# US 2024/0002993 A1 · Coated steel sheet and high strength press hardened steel part and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0002993 A1
- Document ID: US20240002993A1
- Status: Published application
- Kind: A1
- Application number: 18/038,104
- Filed: 2021-12-03
- Published: 2024-01-04
- Earliest claimed: 2020-12-16
- Assignees: ArcelorMittal
- Applicants: ArcelorMittal
- Inventors: Clément PHILIPPOT; Alice DUMONT; Deborah HERRY; Martin BEAUVAIS
- Web page: https://patentgrep.com/patent/US20240002993A1

## CPC

- C23C 2/12: Aluminium or alloys based thereon
- B21C 47/02: Winding-up or coiling
- C21D 1/02: Hardening articles or materials formed by forging or rolling, with no further heating beyond that required for the formation
- C21D 1/673: for die quenching
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/0226: {Hot rolling}
- C21D 8/0257: {with diffusion of elements, e.g. decarburising, nitriding}
- C21D 8/0263: {following hot rolling}
- C21D 8/0273: {Final recrystallisation annealing}
- C21D 8/0278: involving a particular surface treatment (C21D8/0294 takes precedence)
- C21D 9/46: for sheet metals
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/28: with titanium or zirconium
- C22C 38/32: with boron
- C22C 38/38: with more than 1.5% by weight of manganese
- C23C 2/02: Pretreatment of the material to be coated, e.g. for coating on selected surface areas (C23C2/30 takes precedence)
- C23C 2/0224: {Two or more thermal pretreatments}
- C23C 2/024: {by cleaning or etching}
- C23C 2/29: {Cooling or quenching}
- C23C 2/40: Plates; Strips
- C23C 30/00: Coating with metallic material characterised only by the composition of the metallic material, i.e. not characterised by the coating process (C23C26/00, C23C28/00 take precedence)
- C23G 1/08: Iron or steel
- C21D 2211/001: Austenite
- C21D 2211/002: Bainite
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B21C: MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES, PROFILES OR LIKE SEMI-MANUFACTURED PRODUCTS OTHERWISE THAN BY ROLLING; AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKING WITHOUT ESSENTIALLY REMOVING MATERIAL
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23G: CLEANING OR DE-GREASING OF METALLIC MATERIAL BY CHEMICAL METHODS OTHER THAN ELECTROLYSIS

## Abstract

A coated steel sheet and press hardened steel part having a composition including, by weight percent: C 0.15-0.25%, Mn 0.5-1.8%, Si 0.1-1.25%, Al 0.01-0.1%, Cr 0.1-1.0%, Ti 0.01-0.1%, B 0.001-0.004%, P≤0.020%, S≤0.010%, N≤0.010% the remainder of the composition being iron and unavoidable impurities resulting from the smelting. The press hardened steel part includes a bulk having a microstructure including, in surface fraction, more than 95% of martensite and less than 5% of bainite, a coating layer at the surface of the steel part, a ferritic interdiffusion layer between the coating layer and the bulk, and a ratio between the ferritic grain width in the interdiffusion layer GWint over prior austenite grain size in the bulk PAGSbulk, satisfying following equation (GWint/PAGSbulk)−1≥30%.

## Claims

### Claim at position 1

1-7. (canceled)

### Claim at position 2

8: A coated steel sheet made of a steel having a composition comprising, by weight percent:
C: 0.15-0.25%
Mn: 0.5-1.80%
Si: 0.1-1.250%
Al: 0.01-0.10%
Cr: 0.1-1.00%
Ti: 0.01-0.1%
B: 0.001-0.004%
P≤0.020%
S≤0.0100%
N≤0.010%
and comprising optionally one or more of the following elements, by weight percent:
Mo≤0.40%
Nb≤0.08%
Ca≤0.1%
a remainder of the composition being iron and unavoidable impurities resulting from processing;
the coated steel sheet comprising from a bulk to the surface of the coated steel sheet:
the bulk with a microstructure comprising, in surface fraction, from 60% to 90% of ferrite,
a rest being martensite-austenite islands, pearlite or bainite,
a decarburized layer topping the bulk and comprising in upper part a ferrite layer having a thickness from 1 μm to 100 μm; and
a coating layer made of aluminum or aluminum alloy.

