% or less, and Ti: 0.2% or less; and (iv) one or more selected from the group consisting of B: 0.005% or less, Ca: 0.005% or less, and REM: 0.020% or less.

### Claim 4

A production method for a weld joint excellent in low-temperature toughness, comprising:
subjecting steel plates to gas metal arc welding using a solid wire to form a weld metal to obtain the weld joint; and
adjusting welding conditions of the gas metal arc welding to obtain a welding heat input per one pass of 0.5 kJ/mm to 6.0 kJ/mm so that a 0.2% proof stress WPS of the weld metal satisfies the following formula (1) in relation to a yield strength BYS of the steel plate and a tensile strength WTS of the weld metal satisfies the following formula (2) in relation to a tensile strength BTS of the steel plate:
[WPS]≤[BYS]−100 MPa (1)
[WTS]≤[BTS]+100 MPa (2)
where WPS is the 0.2% proof stress of the weld metal in MPa, WTS is the tensile strength of the weld metal in MPa, BYS is the yield strength of the steel plate in MPa, and BTS is the tensile strength of the steel plate in MPa, mass %,
the steel plates comprising a steel plate chemical composition containing, in
C: 0.02% to 0.20%,
Si: 0.05% to 0.50%,
Mn: 0.10% to 1.80%,
P: 0.030% or less,
S: 0.030% or less,
Ni: 6.5% to 10.0%,
N: 0.010% or less, and
O: 0.010% or less,
with a balance consisting of Fe and inevitable impurities, the solid wire comprising a wire chemical composition containing, in mass %,
C: 0.15% to 1.00%,
Si: 0.15% to 1.10%,
Mn: 17.0% to 30.0%,
P: 0.030% or less,
S: 0.030% or less,
Ni: 0.2% to 13.0%,
Cr: 0.4% to 3.8%,
Mo: 0.1% to 5.0%,
N: 0.060% or less, and
O: 0.020% or less,
with a balance consisting of Fe and inevitable impurities, the weld metal comprising:
a weld metal composition containing, in mass %,
C: 0.10% to 0.80%,
Si: 0.10% to 1.00%,
Mn: 13.0% to 25.0%,
P: 0.030% or less,
S: 0.030% or less,
Ni: 1.0% to 12.0%,
Cr: 0.4% to 3.8%,
Mo: 0.1% to 5.0%,
N: 0.080% or less, and
O: 0.100% or less,
with a balance consisting of Fe and inevitable impurities; and
tensile properties of a 0.2% proof stress WPS of 400 MPa or more and a tensile strength WTS of 660 MPa or more.

### Claim 5 (depends on 4)

The production method for a weld joint according to claim 4, wherein the wire chemical composition further contains, in mass %, one or more selected from the following (v) and (vi): (v) one or more selected from the group consisting of V: 1.0% or less, Ti: 1.0% or less, Nb: 1.0% or less, and W: 1.0% or less; and (vi) one or more selected from the group consisting of Cu: 2.0% or less, Al: 1.0% or less, Ca: 0.010% or less, and REM: 0.020% or less, and
the weld metal chemical composition further contains, in mass %, one or more selected from the following (i) and (ii): (i) one or more selected from the group consisting of V: 1.0% or less, Ti: 1.0% or less, Nb: 1.0% or less, and W: 1.0% or less; and (ii) one or more selected from the group consisting of Cu: 2.0% or less, Al: 1.0% or less, Ca: 0.010% or less, and REM: 0.020% or less.

### Claim 6 (depends on 4)

The production method for a weld joint according to claim 4, wherein the steel plate chemical composition further contains, in mass %, one or more selected from the following (iii) and (iv): (iii) one or more selected from the group consisting of Cu: 0.5% or less, Al: 0.1% or less, Cr: 1.0% or less, Mo: 1.0% or less, V: 0.2% or less, Nb: 0.2% or less, and Ti: 0.2% or less; and (iv) one or more selected from the group consisting of B: 0.005% or less, Ca: 0.005% or less, and REM: 0.020% or less.

### Claim 7 (depends on 2)

The weld joint according to claim 2, wherein the steel plate chemical composition further contains, in mass %, one or more selected from the following (iii) and (iv): (iii) one or more selected from the group consisting of Cu: 0.5% or less, Al: 0.1% or less, Cr: 1.0% or less, Mo: 1.0% or less, V: 0.2% or less, Nb: 0.2% or less, and Ti: 0.2% or less; and (iv) one or more selected from the group consisting of B: 0.005% or less, Ca: 0.005% or less, and REM: 0.020% or less.

### Claim 8 (depends on 5)

The production method for a weld joint according to claim 5, wherein the steel plate chemical composition further contains, in mass %, one or more selected from the following (iii) and (iv): (iii) one or more selected from the group consisting of Cu: 0.5% or less, Al: 0.1% or less, Cr: 1.0% or less, Mo: 1.0% or less, V: 0.2% or less, Nb: 0.2% or less, and Ti: 0.2% or less; and (iv) one or more selected from the group consisting of B: 0.005% or less, Ca: 0.005% or less, and REM: 0.020% or less.