# US 2024/0003033 A1 · Compound dispersant and preparation method, and mixed electroplating solution and preparation method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0003033 A1
- Document ID: US20240003033A1
- Status: Published application
- Kind: A1
- Application number: 18/252,829
- Filed: 2022-03-31
- Published: 2024-01-04
- Earliest claimed: 2021-04-01
- Assignees: Zhejiang Chint Electrics Co., Ltd.
- Applicants: Zhejiang Chint Electrics Co.,Ltd.
- Inventors: Yiming HU; Chuan WANG; Rongzhen LIN; Shen JI; Zhengli XU; Jinyu ZHOU; Lang ZENG; Qi SHEN; Junyu LIN; Jianyong ZHENG
- Web page: https://patentgrep.com/patent/US20240003033A1

## CPC

- C01B 32/194: After-treatment
- C25D 3/46: of silver
- C09K 23/017: {Mixtures of compounds}
- C25D 15/00: Electrolytic or electrophoretic production of coatings containing embedded materials, e.g. particles, whiskers, wires
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

A compound dispersant which is composed of distilled water, a nonionic surfactant, an anionic surfactant and a wetting agent. The nonionic surfactant is a Tween compound, the anionic surfactant is a hydrocarbyl sulfonate salt compound, and the wetting agent is an amide compound. The compound dispersant can block or slow down agglomeration of graphene in a dispersion solution. In addition, disclosed are a preparation method of the compound dispersant, which is used for preparing the compound dispersant and is simple to operate, a mixed electroplating solution containing the compound dispersant, in which the graphene is dispersed uniformly and stably, and a preparation method of the mixed electroplating solution, in which graphene is distributed uniformly and stably.

## Claims

### Claim 1

A compound dispersant, being composed of distilled water, a nonionic surfactant, an anionic surfactant and a wetting agent, wherein the nonionic surfactant is a Tween compound, the anionic surfactant is a hydrocarbyl sulfonate salt compound, and the wetting agent is an amide compound.

### Claim 2 (depends on 1)

The compound dispersant as claimed in claim 1, wherein the wetting agent comprises one or more of polyvinylpyrrolidone, alkylamide, diglycolamide laurate, sodium pyrrolidone carboxylate, polyoxyethylene alkylamide and alkylolamide(s).

### Claim 3 (depends on 1)

The compound dispersant as claimed in claim 1, wherein the nonionic surfactant comprises one or more of Tween-20, Tween-40, Tween-60 and Tween-80.

### Claim 4 (depends on 1)

The compound dispersant as claimed in claim 1, wherein the anionic surfactant comprises one or more of dihexyl sodium sulfosuccinate, sodium lauryl succinate monoester sulfonate, disodium 4-dodecyl-2,4′-oxydibenzenesulfonate, lauryl sulfosuccinate monoester sodium two, disodium laureth (3) sulfosuccinate, dioctyl sulfosuccinate sodium salt and dioctyl sulfosuccinate sodium salt.

### Claim 5 (depends on 1)

The compound dispersant as claimed in claim 1, wherein a mass fraction of the nonionic surfactant in the compound dispersant is 1-10%; a mass fraction of the wetting agent in the compound dispersant is 1-10%; and a mass fraction of the anionic surfactant in the compound dispersant is 1-10%.

### Claim 6

A preparation method for a compound dispersant, comprising the following steps:
adding an anionic surfactant and a non-ionic surfactant to distilled water at a temperature of T0, and stirring for t0, 40° C.≤T0≤60° C., 5≤t0≤15 min (Step 1); and
adding a wetting agent to a mixture obtained in Step 1, supplementing with the distilled water and stirring for t1 to obtain the compound dispersant, 5 min≤t1≤15 min, wherein in the compound dispersant, a mass fraction of the nonionic surfactant is 1-10%, a mass fraction of the anionic surfactant is 1-10%, a mass fraction of the wetting agent is 1-10%, and the balance is distilled water.

### Claim 7 (depends on 6)

The preparation method of the compound dispersant as claimed in claim 6, wherein the wetting agent comprises one or more of polyvinylpyrrolidone, alkylamide, diglycolamide laurate, sodium pyrrolidone carboxylate, polyoxyethylene alkylamide and alkylolamide(s).

### Claim 8 (depends on 6)

The preparation method of the compound dispersant as claimed in claim 6, wherein the nonionic surfactant comprises one or more of Tween-20, Tween-40, Tween-60 and Tween-80.

### Claim 9 (depends on 6)

The preparation method of the compound dispersant as claimed in claim 6, wherein the anionic surfactant comprises one or more of dihexyl sodium sulfosuccinate, sodium lauryl succinate monoester sulfonate, disodium 4-dodecyl-2,4′-oxydibenzenesulfonate, lauryl sulfosuccinate monoester sodium two, disodium laureth (3) sulfosuccinate, dioctyl sulfosuccinate sodium salt and dioctyl sulfosuccinate sodium salt.

### Claim 10 (depends on 1)

A mixed electroplating solution, comprising the compound dispersant as claimed in claim 1, a silver-based aqueous solution and graphene, the silver-based aqueous solution comprises KCN and silver ions.

### Claim 11 (depends on 10)

The mixed electroplating solution as claimed in claim 10, wherein,
a volume by volume concentration of the compound dispersant in the mixed electroplating solution is 15.0-45.0 ml/L;
a mass-volume concentration of KCN in the silver-based aqueous solution is 90.0-200.0 g/L;
a mass-volume concentration of silver ions in the silver-based aqueous solution is 15.0-50.0 g/L; and
a mass-volume concentration of graphene in the mixed electroplating solution is 1.0-20.0 g/L.

### Claim 12 (depends on 10)

The mixed electroplating solution as claimed in claim 10, wherein a barrel plating current density of the mixed electroplating solution is 0.5-0.7 A/dm3; and
a rack plating current density of the mixed electroplating solution is 0.7-1.0 A/dm3.

### Claim 13 (depends on 1)

A preparation method of a mixed electroplating solution, comprising the following steps:
preparing a silver-based aqueous solution, wherein in the silver-based aqueous solution, a mass-volume concentration of KCN is 90.0-200.0 g/L, and a mass-volume concentration of silver ions is 15.0-50.0 g/L; and
adding the compound dispersant as claimed in claim 1 and graphene sequentially to the silver-based aqueous solution, and mixing under stirring to prepare the mixed electroplating solution, wherein in the mixed electroplating solution, a volume by volume concentration of the compound dispersant is 15.0-45.0 ml/L, and a mass-volume concentration of the graphene is 1.0-20.0 g/L.