# US 2024/0002967 A1 · Thermal Processing Method for Niobium-Containing High-Alloy Austenitic Heat-Resistant Stainless Steel Bar

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0002967 A1
- Document ID: US20240002967A1
- Status: Published application
- Kind: A1
- Application number: 18/251,842
- Filed: 2022-05-11
- Published: 2024-01-04
- Earliest claimed: 2021-07-14
- Assignees: Shanxi Taigang Stainless Steel Co., Ltd.
- Applicants: Shanxi Taigang Stainless Steel Co., Ltd.
- Inventors: Xudong Fang; Yang Li; Fanghong Xu; Yan Xia; Wei Zhang; Jianwei Zhao
- Web page: https://patentgrep.com/patent/US20240002967A1

## CPC

- C21D 9/08: for tubular bodies or pipes
- B21B 3/02: Rolling special iron alloys {, e.g. stainless steel}
- C21D 7/13: by hot working
- C21D 8/06: during manufacturing of rods or wires
- C21D 8/10: during manufacturing of tubular bodies
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/26: with niobium or tantalum
- C22C 38/48: with niobium or tantalum
- C21D 6/004: {containing Cr and Ni}
- C21D 2211/001: Austenite
- C22C 38/58: with more than 1.5% by weight of manganese
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B21B: ROLLING OF METAL (auxiliary operations used in connection with metal-working operations covered in B21, see B21C; bending by rolling B21D; manufacture of particular objects, e.g. screws, wheels, rings, barrels, balls, by rolling B21H; pressure welding by means of a rolling mill B23K20/04)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The present disclosure relates to a hot working method for stainless steel bars, comprising: step (1) heating a steel ingot at a heating temperature in a range from 1200° C. to 1270° C.; step (2) subjecting the heated steel ingot to radial forging and cogging down according to a total compression ratio greater than 3 to obtain a square billet; step (3) heating the square billet at a heating temperature in a range from 1200° C. to 1270° C.; and step (4) subjecting the heated square billet to hot rolling to obtain a bar. The processing method of the present disclosure can avoid the quality defect of surface crack while ensuring production efficiency by optimizing the process flow and controlling key process parameters, so that niobium-containing high-alloy austenitic heat-resistant stainless steel bars with good surface quality and structure can be prepared.

## Claims

### Claim 1

A hot working method of a stainless steel bar, comprising:
Step (1): heating a steel ingot at a heating temperature in a range from 1,200° C. to 1,270° C.;
Step (2): subjecting the heated steel ingot to cogging by radial forging at a total compression ratio greater than 3 to obtain a square billet;
Step (3): heating the square billet at a heating temperature in a range from 1,200° C. to 1,270° C.; and
Step (4) subjecting the heated square billet to hot rolling to obtain a bar.

### Claim 2 (depends on 1)

The method according to claim 1, wherein in step (1), a holding time is determined according to the following equation:
T1=0.5D+600×w(Nb)×100
where:
T1 is a holding time for the steel ingot, in minutes;
D is a diameter of the steel ingot, in millimetres; and
w(Nb) is a mass percent content of Nb.

### Claim 3 (depends on 1)

The method according to claim 1, wherein in step (2), a surface temperature at the beginning of the radial forging is in a range from 1,000° C. to 1,050° C., and a surface temperature during the radial forging and at the end of the radial forging is in a range from 900° C. to 950° C.

### Claim 4 (depends on 1)

The method according to claim 1, wherein in step (2), the radial forging is carried out in 4 to 10 passes, a single pass deformation and a forging frequency for first and second passes are respectively 4% to 8% and 200 to 240 times/min, and a single pass deformation and a forging frequency for the subsequent passes are respectively 15% to 20% and 30 to 50 times/min.

### Claim 5 (depends on 1)

The method according to claim 1, wherein in step (3), a holding time is determined according to the following equation:
T2=0.5L+100×w(Nb)×100
where:
T2 is a holding time for the square billet, in minutes;
L is a side length of the square billet, in millimetres; and
w(Nb) is a mass percent content of Nb.

### Claim 6 (depends on 1)

The method according to claim 1, wherein in step (4), a surface temperature at the beginning of the hot rolling is in a range from 1,100° C. to 1,150° C., and a surface temperature during the hot rolling and at the end of the hot rolling is 1,000° C. or more.

### Claim 7 (depends on 1)

The method according to claim 1, wherein in step (4), the hot rolling is carried out in 5 to 10 passes, a single pass deformation is 10%-15%, and a rolling speed is 1˜1.2 m/s.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the stainless steel bar has the following elemental composition:
C 0.04% to 0.10%, Si≤0.75%, Mn≤2.00%, P<0.03%, S<0.03%, Cr 24.0% to 26.0%, Ni 17.0% to 23.0%, Nb 0.20% to 0.60%, N 0.15% to 0.35%, and a balance of Fe.

### Claim 9 (depends on 1, 2, 3, 4, 5, 6, 7, 8)

A stainless steel bar, which is prepared by using the hot working method in any one of claims 1 to 8.