# US 2024/0002970 A1 · Steel plate for pressure vessel with excellent cryogenic toughness, and method of manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0002970 A1
- Document ID: US20240002970A1
- Status: Published application
- Kind: A1
- Application number: 18/265,122
- Filed: 2021-11-22
- Published: 2024-01-04
- Earliest claimed: 2020-12-10
- Assignees: Posco
- Applicants: Posco
- Inventors: Soon-Taik HONG
- Web page: https://patentgrep.com/patent/US20240002970A1

## CPC

- C21D 6/001: {containing Ni (C21D6/004 takes precedence)}
- C21D 9/46: for sheet metals
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 1/26: Methods of annealing
- C21D 1/28: Normalising
- C21D 1/56: characterised by the quenching agents
- C21D 1/60: Aqueous agents
- C21D 1/84: Controlled slow cooling (cooling-beds for metal rolling B21B43/00)
- C21D 6/004: {containing Cr and Ni}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0263: {following hot rolling}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/44: with molybdenum or tungsten
- C21D 2211/001: Austenite
- C21D 2211/002: Bainite
- C21D 2211/008: Martensite
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The present invention relates to a method of manufacturing a cryogenic steel plate for a pressure vessel and a cryogenic steel plate for a pressure vessel manufactured thereby, the method comprising the steps of: reheating a slab containing, in weight %, C: 0.05-0.15%, Si: 0.20-0.35%, Mn: 0.5-1.5%, P: 0.012% or less, S: 0.015% or less, Al: 0.02-0.10%, Ni: 6.01-6.49%, Mo: 0.2-0.4%, Cr: and the balance being Fe and inevitable impurities; hot-rolling the reheated steel plate, followed by air cooling; subjecting the air-cooled steel plate to primary heat treatment at 800-880° C. for (2.4×t+(10−40)) minutes (t: slab thickness (mm)), followed by primary water cooling: subjecting the primarily water-cooled steel plate to secondary heat treatment at 700-780° C. for (2.4×t+(10−40)) minutes (t: slab thickness (mm)), followed by secondary water cooling: and tempering the secondarily water-cooled steel plate.

## Claims

### Claim 1

A method of manufacturing a steel plate for a cryogenic pressure vessel, comprising:
reheating a slab containing, in weight %, C: 0.05 to 0.15%, Si: 0.20 to 0.35%, Mn: 0.5 to 1.5%, P: 0.012% or less, S: 0.015% or less, Al: 0.02 to 0.10%, Ni: 6.01 to 6.49%, Mo: 0.2 to 0.4%, Cr: 0.05 to 0.25%, and the balance being Fe and inevitable impurities;
hot-rolling the reheated steel plate, followed by air cooling;
subjecting the air-cooled steel plate to primary heat treatment at 800 to 880° C. for (2.4×t+(10 to 40)) minutes (t: slab thickness (mm)), followed by primary water cooling:
subjecting the primarily water-cooled steel plate to secondary heat treatment at 700 to 780° C. for (2.4×t+(10 to 40)) minutes (t: slab thickness (mm)), followed by secondary water cooling: and
tempering the secondarily water-cooled steel plate.

### Claim 2

A steel plate for a cryogenic pressure vessel, comprising:
in weight %, C: 0.05 to 0.15%, Si: 0.20 to 0.35%, Mn: 0.5 to 1.5%, P: 0.012% or less, S: 0.015% or less, Al: 0.02 to 0.10%, Ni: 6.01 to 6.49%, Mo: 0.2 to 0.4%, Cr: 0.05 to 0.25% and the balance being Fe and inevitable impurities,
wherein the steel microstructure has a three-phase mixed structure of 1 to 9.5% of retained austenite, 40 to 80% of tempered bainite, and the balance being tempered martensite on an area fraction basis.