# US 2024/0003094 A1 · Pulp molded container and fabricating method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0003094 A1
- Document ID: US20240003094A1
- Status: Published application
- Kind: A1
- Application number: 18/341,883
- Filed: 2023-06-27
- Published: 2024-01-04
- Earliest claimed: 2022-06-30
- Assignees: Intlpak Enterprises Corporation
- Applicants: Intlpak Enterprises Corporation
- Inventors: Su-Chu CHEN CHUANG
- Web page: https://patentgrep.com/patent/US20240003094A1

## CPC

- D21J 3/10: of hollow bodies
- D21H 11/00: Pulp or paper, comprising cellulose or lignocellulose fibres of natural origin only
- D21H 27/10: Packing paper (packaging materials of special type or form B65D65/38)
- D21J 3/00: Manufacture of articles by pressing wet fibre pulp, or papier-mâché, between moulds
- D21J 7/00: Manufacture of hollow articles from fibre suspensions or papier-mâché by deposition of fibres in or on a wire-net mould
- D21J: FIBREBOARD; MANUFACTURE OF ARTICLES FROM CELLULOSIC FIBROUS SUSPENSIONS OR FROM PAPIER-MACHE (manufacture of articles by dry processes B27N)
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR

## Abstract

A fabricating method of a pulp molded container includes providing a main material, performing a dispersing step, performing a pulping step, performing an additive adding step, and performing a heat compression molding step. The main material includes a long fiber pulp and a short fiber pulp. In the dispersing step, the main material is dispersed evenly in water to form an aqueous pulp solution. In the pulping step, the aqueous pulp solution is mechanically fibrillated to form a fibrillated pulp. In the additive adding step, an additive is added into the fibrillated pulp and mixed to form a paper pulp. In the heat compression molding step, the paper pulp is formed into the pulp molded container by heat compression molding.

## Claims

### Claim 1

A fabricating method of a pulp molded container, comprising:
providing a main material comprising a long fiber pulp and a short fiber pulp, wherein based on the main material being 100% by weight, the long fiber pulp is 1% by weight to 99% by weight;
performing a dispersing step, wherein the main material is dispersed evenly in water to form an aqueous pulp solution;
performing a pulping step, wherein the aqueous pulp solution is mechanically fibrillated to form a fibrillated pulp;
performing an additive adding step, wherein an additive is added into the fibrillated pulp and mixed to form a paper pulp, the additive comprises a nanocellulose and/or a starch, and based on the main material 100% by weight, an added amount of the nanocellulose is 0.1% by weight to 30% by weight, and an added amount of the starch is 1% by weight to 50% by weight; and
performing a heat compression molding step, wherein the paper pulp is formed into the pulp molded container by heat compression molding.

### Claim 2 (depends on 1)

The fabricating method of the pulp molded container of claim 1, wherein the nanocellulose is a nano cellulose fibril, a cellulose nanocrystal or a bacterial nanocellulose, and the starch is a natural starch or a modified starch.

### Claim 3 (depends on 1)

The fabricating method of the pulp molded container of claim 1, wherein the additive further comprises an inorganic substance and/or a polymer, and the polymer does not comprise the nanocellulose and the starch.

### Claim 4 (depends on 3)

The fabricating method of the pulp molded container of claim 3, wherein the inorganic substance comprises calcium carbonate, bentonite, montmorillonite, shell powder, calcium silicate, kaolin, mica, borax, diatomaceous earth, apatite, talc, titanium dioxide, aluminum compound or a mixture thereof, and the polymer comprises poly-butyleneadipate-co-terephthalate, polybutylene-succinate, polybutylene succinate adipate, poly-hydroxyoctanoate, polycaprolactone, polyvinyl alcohol, polylactide, polyglycolic acid, poly-hydroxyalkanoate, poly-hydroxybutyrate, poly(3-hydroxybutyrate-co-3-hydroxyvalerate), p-hydroxybenzoic acid, xanthan gum, cellulose derivative, animal glue, vegetable glue, chitin, protein, polyolefin fiber, maleic anhydride polymer, polyurethane, wax slurry, polyvinyl furanoate, water-based acrylic, alkyl ketene dimer, poly aluminum chlorohydrate or a mixture thereof.

### Claim 5 (depends on 4)

The fabricating method of the pulp molded container of claim 4, wherein based on the main material being 100% by weight, an added amount of the inorganic substance is 1% by weight to 10% by weight, and an added amount of the polymer is 0.1% by weight to 20% by weight.

### Claim 6 (depends on 1)

The fabricating method of the pulp molded container of claim 1, further comprising performing a coating step, wherein a first coating agent and/or a second coating agent is coated on a surface of the pulp molded container.

### Claim 7 (depends on 6)

The fabricating method of the pulp molded container of claim 6, wherein the first coating agent and the second coating agent respectively comprise calcium carbonate, bentonite, montmorillonite, shell powder, calcium silicate, kaolin, mica, borax, diatomaceous earth, apatite, talc, titanium dioxide, aluminum compound, poly-butyleneadipate-co-terephthalate, polybutylene-succinate, polybutylene succinate adipate, poly-hydroxyoctanoate, polycaprolactone, polyvinyl alcohol, polylactide, polyglycolic acid, poly-hydroxyalkanoate, poly-hydroxybutyrate, poly(3-hydroxybutyrate-co-3-hydroxyvalerate), p-hydroxybenzoic acid, xanthan gum, starch, cellulose, cellulose derivative, animal glue, vegetable glue, chitin, protein, polyolefin fiber, maleic anhydride polymer, polyurethane, wax slurry, polyvinyl furanoate, water-based acrylic, alkyl ketene dimer, poly aluminum chlorohydrate or a mixture thereof, and the first coating agent and the second coating agent are the same or different.

### Claim 8 (depends on 6)

The fabricating method of the pulp molded container of claim 6, wherein based on the main material being 100% by weight, a coating amount of the first coating agent is 0.1% by weight to 40% by weight, and a coating amount of the second coating agent is 0.1% by weight to 40% by weight.

### Claim 9 (depends on 1)

The fabricating method of the pulp molded container of claim 1, further comprising performing a pre-starch gelatinization step before the heat compression molding step, wherein the paper pulp is preheated at a temperature greater than 100° C. for more than 1 second to obtain a pre-starch gelatinized paper pulp.

### Claim 10 (depends on 9)

The fabricating method of the pulp molded container of claim 9, wherein in the heat compression molding step, the pre-starch gelatinized paper pulp is hot-pressed at a temperature above 100° C. for more than 10 seconds to perform a gelatinization reaction and shaping, so as to obtain the pulp molded container.

### Claim 11 (depends on 1)

A pulp molded container, wherein the pulp molded container is manufactured by the fabricating method of the pulp molded container of claim 1, and test seconds of a quantitative air permeance test of the pulp molded container are increased by more than 20%.

### Claim 12 (depends on 11)

The pulp molded container of claim 11, wherein the pulp molded container has a sealability and an easy openability, and an easy opening pull force value of the pulp molded container is 50 g to 1200 g.

### Claim 13 (depends on 11)

The pulp molded container of claim 11, wherein the pulp molded container has a hot oil resistance.

### Claim 14 (depends on 11)

The pulp molded container of claim 11, wherein the pulp molded container is used to contain a ready-to-eat food, and the ready-to-eat food is stored in refrigeration or freezing and/or heated in a microwave oven or an oven.