# US 2024/0002969 A1 · Dual phase stainless steel sheet and dual phase stainless hot-rolled sheet, and method for manufacturing dual phase stainless steel sheet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0002969 A1
- Document ID: US20240002969A1
- Status: Published application
- Kind: A1
- Application number: 18/039,191
- Filed: 2021-11-26
- Published: 2024-01-04
- Earliest claimed: 2020-11-30
- Assignees: Nippon Steel Stainless Steel Corporation
- Applicants: NIPPON STEEL Stainless Steel Corporation
- Inventors: Takuya SAKURABA; Eiichiro ISHIMARU
- Web page: https://patentgrep.com/patent/US20240002969A1

## CPC

- C21D 9/46: for sheet metals
- C21D 6/004: {containing Cr and Ni}
- C21D 6/005: {containing Mn}
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0263: {following hot rolling}
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/008: {containing tin}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/52: with cobalt
- C22C 38/54: with boron
- C22C 38/58: with more than 1.5% by weight of manganese
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- C21D 2201/05: Grain orientation
- C21D 2211/001: Austenite
- C21D 2211/005: Ferrite
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

This titanium material is a dual phase stainless steel sheet containing an austenite and a ferrite and has a predetermined chemical composition, wherein, in a center part in a sheet thickness of a cross section in a perpendicular-to-rolling direction which is a direction perpendicular to a rolling direction on a rolled surface and a direction parallel to a sheet thickness direction, an area ratio S<001>/S<111> which is a ratio of an area proportion S<001> of a texture of a ferrite with the <001> direction oriented in the perpendicular-to-rolling direction to an area proportion S<111> of a texture of a ferrite with the <111> direction oriented in the perpendicular-to-rolling direction is 0.90 to 1.10.

## Claims

### Claim at position 1

-9. (canceled)

### Claim 10

A dual phase stainless steel sheet containing an austenite and a ferrite,
wherein the dual phase stainless steel sheet comprises:
in mass %,
C: 0.080% or less,
Si: 1.00% or less,
Mn: 4.00% or less,
P: 0.040% or less,
S: 0.0300% or less,
Ni: 1.50 to 8.00%,
Cr: 18.00 to 28.00%,
Mo: 5.00% or less,
Cu: 0.05 to 1.50%, and,
N: 0.080 to 0.320%, with the remainder of Fe and impurities,
wherein, in a center part in a sheet thickness of a cross section in a perpendicular-to-rolling direction which is a direction perpendicular to a rolling direction on a rolled surface and a direction parallel to a sheet thickness direction, an area ratio S<001>/S<111> which is a ratio of an area proportion S<001> of a texture of a ferrite with the <001> direction oriented in the perpendicular-to-rolling direction to an area proportion S<111> of a texture of a ferrite with the <111> direction oriented in the perpendicular-to-rolling direction is 0.90 to 1.10.

### Claim 11 (depends on 10)

The dual phase stainless steel sheet according to claim 10,
wherein the surface waviness height in the rolling direction is 0.3 μm or less.

### Claim 12 (depends on 10)

The dual phase stainless steel sheet according to claim 10, comprising,
in mass %,
C: 0.030% or less,
Si: 0.75% or less,
Mn: 2.00 to 4.00%,
P: 0.040% or less,
S: 0.0200% or less,
Ni: 1.50 to 2.50%,
Cr: 18.00 to 21.50%,
Mo: 0.60% or less,
Cu: 0.50 to 1.50%, and,
N: 0.150 to 0.200%, with the remainder of Fe and impurities.

### Claim 13 (depends on 11)

The dual phase stainless steel sheet according to claim 11, comprising,
in mass %,
C: 0.030% or less,
Si: 0.75% or less,
Mn: 2.00 to 4.00%,
P: 0.040% or less,
S: 0.0200% or less,
Ni: 1.50 to 2.50%,
Cr: 18.00 to 21.50%,
Mo: 0.60% or less,
Cu: 0.50 to 1.50%, and,
N: 0.150 to 0.200%, with the remainder of Fe and impurities.

### Claim 14 (depends on 10)

The dual phase stainless steel sheet according to claim 10 comprising, in mass %, in place of some Fe, one or more of
Al: 0.003 to 0.050%,
O: 0.0070% or less,
Nb: 0.005 to 0.20%,
Ti: 0.005 to 0.20%,
Co: 0.005 to 0.25%,
V: 0.005 to 0.15%,
Sn: 0.005 to 0.20%,
Sb: 0.005 to 0.20%,
Ga: 0.001 to 0.050%,
Zr: 0.005 to 0.50%,
Ta: 0.005 to 0.100%, and,
B: 0.0002 to 0.0050%.

### Claim 15 (depends on 11)

The dual phase stainless steel sheet according to claim 11, comprising, in mass %, in place of some Fe, one or more of
Al: 0.003 to 0.050%,
0.0070% or less,
Nb: 0.005 to 0.20%,
Ti: 0.005 to 0.20%,
Co: 0.005 to 0.25%,
V: 0.005 to 0.15%,
Sn: 0.005 to 0.20%,
Sb: 0.005 to 0.20%,
Ga: 0.001 to 0.050%,
Zr: 0.005 to 0.50%,
Ta: 0.005 to 0.100%, and,
B: 0.0002 to 0.0050%.

