# US 2024/0003095 A1 · Wet cellulose fiber sheet and method for producing cellulose fiber molded body

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0003095 A1
- Document ID: US20240003095A1
- Status: Published application
- Kind: A1
- Application number: 18/038,119
- Filed: 2021-12-01
- Published: 2024-01-04
- Earliest claimed: 2020-12-02
- Assignees: Daio Paper Corporation
- Applicants: Daio Paper Corporation
- Inventors: Kazuto Sawada; Masashi Uno; Kazuo Fujita; Takahiro Miyoshi; Takaaki Imai
- Web page: https://patentgrep.com/patent/US20240003095A1

## CPC

- D21J 3/00: Manufacture of articles by pressing wet fibre pulp, or papier-mâché, between moulds
- D21J 3/12: of sheets; of diaphragms
- D21H 11/18: Highly hydrated, swollen or fibrillatable fibres
- D21H 15/02: characterised by configuration
- D21J: FIBREBOARD; MANUFACTURE OF ARTICLES FROM CELLULOSIC FIBROUS SUSPENSIONS OR FROM PAPIER-MACHE (manufacture of articles by dry processes B27N)
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR

## Abstract

A wet sheet which is hard to be fractured during production into a molded body, stable in shape, and easy to handle in processing, and a method for producing a molded body from the wet sheet. The wet sheet includes fine cellulose fibers having an average fiber diameter of 10000 nm or smaller, and pulp, wherein the wet sheet has a water content of 60 mass % or higher, and a thickness of 0.5 mm or more and 10 mm or less. A method for producing a molded body includes applying heat and pressure to a wet sheet to obtain a molded body, wherein the wet sheet includes fine cellulose fibers having an average fiber diameter of 10000 nm or smaller, and pulp, and has a water content of 60 mass % or higher, and a thickness of 0.5 mm or more and 10 mm or less.

## Claims

### Claim 1

A wet sheet comprising:
fine cellulose fibers having an average fiber diameter of 10000 nm or smaller; and
pulp,
wherein the wet sheet has a water content of 60 mass % or higher, and a thickness of 0.5 mm or more and 10 mm or less.

### Claim 2 (depends on 1)

The wet sheet according to claim 1,
wherein the fine cellulose fibers are at least either of cellulose nanofibers and microfibrillated cellulose having a larger average fiber diameter than that of the cellulose nanofibers.

### Claim 3 (depends on 1)

The wet sheet according to claim 1,
wherein a rate of thickness change determined by formula 1 is 0.4 or lower:
Rate of thickness change=((Thickness of wet sheet after application of pressure at 100 kPa in thickness direction for 1 second)−(Thickness of wet sheet after application of pressure at 100 kPa in thickness direction for 5 seconds))/(Thickness of wet sheet after application of pressure at 100 kPa in thickness direction for 1 second). Formula 1:

### Claim 4 (depends on 1)

The wet sheet according to claim 1,
wherein a solid concentration of the fine cellulose fibers in the wet sheet is 10 mass % or more.

### Claim 5

A method for producing a molded body, comprising:
applying heat and pressure to a wet sheet to obtain a molded body,
wherein the wet sheet includes fine cellulose fibers having an average fiber diameter of 10000 nm or smaller, and pulp, and has a water content of 60 mass % or higher, and a thickness of 0.5 mm or more and 10 mm or less.

### Claim 6

A method for producing a molded body, comprising:
preparing a slurry by mixing fine cellulose fibers having an average fiber diameter of 10000 nm or smaller, and pulp,
shaping the slurry into a wet sheet by holding the slurry between two facing net sheets and applying pressure to the slurry to dewater, and
applying heat and pressure to the wet sheet to obtain a molded body,
wherein the wet sheet has a water content of 60 mass % or higher and a thickness of 0.5 mm or more and 10 mm or less.

### Claim 7 (depends on 5)

The method for producing a molded body according to claim 5,
wherein the fine cellulose fibers are at least either of cellulose nanofibers and microfibrillated cellulose having a larger average fiber diameter than that of the cellulose nanofibers.

### Claim 8 (depends on 5)

The method for producing a molded body according to claim 5,
wherein a rate of thickness change determined by formula 1 is 0.4 or lower:
Rate of thickness change=((Thickness of wet sheet after application of pressure at 100 kPa in thickness direction for 1 second)−(Thickness of wet sheet after application of pressure at 100 kPa in thickness direction for 5 seconds))/(Thickness of wet sheet after application of pressure at 100 kPa in thickness direction for 1 second). Formula 1:

### Claim 9 (depends on 5)

The method for producing a molded body according to claim 5,
wherein a solid concentration of the fine cellulose fibers in the wet sheet is 10 mass % or more.

### Claim 10 (depends on 5)

The method for producing a molded body according to claim 5,
wherein the dewatering is carried out substantially without heating.

### Claim 11 (depends on 2)

The wet sheet according to claim 2,
wherein a rate of thickness change determined by formula 1 is 0.4 or lower:
Rate of thickness change=((Thickness of wet sheet after application of pressure at 100 kPa in thickness direction for 1 second)−(Thickness of wet sheet after application of pressure at 100 kPa in thickness direction for 5 seconds))/(Thickness of wet sheet after application of pressure at 100 kPa in thickness direction for 1 second). Formula 1:

### Claim 12 (depends on 6)

The method for producing a molded body according to claim 6,
wherein the fine cellulose fibers are at least either of cellulose nanofibers and microfibrillated cellulose having a larger average fiber diameter than that of the cellulose nanofibers.