# US 2024/0003090 A1 · Method for manufacturing molded body

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0003090 A1
- Document ID: US20240003090A1
- Status: Published application
- Kind: A1
- Application number: 18/341,797
- Filed: 2023-06-27
- Published: 2024-01-04
- Earliest claimed: 2022-06-29
- Assignees: Seiko Epson Corporation
- Applicants: Seiko Epson Corporation
- Inventors: Shigemi WAKABAYASHI; Masahiko NAKAZAWA; Takumi SAGO; Takashi SHINOHARA
- Web page: https://patentgrep.com/patent/US20240003090A1

## CPC

- D21H 23/08: by measuring pulp properties, e.g. zeta potential, pH
- B31D 5/02: including pressing
- D21F 5/022: {Heating the cylinders}
- D21H 17/28: Starch
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR
- B31D: MAKING ARTICLES OF PAPER, CARDBOARD OR MATERIAL WORKED IN A MANNER ANALOGOUS TO PAPER, NOT PROVIDED FOR IN SUBCLASSES B31B OR B31C (manufacture by dry processes of articles made from particles or fibres consisting of wood or other lignocellulosic or like organic material B27N; making layered products not composed wholly of paper or cardboard B32B; making articles from cellulosic fibrous suspensions, e.g. wood pulp, D21J)
- D21F: PAPER-MAKING MACHINES; METHODS OF PRODUCING PAPER THEREON

## Abstract

A method for manufacturing a molded body, includes a deposition step of depositing a mixture containing fibers and a starch in air; a moisturizing step of applying water to the mixture; and a molding step of forming a molded body by heating and pressurizing the mixture to which the water is applied. In the method described above, the starch has a setback viscosity (η50-η93) of 40 to 200 mPa·s, the setback viscosity (η50-η93) being obtained by measurement performed in accordance with the following measurement methods (1) to (4) using a rapid visco analyzer (RVA). The measurement is performed such that (1) after a water suspension containing the starch at 25 percent by mass is charged in the RVA as a measurement sample, the temperature thereof is increased to 50° C. and then maintained for one minute; (2) the temperature of the measurement sample is increased from 50° C. to 93° C. over 4 minutes and then maintained at 93° C. for 7 minutes; (3) the temperature of the measurement sample is decreased from 93° C. to 50° C. over 4 minutes and then maintained at 50° C. for 3 minutes; and (4) in the above (2) and (3), a rotational speed of a measurement paddle of the RVA is set to 960 rpm for 10 seconds after the start of the viscosity measurement and is then set to 160 rpm 10 seconds thereafter.

## Claims

### Claim 1

A method for manufacturing a molded body, comprising:
a deposition step of depositing a mixture containing fibers and a starch in air;
a moisturizing step of applying water to the mixture; and
a molding step of forming a molded body by heating and pressurizing the mixture to which the water is applied,
wherein the starch has a setback viscosity (η50-η93) of 40 to 200 mPa·s, the setback viscosity (η50-η93) being obtained by measurement performed in accordance with the following measurement methods (1) to (4) using a rapid visco analyzer (RVA), and
the measurement is performed such that
(1) after a water suspension containing the starch at 25 percent by mass is charged in the RVA as a measurement sample, the temperature thereof is increased to 50° C. and then maintained for one minute;
(2) the temperature of the measurement sample is increased from 50° C. to 93° C. over 4 minutes and then maintained at 93° C. for 7 minutes;
(3) the temperature of the measurement sample is decreased from 93° C. to 50° C. over 4 minutes and then maintained at 50° C. for 3 minutes; and
(4) in the above (2) and (3), a rotational speed of a measurement paddle of the RVA is set to 960 rpm for 10 seconds after the start of the viscosity measurement and is then set to 160 rpm 10 seconds thereafter.

### Claim 2 (depends on 1)

The method for manufacturing a molded body according to claim 1,
wherein a heating temperature of the mixture in the molding step is 60° C. to 200° C.

### Claim 3 (depends on 1)

The method for manufacturing a molded body according to claim 1,
wherein the molding step is performed by a pair of heating rollers.

### Claim 4 (depends on 1)

The method for manufacturing a molded body according to claim 1,
wherein a pressurizing force in the molding step is 0.2 to 10.0 MPa.

### Claim 5 (depends on 1)

The method for manufacturing a molded body according to claim 1,
wherein an amount of the water applied in the moisturizing step with respect to a total mass of the mixture is 12 to 40 percent by mass.

### Claim 6 (depends on 1)

The method for manufacturing a molded body according to claim 1,
wherein the starch is in the form of powder composed of a plurality of starch particles, and an average particle diameter of the starch particles is 1.0 to 30.0 μm.

### Claim 7 (depends on 6)

The method for manufacturing a molded body according to claim 6,