# US 2023/0422403 A1 · Methods and systems for improving surface mount joinder

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0422403 A1
- Document ID: US20230422403A1
- Status: Published application
- Kind: A1
- Application number: 17/851,097
- Filed: 2022-06-28
- Published: 2023-12-28
- Earliest claimed: 2022-06-28
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company
- Inventors: Hsien-Wen Liu; Shih-Ting Hung; Jyun-Lin Wu; Yao-Chun Chuang; Yinlung Lu
- Web page: https://patentgrep.com/patent/US20230422403A1

## CPC

- H05K 3/225: {Correcting or repairing of printed circuits (H05K1/0292, H05K3/222, H05K3/288, H05K3/4685 take precedence)}
- B23K 1/0016: {Soldering of electronic components}
- B23K 1/008: Soldering within a furnace (B23K1/012 takes precedence)
- B23K 1/20: Preliminary treatment of work or areas to be soldered, e.g. in respect of a galvanic coating
- H05K 1/0271: {Arrangements for reducing stress or warp in rigid printed circuit boards, e.g. caused by loads, vibrations or differences in thermal expansion}
- H05K 1/181: associated with surface mounted components
- H05K 3/341: Surface mounted components
- B23K 2101/42: Printed circuits
- H05K 1/111: {Pads for surface mounting, e.g. lay-out}
- H05K 3/3436: {having an array of bottom contacts, e.g. pad grid array or ball grid array components}
- H05K 2201/09136: Means for correcting warpage
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Methods for improving joinder between a surface-mount package and a printed circuit board are disclosed. The warpage at a corner of the surface-mount package and at a corresponding corner of a joint area on the printed circuit board are measured to determine the degree of mismatch. A mini-pad is applied to the corner between the surface-mount package and the joint area on the printed circuit board. The thickness of the mini-pad pushes against the surface-mount package and the printed circuit board, reducing the degree of mismatch below a critical dimension of a ball grid array of the surface-mount package. The surface-mount package can then be soldered to the joint area, reducing or preventing the formation of solder bridges and short circuits.

## Claims

### Claim 1

A method for reducing solder bridges between a surface-mount package and a printed circuit board, comprising:
applying a mini-pad to a corner of a joint area on the printed circuit board to counter any mismatch; and
soldering the surface-mount package to the joint area of the printed circuit board.

### Claim 2 (depends on 1)

The method of claim 1, wherein the joint area lacks conductive pads in a corner where the mini-pad is applied.

### Claim 3 (depends on 1)

The method of claim 1, wherein the mini-pad has a length of about 1 millimeter to about 100 millimeters, a width of about 1 millimeter to about 100 millimeters, and a thickness of about 50 micrometers to about 500 micrometers.

### Claim 4 (depends on 1)

The method of claim 1, wherein the mini-pad is in the shape of a rectangle, a triangle, an L-shape, a circle, a cross, or a trapezoid.

### Claim 5 (depends on 1)

The method of claim 1, wherein the mini-pad is formed from a polymer that is heat resistant at temperatures above 250° C.

### Claim 6 (depends on 1)

The method of claim 1, wherein the mini-pad is fixed to the printed circuit board using an adhesive.

### Claim 7 (depends on 1)

The method of claim 1, wherein the surface mount package has a size of greater than 85 mm×85 mm.

### Claim 8 (depends on 1)

The method of claim 1, wherein the total warpage between the surface-mount package and the printed circuit board is from about 50 micrometers to about 500 micrometers.

### Claim 9 (depends on 1)

The method of claim 1, wherein the joint area comprises a plurality of conductive pads in the shape of an octagon having four sides of a first length and four sides of a second length that is different from the first length.

### Claim 10 (depends on 1)

The method of claim 1, wherein the mini-pad comprises an overhang which is located upon a conductive pad and a second part that rests upon a surface of the printed circuit board.

### Claim 11 (depends on 1)

The method of claim 1, wherein the joint area comprises a central square region with conductive pads having a first diameter, an octagonal region surrounding the central square region with conductive pads having a second diameter, and four trapezoidal regions on alternating sides of the octagonal region with conductive pads having a third diameter;
wherein the first diameter is greater than the second diameter, and the second diameter is greater than the third diameter.

### Claim 12

A method for improving joinder between a surface-mount package and a printed circuit board, comprising:
measuring a warpage at a corner of the surface-mount package;
measuring a warpage at a corresponding corner of a joint area of the printed circuit board;
determining a degree of mismatch between the corner of the surface-mount package and the corresponding corner of the joint area;
applying a mini-pad to the corresponding corner of the joint area, the mini-pad having a thickness sufficient to reduce the degree of mismatch below a critical dimension of a ball grid array of the surface-mount package; and
soldering the surface-mount package to the joint area of the printed circuit board.

### Claim 13 (depends on 12)

The method of claim 12, wherein the critical dimension is about 50 micrometers to about 500 micrometers.

### Claim 14 (depends on 12)

The method of claim 12, wherein the mini-pad has a thickness of about 50 micrometers to about 500 micrometers.

### Claim 15

A circuit board assembly, comprising:
a printed circuit board having a joint area on a surface thereof, and a raised pad in each corner of the joint area, the raised pad having a thickness of about 50 micrometers to about 500 micrometers; and
a surface-mount package joined to the printed circuit board in the joint area.

### Claim 16 (depends on 15)

The circuit board assembly of claim 15, wherein each raised pad is integral to a solder mask of the printed circuit board.

### Claim 17 (depends on 15)

The circuit board assembly of claim 15, wherein each raised pad has a length of about 1 millimeter to about 100 millimeters, a width of about 1 millimeter to about 100 millimeters, and a thickness of about 50 micrometers to about 500 micrometers.

### Claim 18 (depends on 15)

The circuit board assembly of claim 15, wherein each raised pad is in the shape of a rectangle, a triangle, an L-shape, a circle, a cross, or a trapezoid.

### Claim 19 (depends on 15)

The circuit board assembly of claim 15, wherein the surface mount package has a size of greater than 85 mm×85 mm.

### Claim 20 (depends on 15)

The circuit board assembly of claim 15, wherein the joint area comprises a square array of conductive pads that is missing a trapezoidal pattern of pads in each corner of the square array.