# US 2023/0420669 A1 · Positive Electrode Active Material, And Positive Electrode And Lithium Secondary Battery Including Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2023/0420669 A1
- Document ID: US20230420669A1
- Status: Published application
- Kind: A1
- Application number: 18/038,923
- Filed: 2021-11-30
- Published: 2023-12-28
- Earliest claimed: 2020-11-30
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution, Ltd.
- Inventors: Sang Wook Lee; Dae Jin Lee; Sang Min Park; Min Kwak; Wang Mo Jung; Gi Beom Han; Eun Sol Lho; Joong Yeop Do; Kang Joon Park
- Web page: https://patentgrep.com/patent/US20230420669A1

## CPC

- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- C01G 53/504: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.5, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.5
- C01G 53/506: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.8, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.8
- C01G 53/82: Compounds containing nickel, with or without oxygen or hydrogen, and containing two or more other elements
- H01M 4/364: {as mixtures}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 10/052: Li-accumulators
- C01P 2004/51: Particles with a specific particle size distribution
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- C01P 2004/80: Particles consisting of a mixture of two or more inorganic phases
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention relates to a positive electrode active material having low nickel disorder and high particle strength in a crystal structure, and capable of implementing a battery having excellent capacity properties and capacity retention, and a positive electrode and a lithium secondary battery including the same, wherein the positive electrode active material includes a large-diameter lithium transition metal oxide and a small-diameter lithium transition metal oxide whose average particle diameter (D50) is smaller than that of the large-diameter lithium transition metal oxide, wherein the large-diameter lithium transition metal oxide and the small-diameter lithium transition metal oxide each independently have a composition represented by Formula 1, and has a crystal grain size of 100 nm to 150 nm, wherein the difference in crystal grain size between the large-diameter lithium transition metal oxide and the small-diameter lithium transition metal oxide is less than 40 nm, and the positive electrode active material has a nickel disorder (Ni-disorder) of 1.5% or less.

## Claims

### Claim 1

A positive electrode active material comprising:
a large-diameter lithium transition metal oxide; and
a small-diameter lithium transition metal oxide whose average particle diameter (D50) is smaller than that of the large-diameter lithium transition metal oxide,
wherein the large-diameter lithium transition metal oxide and the small-diameter lithium transition metal oxide each independently have a composition represented by Formula 1 below, and have a crystal grain size of 100 nm to 150 nm, wherein a difference in crystal grain size between the large-diameter lithium transition metal oxide and the small-diameter lithium transition metal oxide is less than 40 nm, and
the positive electrode active material has a nickel disorder (Ni-disorder) of 1.5% or less:
Lix1[Nia1Cob1Mnc11Alc12Zrd1M2e1]O2 [Formula 1]
wherein in Formula 1 above,
M2 is one or more selected from B, Mg, Ca, V, Cr, Fe, Zn, Ga, Y, Nb, Mo, Ta, and W, and
1.03≤x1≤1.07, 0.7≤a1<1, 0<b1<0.3, 0<c11<0.3, 0.001<c12<0.05, 0.001≤d1≤0.0065, 0≤e1≤0.1, and a1+b1+c11+c12+d1+e1=1.

### Claim 2 (depends on 1)

The positive electrode active material of claim 1, wherein the a1 satisfies 0.8≤a1<1.

### Claim 3 (depends on 1)

The positive electrode active material of claim 1, wherein the d1 satisfies 0.002≤d1≤0.0045.

### Claim 4 (depends on 1)

The positive electrode active material of claim 1, wherein the large-diameter lithium transition metal oxide and the small-diameter lithium transition metal oxide each independently have the crystal grain size of 100 nm to 140 nm.

### Claim 5 (depends on 1)

The positive electrode active material of claim 1, wherein the large-diameter lithium transition metal oxide has a particle strength of 140 MPa to 180 MPa.

### Claim 6 (depends on 1)

The positive electrode active material of claim 1, wherein the small-diameter lithium transition metal oxide has a particle strength of 110 MPa to 150 MPa.

### Claim 7 (depends on 1)

The positive electrode active material of claim 1, wherein the large-diameter lithium transition metal oxide has the average particle diameter (50) of 8 μm to 15 μm.

### Claim 8 (depends on 1)

The positive electrode active material of claim 1, wherein the small-diameter lithium transition metal oxide has the average particle diameter (D50) of 3 μm to 7 μm.

### Claim 9 (depends on 1)

The positive electrode active material of claim 1, wherein a weight ratio of the large-diameter lithium transition metal oxide and the small-diameter lithium transition metal oxide is 5:5 to 9:1.

### Claim 10 (depends on 1)

A positive electrode comprising a positive electrode active material according to claim 1.

### Claim 11 (depends on 10)

A lithium secondary battery comprising the positive electrode according to claim 10.