# US 2024/0003046 A1 · Single crystal manufacturing apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0003046 A1
- Document ID: US20240003046A1
- Status: Published application
- Kind: A1
- Application number: 18/037,802
- Filed: 2021-11-01
- Published: 2024-01-04
- Earliest claimed: 2020-12-10
- Assignees: Shin-Etsu Handotai Co., Ltd.
- Applicants: Shin-Etsu Handotai Co., Ltd.
- Inventors: Keisuke MIHARA; Kazuya YANASE; Nobuaki MITAMURA; Kiyotaka TAKANO
- Web page: https://patentgrep.com/patent/US20240003046A1

## CPC

- C30B 15/14: Heating of the melt or the crystallised materials
- C30B 15/10: Crucibles or containers for supporting the melt
- C30B 29/06: Silicon
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

A single crystal manufacturing including: main chamber; pulling chamber; thermal shield member provided so as to face a silicon melt; rectifying cylinder provided on the thermal shield member so as to enclose the silicon single crystal being pulled up; cooling cylinder provided so as to encircle the silicon single crystal being pulled up and including an extending portion extending toward the silicon melt; and cooling auxiliary cylinder fitted to inside of the cooling cylinder. The extending portion of the cooling cylinder includes a bottom surface facing the silicon melt. The cooling auxiliary cylinder includes at least a first portion surrounding the bottom surface of the cooling cylinder and a second portion surrounding an upper end portion of the rectifying cylinder. This enables provision of the apparatus capable of manufacturing a single crystal with a carbon concentration lower than that according to the conventional technologies.

## Claims

### Claim 1

A single crystal manufacturing apparatus for growing a single crystal by using a Czochralski method, the apparatus comprising:
a main chamber comprising a ceiling portion, and housing a crucible for containing a silicon melt;
a pulling chamber provided continuously at an upper portion of the ceiling portion of the main chamber via a gate valve, and configured to contain a silicon single crystal to be pulled up from the silicon melt;
a thermal shield member provided so as to face the silicon melt contained in the crucible;
a rectifying cylinder provided on the thermal shield member so as to enclose the silicon single crystal being pulled up;
a cooling cylinder provided so as to encircle the silicon single crystal being pulled up, comprising an extending portion extending from the ceiling portion of the main chamber toward the silicon melt, and configured to be forcibly cooled by a cooling medium; and
a cooling auxiliary cylinder fitted to inside of the cooling cylinder,
wherein the extending portion of the cooling cylinder includes a bottom surface facing the silicon melt, and
wherein the cooling auxiliary cylinder includes at least a first portion surrounding the bottom surface of the cooling cylinder and a second portion surrounding an upper end portion of the rectifying cylinder.

### Claim 2 (depends on 1)

The single crystal manufacturing apparatus according to claim 1, wherein the rectifying cylinder is made of synthetic quartz.

### Claim 3 (depends on 1)

The single crystal manufacturing apparatus according claim 1,
wherein the cooling auxiliary cylinder includes at least one selected from the group consisting of a graphite member, a carbon composite member, stainless steel, molybdenum, and tungsten, and
wherein the first portion of the cooling auxiliary cylinder has a structure of covering the bottom surface of the cooling cylinder, and a gap between the first portion of the cooling auxiliary cylinder and the bottom surface of the cooling cylinder is 1.0 mm or less.

### Claim 4 (depends on 1)

The single crystal manufacturing apparatus according claim 1, wherein the second portion of the cooling auxiliary cylinder includes a groove portion covering a region having an area of 10% or more and 35% or less of a whole area of a side surface of the rectifying cylinder.

### Claim 5 (depends on 4)

The single crystal manufacturing apparatus according to claim 4, wherein a clearance between each of side surfaces of the upper end portion of the rectifying cylinder and a side surface of the groove portion of the second portion of the cooling auxiliary cylinder is 5 mm or more and 25 mm or less.

### Claim 6 (depends on 1)

The single crystal manufacturing apparatus according claim 1, wherein the rectifying cylinder includes an opening in a side surface thereof, and the opening of the rectifying cylinder is formed at such a position as that a height of an upper end of the opening of the rectifying cylinder is 35% or less of a whole height of the rectifying cylinder.

### Claim 7

A single crystal manufacturing apparatus for growing a single crystal by using a Czochralski method, the apparatus comprising:
a main chamber comprising a ceiling portion, and housing a crucible for containing a silicon melt;
a pulling chamber provided continuously at an upper portion of the ceiling portion of the main chamber via a gate valve, and configured to contain a silicon single crystal to be pulled up from the silicon melt;
a thermal shield member provided so as to face the silicon melt contained in the crucible;
a rectifying cylinder provided on the thermal shield member so as to enclose the silicon single crystal being pulled up;
a cooling cylinder provided so as to encircle the silicon single crystal being pulled up, comprising an extending portion extending from the ceiling portion of the main chamber toward the silicon melt, and configured to be forcibly cooled by a cooling medium; and
a cooling auxiliary cylinder fitted to inside of the cooling cylinder,
wherein an upper portion of the rectifying cylinder has a structure of surrounding a lower portion of the cooling auxiliary cylinder, the lower portion being a portion projecting downward from the cooling cylinder.

### Claim 8 (depends on 7)

The single crystal manufacturing apparatus according to claim 7, wherein the rectifying cylinder is made of synthetic quartz.

### Claim 9 (depends on 7)

The single crystal manufacturing apparatus according claim 7, wherein a material of the cooling auxiliary cylinder is at least one selected from the group consisting of a graphite member, a carbon composite member, stainless steel, molybdenum, and tungsten.

### Claim 10 (depends on 7)

The single crystal manufacturing apparatus according to claim 7, wherein the rectifying cylinder has a structure of surrounding a region having an area of 5% or more of a whole area of a side surface of the portion of the cooling auxiliary cylinder projecting downward from the cooling cylinder with an upper portion of the rectifying cylinder.

### Claim 11 (depends on 7)

The single crystal manufacturing apparatus according to claim 7, wherein a clearance between a side surface of the rectifying cylinder and a side surface of the portion of the cooling auxiliary cylinder, the portion projecting downward from the cooling cylinder, is 3 mm or more and less than 15 mm.

### Claim 12 (depends on 7)

The single crystal manufacturing apparatus according to claim 7, wherein the rectifying cylinder includes an opening in a side surface thereof, and the opening of the rectifying cylinder is formed at such a position as that a height of an upper end of the opening of the rectifying cylinder is 35% or less of a whole height of the rectifying cylinder.