# US 2024/0003034 A1 · Composite dispersant, preparation method therefor, mixed electroplating solution, and preparation method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0003034 A1
- Document ID: US20240003034A1
- Status: Published application
- Kind: A1
- Application number: 18/252,840
- Filed: 2022-03-31
- Published: 2024-01-04
- Earliest claimed: 2021-04-01
- Assignees: Zhejiang Chint Electrics Co., Ltd.
- Applicants: Zhejiang Chint Electrics Co.,Ltd.
- Inventors: Qi SHEN; Junyu LIN; Jianyong ZHENG; Yiming HU; Chuan WANG; Rongzhen LIN; Shen JI; Zhengli XU; Jinyu ZHOU; Lang ZENG
- Web page: https://patentgrep.com/patent/US20240003034A1

## CPC

- C25D 3/46: of silver
- C25D 15/00: Electrolytic or electrophoretic production of coatings containing embedded materials, e.g. particles, whiskers, wires
- C01B 32/194: After-treatment
- C09K 23/017: {Mixtures of compounds}
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

A compound dispersant which is composed of distilled water, a nonionic surfactant, an anionic surfactant and a wetting agent. The nonionic surfactant is a Tween compound, and the anionic surfactant is hydrocarbyl sulfate salts. The compound dispersant can block or slow down agglomeration of graphene in a dispersion solution. Also disclosed are a preparation method of the compound dispersant, which is simple to operate, a mixed electroplating solution containing the compound dispersant, in which the graphene is dispersed uniformly and stably, and a preparation method of the mixed electroplating solution, in which graphene is distributed uniformly and stably.

## Claims

### Claim 1

A compound dispersant, composed of distilled water, a nonionic surfactant, an anionic surfactant and a wetting agent, wherein the nonionic surfactant is a Tween compound, and the anionic surfactant is hydrocarbyl sulfate salts.

### Claim 2 (depends on 1)

The compound dispersant as claimed in claim 1, wherein the wetting agent comprises one or more of polyvinylpyrrolidone, dodecylphenol ethoxylate, sodium pyrrolidone carboxylate and macrogol 600.

### Claim 3 (depends on 1)

The compound dispersant as claimed in claim 1, wherein the Tween compound comprises one or more of Tween-20, Tween-40, Tween-60 and Tween-80.

### Claim 4 (depends on 1)

The compound dispersant as claimed in claim 1, wherein the hydrocarbyl sulfate salts includes one or more of sodium 2-ethylhexyl sulfate, sodium dodecyl sulfate, sodium lauryl ether sulfate, sodium fatty alcohol ethoxyethylene sulfate, glycerol fatty acid ester sulfate, sulfated sodium ricinoleate and sulfated fatty acid salt.

### Claim 5 (depends on 1)

The compound dispersant as claimed in claim 1, wherein a mass fraction of the nonionic surfactant in the compound dispersant is 1-10%.

### Claim 6 (depends on 1)

The compound dispersant as claimed in claim 1, wherein a mass fraction of the wetting agent in the compound dispersant is 1-10%.

### Claim 7 (depends on 1)

The compound dispersant as claimed in claim 1, wherein a mass fraction of the anionic surfactant in the compound dispersant is 1-10%.

### Claim 8

A preparation method for a compound dispersant, comprising the following steps:
adding an anionic surfactant and a nonionic surfactant to distilled water at a temperature of T0, and stirring for t0, 40° C.≤T0≤60° C., 5 min≤t0≤15 min, wherein the anionic surfactant is hydrocarbyl sulfate salts, and the nonionic surfactant is a Tween compound (Step 1); and
adding a wetting agent to a mixture obtained in Step 1, supplementing with distilled water and stirring for t1 to obtain the compound dispersant, 5 min≤t1≤15 min, wherein in the compound dispersant, a mass fraction of the nonionic surfactant is 1-10%, a mass fraction of the anionic surfactant is 1-10%, a mass fraction of the wetting agent is 1-10%, and the balance is distilled water.

### Claim 9 (depends on 1)

A mixed electroplating solution, comprising the compound dispersant as claimed in claim 1, a silver-based aqueous solution and graphene, the silver-based aqueous solution comprises KCN and silver ions.

### Claim 10 (depends on 9)

The mixed electroplating solution as claimed in claim 9, wherein in the silver-based aqueous solution, a mass-volume concentration of KCN is 90.0-200.0 g/L, and a mass-volume concentration of silver ions is 15.0-50.0 g/L.

### Claim 11 (depends on 9)

The mixed electroplating solution as claimed in claim 9, wherein a mass-volume concentration of graphene in the mixed electroplating solution is 1.0-20.0 g/L; and a volume by volume concentration of the compound dispersant in the mixed electroplating solution is 15.0-35.0 ml/L.

### Claim 12 (depends on 9)

The mixed electroplating solution as claimed in claim 9, wherein a barrel plating current density of the mixed electroplating solution is 0.5-0.7 A/dm3; and a rack plating current density of the mixed electroplating solution is 0.7-1.0 A/dm3.

### Claim 13 (depends on 1)

A preparation method of a mixed electroplating solution, comprising the following steps:
preparing a silver-based aqueous solution, wherein in the silver-based aqueous solution, a mass-volume concentration of KCN is 90.0-200.0 g/L, and a mass-volume concentration of silver ions is 15.0-50.0 g/L (S1); and
adding the compound dispersant as claimed in claim 1 and graphene sequentially to the mixture obtained in S1, and stirring to prepare the mixed electroplating solution, wherein in the mixed electroplating solution, a volume by volume concentration of the graphene is 1.0-20.0 g/L, and a volume by volume concentration of the compound dispersant is 15.0-35.0 ml/L.