# US 2024/0002722 A1 · Green fluorescent ceramic material, preparation method therefor and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0002722 A1
- Document ID: US20240002722A1
- Status: Published application
- Kind: A1
- Application number: 18/252,400
- Filed: 2021-11-11
- Published: 2024-01-04
- Earliest claimed: 2020-11-11
- Assignees: Fujian Institute of Research On the Structure of Matter, Chinese Academy of Sciences; Fujian Cas-Ceramic Optoelectronics Technology Co., Ltd
- Applicants: Fujian Institute of Research On the Structure of Matter, Chinese Academy of Sciences; Fujian Cas-Ceramic Optoelectronics Technology Co.,Ltd
- Inventors: Youfu ZHOU; Maochun HONG; Junrong LING; Xiuqiang ZHANG
- Web page: https://patentgrep.com/patent/US20240002722A1

## CPC

- C09K 11/7774: {Aluminates}
- C04B 35/44: based on aluminates
- C04B 35/6261: {Milling}
- C04B 35/62625: {Wet mixtures}
- C04B 35/62645: {Thermal treatment of powders or mixtures thereof other than sintering}
- C04B 35/62675: {characterised by the treatment temperature}
- C04B 35/638: Removal thereof
- C04B 35/64: Burning or sintering processes (C04B33/32 takes precedence {; powder metallurgy B22F})
- C09K 11/02: Use of particular materials as binders, particle coatings or suspension media therefor
- C09K 11/77: containing rare earth metals
- H10H 20/851: Wavelength conversion means
- C04B 2235/3206: Magnesium oxides or oxide-forming salts thereof
- C04B 2235/3208: Calcium oxide or oxide-forming salts thereof, e.g. lime
- C04B 2235/3222: Aluminates other than alumino-silicates, e.g. spinel (MgAl2O4)
- C04B 2235/3224: Rare earth oxide or oxide forming salts thereof, e.g. scandium oxide
- C04B 2235/3225: Yttrium oxide or oxide-forming salts thereof
- C04B 2235/3229: Cerium oxides or oxide-forming salts thereof
- C04B 2235/3418: Silicon oxide, silicic acids or oxide forming salts thereof, e.g. silica sol, fused silica, silica fume, cristobalite, quartz or flint
- C04B 2235/422: Carbon
- C04B 2235/441: Alkoxides, e.g. methoxide, tert-butoxide
- C04B 2235/483: Si-containing organic compounds, e.g. silicone resins, (poly)silanes, (poly)siloxanes or (poly)silazanes
- C04B 2235/5292: Flakes, platelets or plates
- C04B 2235/6581: Total pressure below 1 atmosphere, e.g. vacuum
- C04B 2235/764: Garnet structure A3B2(CO4)3
- C04B 2235/9607: Thermal properties, e.g. thermal expansion coefficient
- C04B 2235/9646: Optical properties
- C04B 2235/9653: Translucent or transparent ceramics other than alumina
- C04B 2235/9661: Colour
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS

## Abstract

A green fluorescent ceramic material, a preparation method therefor and the use thereof, are applicable in the field of fluorescent ceramics for LED lighting. The chemical constitution of the green fluorescent ceramic material is graphene-Y3-x-yAl5O12:x Ce3+, y Lu3+, with 0.0001≤x≤0.1, and 0.01≤y≤2.9; and the mass percentage of graphene is less than 0.5 wt % but is not 0 on the basis of the total weight of the green fluorescent ceramic material. The green fluorescent ceramic material has the characteristics of a high heat conductivity, a good heat dissipation property, and a controllable light-emitting wavelength within a range of 490-540 nm; and same is suitable for use as an LED encapsulating material.

## Claims

### Claim 1

A green fluorescent ceramic material, wherein the green fluorescent ceramic material has a chemical composition of graphene-Y3-x-yAl5O12:x Ce3+, y LU3+ with 0.0001≤x≤0.1, and 0.01≤y≤2.9; and based on the total weight of the green fluorescent ceramic material, a mass percentage of the graphene is less than 0.5 wt % but is not 0.

### Claim 2 (depends on 1)

The material as claimed in claim 1, wherein x is in a range of 0.0005≤x≤0.06, preferably 0.001≤x≤0.01;
preferably, y is in a range of 0.1≤y≤2.5, preferably 0.5≤y≤1.5;
preferably, based on the total mass of the green fluorescent ceramic material, the mass fraction of the graphene is less than or equal to 0.1 wt % and is not 0; preferably, the mass fraction of the graphene is less than or equal to 0.05 wt % and is not 0.

### Claim 3 (depends on 1)

The material as claimed in claim 1, wherein the green fluorescent ceramic material has a chemical composition of:
0.03 wt % graphene-Y2.989Al5O12:0.001 Ce3+, 0.01 Lu3+;
0.05 wt % graphene-Y2.497Al5O12:0.003 Ce3+, 0.5 Lu3+;
0.01 wt % graphene-Y1.493Al5O12:0.007 Ce3+, 1.5 Lu3+; or
0.05 wt % graphene-Y0.0985Al5O12:0.0015 Ce3+, 2.9 Lu3+.

