# US 2024/0002986 A1 · Iron-containing alloys and associated systems and methods

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0002986 A1
- Document ID: US20240002986A1
- Status: Published application
- Kind: A1
- Application number: 18/316,792
- Filed: 2023-05-12
- Published: 2024-01-04
- Earliest claimed: 2017-05-04
- Assignees: Massachusetts Institute of Technology
- Applicants: Massachusetts Institute of Technology
- Inventors: Dor Amram; Christopher A. Schuh
- Web page: https://patentgrep.com/patent/US20240002986A1

## CPC

- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 23/00: Alloys based on magnesium
- C22C 33/0257: {characterised by the range of the alloying elements}
- C22C 33/0278: {with at least one alloying element having a minimum content above 5%}
- C22C 38/008: {containing tin}
- C22C 38/06: containing aluminium
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/10: containing cobalt
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/16: containing copper
- C22C 38/18: containing chromium
- B22F 1/054: Nanosized particles
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- C22C 33/02: by powder metallurgy
- C22C 2200/04: Nanocrystalline
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER

## Abstract

Iron-containing alloys, and associated systems and methods, are generally described. The iron-containing alloys are, according to certain embodiments, nanocrystalline. According to certain embodiments, the iron-containing alloys have high relative densities. The iron-containing alloys can be relatively stable, according to certain embodiments. Inventive methods for making iron-containing alloys are also described herein. The inventive methods for making iron-containing alloys can involve, according to certain embodiments, sintering nanocrystalline particulates comprising iron and at least one other element (e.g., at least one other metal or a metalloid) to form an iron-containing nanocrystalline alloy.

## Claims

### Claim at position 1

1-51. (canceled)

### Claim 52

A method of forming a nanocrystalline metal alloy, comprising:
sintering a plurality of nanocrystalline particulates to form the nanocrystalline metal alloy;
wherein at least some of the nanocrystalline particulates comprise Fe and a second element, and wherein:
Fe is the most abundant element by atomic percentage in at least some of the nanocrystalline particulates; and/or
sintering the plurality of nanocrystalline particulates involves heating the nanocrystalline particulates to a first sintering temperature that is greater than or equal to 500° C. and less than or equal to 1100° C. for a sintering duration greater than or equal to 6 hours and less than or equal to 24 hours; and/or
sintering the plurality of nanocrystalline particulates involves heating the nanocrystalline particulates such that the nanocrystalline particulates are not at a temperature of greater than or equal to 1100° C. for more than 24 hours; and/or
the second element and Fe exhibit a miscibility gap.

### Claim at position 3

53-57. (canceled)

### Claim 58

A method of forming a metal alloy, comprising:
sintering powder comprising Fe and Mg to produce the metal alloy, wherein the metal alloy has a relative density of greater than or equal to 80%.

### Claim 59 (depends on 52)

The method of claim 52, wherein the second element is a second metal.

### Claim 60

(canceled)

### Claim 61 (depends on 52)

The method of claim 52, wherein the Fe and the second element are present in a non-equilibrium phase.

### Claim 62 (depends on 52)

The method of claim 52, wherein the non-equilibrium phase undergoes decomposition during the sintering.

### Claim 63 (depends on 52)

The method of claim 52, wherein the non-equilibrium phase undergoes decomposition during the sintering, and the decomposition of the non-equilibrium phase accelerates a rate of sintering of the nanocrystalline particulates.

### Claim 64 (depends on 52)

The method of claim 52, wherein the non-equilibrium phase comprises a supersaturated phase comprising the second element dissolved in Fe.

### Claim 65 (depends on 52)

The method of claim 52, wherein the second element is selected from the group consisting of magnesium (Mg), boron (B), zirconium (Zr), gold (Au), chromium (Cr), nickel (Ni), vanadium (V), platinum (Pt), lead (Pb), copper (Cu), cobalt (Co), and tin (Sn).

### Claim 66 (depends on 52)

The method of claim 52, wherein the second element is Mg.

### Claim 67 (depends on 52)

The method of claim 52, further comprising cold pressing the plurality of nanocrystalline particulates during at least one portion of time prior to the sintering.

### Claim 68

(canceled)

### Claim 69 (depends on 52)

The method of claim 52, wherein the cold pressing comprises cold compression of the plurality of nanocrystalline particulates at a force greater than or equal to 300 MPa and less than or equal to 1400 MPa.

### Claim 70 (depends on 52)

The method of claim 52, wherein the sintering comprises heating the nanocrystalline particulates to a first sintering temperature lower than a second sintering temperature needed for sintering Fe in the absence of the second element.

### Claim 71 (depends on 52)

The method of claim 52, wherein the sintering comprises heating the nanocrystalline particulates to a temperature greater than or equal to 600° C. and less than or equal to 1100° C. for a duration greater than or equal to 6 hours and less than or equal to 24 hours.

### Claim 72

(canceled)

### Claim 73 (depends on 52)

The method of claim 52, wherein the non-equilibrium phase comprises a solid solution.

### Claim 74 (depends on 52)

The method of claim 52, further comprising forming at least some of the nanocrystalline particulates by mechanically working a powder comprising Fe and the second element.

### Claim 75 (depends on 52)

The method of claim 52, further comprising forming at least some of the nanocrystalline particulates by ball milling a powder comprising Fe and the second element.

### Claim 76 (depends on 52)

The method of claim 52, wherein at least some of the nanocrystalline particulates have a grain size of smaller than or equal to 50 nm.

### Claim at position 23

77-78. (canceled)

### Claim 79 (depends on 52)

The method of claim 52, wherein the second element is present in the nanocrystalline particulates in an amount of less than or equal to 30 at % of the nanocrystalline particulates.

### Claim at position 25

80-84. (canceled)

### Claim 85 (depends on 52)

The method of claim 52, wherein the nanocrystalline metal alloy has a relative density of at least 90%.

### Claim 86 (depends on 52)

The method of claim 52, wherein the sintering further comprises forming a second phase at at least one of a surface and a grain boundary of the nanocrystalline particulates during the sintering.

### Claim 87 (depends on 52)

The method of claim 52, wherein the sintering further comprises forming a second phase at at least one of a surface and a grain boundary of the nanocrystalline particulates during the sintering; and the second phase is rich in the second element.

### Claim 88 (depends on 52)

The method of claim 52, wherein the nanocrystalline metal alloy has a first grain size and a sintered material comprising Fe in the absence of the second element has a second grain size, the first grain size being smaller than the second grain size.

### Claim 89

(canceled)

### Claim 90 (depends on 52)

The method of claim 52, wherein the sintering is conducted essentially free of external applied stress.

### Claim 91

(canceled)

### Claim 92 (depends on 52)

A nanocrystalline metal alloy produced by the method of claim 52.

### Claim 93

(canceled)

### Claim 94 (depends on 52)

The method of claim 52, wherein for at least 20% of the time during which sintering is performed, the maximum external pressure applied to the nanocrystalline particulates is less than or equal to 2 MPa.

### Claim 95 (depends on 52)

The method of claim 52, wherein the sintering is pressureless sintering.