### Claim at position 3

9: A method for producing a coated steel sheet, the method comprising the following successive steps:
casting a steel to obtain a slab, the steel having a composition comprising, by weight percent:
C: 0.15-0.25%
Mn: 0.5-1.80%
Si: 0.1-1.250%
Al: 0.01-0.1%
Cr: 0.1-1.00%
Ti: 0.01-0.1%
B: 0.001-0.004%
P≤0.020%
S≤0.0100%
N≤0.010%
and comprising optionally one or more of the following elements, by weight percent:
Mo≤0.40%
Nb≤0.08%
Ca≤0.1%
a remainder of the composition being iron and unavoidable impurities resulting from processing;
reheating the slab at a temperature Treheat of 1100° C. to 1300° C.;
hot rolling the reheated slab at a finish hot rolling temperature of 800° C. to 950° C.;
coiling the hot rolled steel sheet at a coiling temperature Tcoil lower than 670° C. to obtain a coiled steel sheet;
optionally pickling the coiled steel sheet;
optionally cold rolling the coiled steel sheet to obtain a cold rolled steel sheet;
heating the hot rolled steel sheet or the cold rolled steel sheet to an annealing temperature TA of 700° C. to 850° C. and maintaining the steel sheet at the temperature TA for a holding time tA of 10s to 1200s, to obtain an annealed steel sheet, the atmosphere comprising from 0% to 15% of H2 and having a dew point TDP1 strictly higher than −10° C. and below or equal to +20° C.;
cooling the annealed steel sheet to a temperature range from 560° C. to 700° C.;
coating the annealed steel sheet with aluminum or with an aluminum alloy coating; and
cooling the coated steel sheet to room temperature.

### Claim at position 4

10: A press hardened steel part, the steel part having a composition comprising, by weight percent:
C: 0.15-0.25%
Mn: 0.5-1.80%
Si: 0.1-1.250%
Al: 0.01-0.1%
Cr: 0.1-1.00%
Ti: 0.01-0.1%
B: 0.001-0.004%
P≤0.020%
S≤0.0100%
N≤0.010%
and comprising optionally one or more of the following elements, by weight percent:
Mo≤0.40%
Nb≤0.08%
Ca≤0.1%
the remainder of the composition being iron and unavoidable impurities resulting from processing;
the steel part comprising successively from the bulk to the surface of the steel part:
a bulk having a microstructure comprising, in surface fraction, more than 95% of martensite and less than 5% of bainite,
a ferritic interdiffusion layer,
a coating layer based on aluminum,
wherein a ratio between the ferritic grain width in the interdiffusion layer GWint over prior austenite grain size in the bulk PAGSbulk, satisfies the following equation:
(GWint/PAGSbulk)−1≥30%

### Claim at position 5 (depends on 10)

11: The press hardened steel part as recited in claim 10 wherein the press hardened steel part includes a layer of martensite with a carbon gradient between the bulk and the ferritic interdiffusion layer.

### Claim at position 6 (depends on 10)

12: The press hardened steel part as recited in claim 10 wherein the press hardened steel part has a tensile strength TS above or equal to 1350 MPa and a bending angle higher than 70°.

### Claim at position 7 (depends on 12)

13: The press hardened steel part as recited in claim 12 wherein the press hardened steel part has a yield strength YS above or equal to 1000 MPa

### Claim at position 8 (depends on 12)

14: A process for manufacturing the press hardened steel part as recited in claim 12, the process comprising the following successive steps:
providing a steel sheet having the composition;
cutting the steel sheet to a predetermined shape, so as to obtain a steel blank;
heating the steel blank to a temperature of 880° C. to 950° C. for 10s to 900s to obtain a heated steel blank;
transferring the heated steel blank to a forming press;
hot-forming the heated blank in the forming press to obtain a formed part; and
die-quenching the formed part.