### Claim 4 (depends on 1)

The material as claimed in claim 1, wherein the green fluorescent ceramic material is a transparent ceramic material;
for example, the green fluorescent ceramic material has a visible light transmittance of greater than or equal to 75%, preferably greater than or equal to 78%;
preferably, the green fluorescent ceramic material has a thermal conductivity of greater than 5 Wm−1 K−1, preferably greater than or equal to 7 Wm−1 K−1, and more preferably greater than or equal to 10 Wm−1 K−1.

### Claim 5 (depends on 1)

A method for preparing the green fluorescent ceramic material as claimed in claim 1, comprising the following steps:
1) weighing out starting materials and mixing by ball-milling: weighing out graphene, Y2O3, Al2O3, Lu2O3 and a Ce-containing compound as starting materials according to the above chemical composition of the green fluorescent ceramic material, adding a sintering aid into the starting materials, and performing ball-milling to obtain a uniformly dispersed slurry;
2) preparing a ceramic green body; and
3) embedding the ceramic green body obtained in step 2) with a powder, and performing vacuum sintering to obtain the green fluorescent ceramic material.

### Claim 6 (depends on 5)

The method as claimed in claim 5, wherein the sintering aid is one, two or more of CaO, MgO, SiO2 and TEOS, preferably a combination of CaO and TEOS, MgO, or a combination of MgO and TEOS;
preferably, the Ce-containing compound is selected from CeO2 and/or CeN3O9·6H2O;
preferably, based on the total weight of the green fluorescent ceramic material, when the sintering aid comprises CaO and/or MgO, a mass fraction of CaO or MgO is 0.001-0.01 wt %, for example 0.003-0.008 wt %;
preferably, based on the total weight of the green fluorescent ceramic material, when the sintering aid comprises SiO2 and/or TEOS, a mass fraction of SiO2 or TEOS is 0.01-0.1 wt %, for example 0.03-0.08 wt %;
preferably, the ball-milling is wet ball-milling; for example, a medium for the ball-milling is absolute ethanol or acetone; for example, the ball-milling is performed for a time period of 4-30 h;
preferably, the preparation of the ceramic green body in step 2) specifically comprises: subjecting the slurry obtained in step 1) to drying, sieving, dry pressing and cold isostatic pressing molding, and dewaxing to obtain the ceramic green body;
preferably, the sieving is performed through a 150 to 200-mesh sieve;
preferably, the degreasing is performed at a temperature of 250-600° C., preferably 400-550° C.; for example, the degreasing is performed for a time period of 2-10 h, preferably 4-8 h.

### Claim 7 (depends on 5)

The method as claimed in claim 5, wherein the powder for the embedding is one of or a mixture of two of Al2O3 and Y2O3;
preferably, in step 3), the powder needs to be subjected to calcination and crushing treatment at least once before the embedding;
preferably, before the embedding, the powder for the embedding is subjected to calcination and crushing in air at least once, for example, at least twice; preferably, the calcination is performed at a temperature of 1500-1750° C., preferably 1650-1750° C.; preferably, the calcination is performed for a time period of 4-15 h, preferably 6-10 h;
preferably, the powder for the embedding that has been subjected to calcination and crushing treatment at least once needs to be further sieved;
preferably, the embedding is performed by uniformly covering a surface, preferably an upper surface and a lower surface, of the ceramic green body with the powder for the embedding; preferably, a thickness for the embedding is 0.3-0.6 mm, for example 0.4-0.5 mm;
preferably, the vacuum sintering is performed at a temperature of 1600-1750° C., preferably 1650-1750° C.;
preferably, the vacuum sintering is performed with a holding time of 2-20 h, preferably 4-15 h.

### Claim 8 (depends on 5)

The method as claimed in claim 5, wherein the method for preparing the green fluorescent ceramic material comprises the following steps:
a) taking graphene, Y2O3, Al2O3, Lu2O3, as well as CeO2 and/or CeN3O9·6H2O as starting materials, and weighing out each of the starting materials according to the above chemical composition of the green fluorescent ceramic material;
b) adding a sintering aid to the above-formulated starting materials to obtain a mixed material;
c) taking absolute ethanol or acetone as a medium, and performing wet ball-milling on the mixed material to obtain a uniformly dispersed slurry;
d) subjecting the slurry to vacuum drying, sieving, dry pressing and cold isostatic pressing molding and a dewaxing procedure to obtain a ceramic green body; and
e) taking Al2O3 and/or Y2O3 that have been subjected to calcination and crushing treatment at least once as an embedding powder, embedding an upper surface and a lower surface of the ceramic green body, and then performing vacuum sintering to obtain the green fluorescent ceramic material.

### Claim 9 (depends on 1)

Use of the green fluorescent ceramic material as claimed in claim 1 in LEDs, preferably as an LED encapsulating material.

### Claim 10 (depends on 1)

An LED encapsulating material or an LED device comprising the green fluorescent ceramic material as claimed in claim 1;
preferably, the LED device has a luminous efficiency of no less than 160 lm/W, for example, no less than 165 lm/W;
preferably, the LED device has a luminescence peak wavelength in the green light region (490-540 nm);
preferably, the LED device is an LED lighting device;
preferably, the LED lighting device is a green LED lighting device; more preferably, the LED lighting device is a green LED fish gathering lamp.