### Claim 16 (depends on 12)

The dual phase stainless steel sheet according to claim 12, comprising, in mass %, in place of some Fe, one or more of
Al: 0.003 to 0.050%,
O: 0.0070% or less,
Nb: 0.005 to 0.20%,
Ti: 0.005 to 0.20%,
Co: 0.005 to 0.25%,
V: 0.005 to 0.15%,
Sn: 0.005 to 0.20%,
Sb: 0.005 to 0.20%,
Ga: 0.001 to 0.050%,
Zr: 0.005 to 0.50%,
Ta: 0.005 to 0.100%, and,
B: 0.0002 to 0.0050%.

### Claim 17 (depends on 13)

The dual phase stainless steel sheet according to claim 13, comprising, in mass %, in place of some Fe, one or more of
Al: 0.003 to 0.050%,
O: 0.0070% or less,
Nb: 0.005 to 0.20%,
Ti: 0.005 to 0.20%,
Co: 0.005 to 0.25%,
V: 0.005 to 0.15%,
Sn: 0.005 to 0.20%,
Sb: 0.005 to 0.20%,
Ga: 0.001 to 0.050%,
Zr: 0.005 to 0.50%,
Ta: 0.005 to 0.100%, and,
B: 0.0002 to 0.0050%.

### Claim 18

A dual phase stainless hot-rolled sheet containing an austenite and a ferrite,
wherein the dual phase stainless hot-rolled sheet comprises:
in mass %,
C: 0.080% or less,
Si: 1.00% or less,
Mn: 4.00% or less,
P: 0.040% or less,
S: 0.0300% or less,
Ni: 1.50 to 8.00%,
Cr: 18.00 to 28.00%,
Mo: 5.00% or less,
Cu: 0.05 to 1.50%, and,
N: 0.080 to 0.320%, with the remainder of Fe and impurities
wherein the difference between the Vickers hardness of the austenite and the Vickers hardness of the ferrite is 50 HV or more and 75 HV or less.

### Claim 19 (depends on 18)

The dual phase stainless hot-rolled sheet according to claim 18, comprising, in mass %, Ni: 2.00 to 8.00%.

### Claim 20 (depends on 18)

The dual phase stainless hot-rolled sheet according to claim 18, comprising, in mass %, in place of some Fe, one or more of
Al: 0.003 to 0.050%,
O: 0.0070% or less,
Nb: 0.005 to 0.20%,
Ti: 0.005 to 0.20%,
Co: 0.005 to 0.25%,
V: 0.005 to 0.15%,
Sn: 0.005 to 0.20%,
Sb: 0.005 to 0.20%,
Ga: 0.001 to 0.050%,
Zr: 0.005 to 0.50%,
Ta: 0.005 to 0.100%, and,
B: 0.0002 to 0.0050%.

### Claim 21 (depends on 19)

The dual phase stainless hot-rolled sheet according to claim 19, comprising, in mass %, in place of some Fe, one or more of
Al: 0.003 to 0.050%,
O: 0.0070% or less,
Nb: 0.005 to 0.20%,
Ti: 0.005 to 0.20%,
Co: 0.005 to 0.25%,
V: 0.005 to 0.15%,
Sn: 0.005 to 0.20%,
Sb: 0.005 to 0.20%,
Ga: 0.001 to 0.050%,
Zr: 0.005 to 0.50%,
Ta: 0.005 to 0.100%, and,
B: 0.0002 to 0.0050%.

### Claim 22

A method for manufacturing a dual phase stainless steel sheet, comprising:
a hot rolling process in which a stainless steel containing, in mass %,
C: 0.080% or less,
Si: 1.00% or less,
Mn: 4.00% or less,
P: 0.040% or less,
S: 0.0300% or less,
Ni: 1.50 to 6.80%,
Cr: 18.00 to 28.00%,
Mo: 5.00% or less,
Cu: 0.05 to 1.50%, and
N: 0.080 to 0.320%, with the remainder of Fe and impurities is subjected to hot rolling and coiled at a temperature of 680° C. or higher;
a heat treatment process in which the stainless steel after the hot rolling process is heated at a temperature of 500° C. or higher and lower than 600° C. and maintained for 1 hour or longer; and
a cold rolling process in which the stainless steel after the heat treatment process is cold-rolled.

### Claim 23 (depends on 22)

The method for manufacturing a dual phase stainless steel sheet according to claim 22, comprising, in mass %, in place of some Fe, one or more of
Al: 0.003 to 0.050%,
O: 0.0070% or less,
Nb: 0.005 to 0.20%,
Ti: 0.005 to 0.20%,
Co: 0.005 to 0.25%,
V: 0.005 to 0.15%,
Sn: 0.005 to 0.20%,
Sb: 0.005 to 0.20%,
Ga: 0.001 to 0.050%,
Zr: 0.005 to 0.50%,
Ta: 0.005 to 0.100%, and,
B: 0.0002 to 0.0050%.