# US 2024/0002992 A1 · Hot press formed product having excellent corrosion resistance and method for preparing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0002992 A1
- Document ID: US20240002992A1
- Status: Published application
- Kind: A1
- Application number: 18/468,268
- Filed: 2023-09-15
- Published: 2024-01-04
- Earliest claimed: 2015-12-22
- Assignees: Posco
- Applicants: Posco Co., Ltd
- Inventors: Il-Ryoung SOHN; Hyeon-Seok HWANG; Jong-Sang KIM
- Web page: https://patentgrep.com/patent/US20240002992A1

## CPC

- C23C 2/06: Zinc or cadmium or alloys based thereon
- B21D 22/02: Stamping using rigid devices or tools
- B21D 22/022: {by heating the blank or stamping associated with heat treatment (C21D takes precedence)}
- B21D 37/16: Heating or cooling
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0247: characterised by the heat treatment
- C21D 8/0278: involving a particular surface treatment (C21D8/0294 takes precedence)
- C21D 9/46: for sheet metals
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C23C 2/02: Pretreatment of the material to be coated, e.g. for coating on selected surface areas (C23C2/30 takes precedence)
- C23C 2/022: {by heating}
- C23C 2/261: {in a gas atmosphere, e.g. inert or reducing atmosphere}
- C23C 2/29: {Cooling or quenching}
- B21D 35/005: {characterized by the material of the blank or the workpiece (B21D26/053 takes precedence)}
- B21D 53/88: other parts for vehicles, e.g. cowlings, mudguards
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B21D: WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS OR PROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL; PUNCHING METAL (working or processing of wire B21F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

Provided is a hot press formed product, which is prepared by means of hot press forming of a Zn—Al—Mg-based plated steel material comprising base iron and a Zn—Al—Mg-based plated layer, and a method for preparing the same, the hot press formed product comprising an oxide layer formed on the surface thereof, wherein the content ratio of Al to Mg (Al/Mg) in the oxide layer is 0.8 or more.

## Claims

### Claim 1

A hot press formed product comprising:
a base iron,
a Zn—Al—Mg based layer formed on the base iron,
an oxide layer formed on the Zn—Al—Mg based layer, and a content ratio of Al to Mg (Al/Mg) in the oxide layer is 0.8 or more.

### Claim 2 (depends on 1)

The hot press formed product of claim 1, wherein the content ratio of Al to Mg is 0.9 or more.

### Claim 3 (depends on 1)

The hot press formed product of claim 1, wherein a total weight of the oxide layer is 700 mg/m2 or less (exclusive of 0 mg/m2).

### Claim 4 (depends on 1)

The hot press formed product of claim 1, wherein the oxide layer contains at least one selected from the group consisting of Mn, Si and Fe, and a sum of contents of Mn, Si and Fe in the oxide layer is 50% or less relative to a total contents of metals in the oxide layer.

### Claim 5 (depends on 1)

The hot press formed product of claim 1, wherein a ratio of a total amount of Mg (Mgo) contained in the oxide layer to a total amount of Mg (Mgc) contained in the Zn—Al—Mg based plating layer is 1 or less.

### Claim 6 (depends on 1)

The hot press formed product of claim 1, wherein an alloying degree of Fe in the Zn—Al—Mg based layer is 20-70%.

### Claim 7 (depends on 1)

The hot press formed product of claim 1, wherein the Zn—Al—Mg-based plating layer contains: 0.9-3.5% by weight of Mg, and 1.0-15% by weight of Al, with a balance of Zn and other unavoidable impurities.

### Claim 8 (depends on 1)

The hot press formed product of claim 1, wherein the base iron contains: 0.15-0.35% by weight of C, 0.5% by weight or less (exclusive of 0% by weight) of Si, 0.5-8.0% by weight of Mn, and 0.0020-0.0050% by weight of B, with a balance of Fe and unavoidable impurities.

### Claim 9 (depends on 1)

The hot press formed product of claim 1, wherein the hot press formed product has a maximum corrosion depth of 0.5 mm or less when measured after a salt spray test for 1200 hours according to KS R 1127.

### Claim 10 (depends on 1)

The hot press formed product of claim 1, wherein the hot press formed product has a tensile strength of 1300 MPa or more.

### Claim 11

A method for preparing a hot press formed product, comprising:
immersing base iron in a Zn—Al—Mg-based plating bath, and performing plating to obtain a Zn—Al—Mg-based plated steel material;
heating the Zn—Al—Mg-based plated steel material to a heating temperature of 600-950° C. at a rate of 10° C./sec or more in a heating furnace; and
forming the Zn—Al—Mg-based plated steel material which has reached the heating temperature with a mold simultaneously with quenching,
wherein a residence time is 120 seconds or less, the residence time representing a time during which the Zn—Al—Mg-based plated steel material which has reached the heating temperature resides in the heating furnace.

### Claim 12 (depends on 11)

The method of claim 11, wherein the heating temperature is 800° C. or more and 950° C. or less, an average heating rate to the heating temperature is 20° C./sec or more, and the residence time is 60 seconds or less.

### Claim 13 (depends on 11)

The method of claim 11, wherein the heating is carried out by any one method of radiant heating, high-frequency induction heating and ohmic heating.

### Claim 14 (depends on 11)

The method of claim 11, wherein the heating is carried out under an inert gas atmosphere.

### Claim 15 (depends on 11)

The method of claim 11, wherein the content ratio of Al to Mg (Al/Mg) in the Zn—Al—Mg-based plating bath is 0.8 or more.

### Claim 16 (depends on 11)

The method of claim 11, wherein the base iron is a cold rolled steel plate, and the cold rolled steel plate has a surface roughness of 2.0 μm or less before plating.

### Claim 17 (depends on 11)

The method of claim 11, wherein the base iron contains: 0.15-0.35% by weight of C, 0.5% by weight or less (exclusive of 0%) of Si, 0.5-8.0% by weight of Mn, and 0.0020-0.0050% by weight of B, with a balance of Fe and unavoidable impurities.

### Claim 18 (depends on 17)

The method of claim 17, further comprising the following before obtaining the plated steel material:
pre-plating one or more metals selected from the group consisting of Fe, Ni, Cu, Sn and Sb to an average thickness of 5-100 nm on a surface of the base iron; and
annealing the pre-plated base iron.

### Claim 19 (depends on 18)

The method of claim 18, wherein the annealing is carried out under 1-15% by volume of hydrogen gas and remaining nitrogen gas.