# US 2024/0003049 A1 · Method for growing silicon single crystal

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0003049 A1
- Document ID: US20240003049A1
- Status: Published application
- Kind: A1
- Application number: 18/030,000
- Filed: 2021-07-30
- Published: 2024-01-04
- Earliest claimed: 2020-10-09
- Assignees: Sumco Corporation
- Applicants: Sumco Corporation
- Inventors: Yasufumi KAWAKAMI; Kazuyoshi SAKATANI
- Web page: https://patentgrep.com/patent/US20240003049A1

## CPC

- C30B 15/22: Stabilisation or shape controlling of the molten zone near the pulled crystal; Controlling the section of the crystal
- C30B 15/04: adding doping materials, e.g. for n-p-junction
- C30B 29/06: Silicon
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

A method of growing monocrystalline silicon through a Czochralski process uses a monocrystalline silicon growth device, the device including: a chamber; a crucible; a heater configured to heat a silicon melt contained in the crucible, in which the heater includes: an upper heater configured to heat an upper portion of the crucible; and a lower heater configured to heat a lower portion of the crucible; and a pull-up unit configured to pull up a seed crystal after bringing the seed crystal into contact with the silicon melt. The method includes: adding a volatile dopant to the silicon melt; and subsequently to the step, pulling up the monocrystalline silicon. In the step, the crucible is heated in a manner that no solidified layer is formed on a liquid surface of the silicon melt and heat generation amounts Qd, Qu of the lower heater and the upper heater satisfy Qd>Qu.

## Claims

### Claim 1

A method of growing monocrystalline silicon according to a Czochralski process using a monocrystalline silicon growth device, the device comprising:
a chamber;
a crucible disposed in the chamber;
a heater configured to heat a silicon melt contained in the crucible, the heater comprising an upper heater configured to heat an upper portion of the crucible and a lower heater configured to heat a lower portion of the crucible; and
a pull-up unit configured to pull up a seed crystal after bringing the seed crystal into contact with the silicon melt, the method comprising:
adding a volatile dopant to the silicon melt;
subsequently to the adding of the volatile dopant, pulling up the monocrystalline silicon, wherein
in the adding of the volatile dopant, the crucible is heated in a manner that no solidified layer is formed on a liquid surface of the silicon melt and a heat generation amount Qd of the lower heater and a heat generation amount Qu of the upper heater satisfy Qd>Qu.

### Claim 2 (depends on 1)

The method of growing monocrystalline silicon according to claim 1, wherein the volatile dopant is red phosphorus, arsenic, or antimony.

### Claim 3 (depends on 1)

The method of growing monocrystalline silicon according to claim 1, wherein in the adding of the volatile dopant, the crucible is heated in a manner that a heat generation ratio Qd/Qu is in a range from 1.5 to 4.0, the heat generation ratio Qd/Qu being obtained by dividing the heat generation amount Qd of the lower heater by the heat generation amount Qu of the upper heater.

### Claim 4 (depends on 3)

The method of growing monocrystalline silicon according to claim 3, wherein
the pulling up of the monocrystalline silicon comprises growing a neck, and
a heat generation ratio Qd/Qu in the growing of the neck is 100±10% of the heat generation ratio Qd/Qu in the adding of the volatile dopant.

### Claim 5 (depends on 3)

The method of growing monocrystalline silicon according to claim 3, wherein
the pulling up of the monocrystalline silicon comprises growing a shoulder,
in a case where a target oxygen concentration in a straight body is 12.0×1017 atoms/cm3 or more, a heat generation ratio Qd/Qu at least at completion of the growing of the shoulder is in a range from 3.5 to 4.5, and
in a case where the target oxygen concentration in the straight body is less than 12.0×1017 atoms/cm3, the heat generation ratio Qd/Qu at least at the completion of the growing of the shoulder is in a range from 0.75 to 1.25.

### Claim 6 (depends on 5)

The method of growing monocrystalline silicon according to claim 5, further comprising, in or after the growing of the shoulder, determining first whether a dislocation occurs in the shoulder, wherein
in a case where it is determined that the dislocation occurs in the shoulder in the first determining of whether the dislocation occurs, the pull-up operation is stopped and melting the monocrystalline silicon into the silicon melt is executed, and
a heat generation ratio Qd/Qu in the melting of the monocrystalline silicon is in a range from 1.5 to 3.0.

### Claim 7 (depends on 3)

The method of growing monocrystalline silicon according to claim 3, further comprising, subsequently to the pulling up of the monocrystalline silicon, pulling up another or more pieces of monocrystalline silicon using the crucible unchanged, wherein
prior to the pulling up of the another or more pieces of monocrystalline silicon, the volatile dopant is added to a silicon melt for the another or more pieces of monocrystalline silicon, and
in the adding of the volatile dopant, the crucible is heated in a manner that the heat generation ratio Qd/Qu is in a range from 1.5 to 4.0.